daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

High Pressure Leaching of Tungsten and Vanadium with Sodium Carbonate from Spent SCR Denitration Catalyst AITranslate

School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University;School of Metallurgy and Environment, Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tungsten and vanadium were recovered from spent SCR denitration catalyst by high pressure leaching with Na2CO3.The effects were investigated of roasting pretreatment temperature,type and dosage of the leaching additive,Na_2CO_3 dosage,liquid-solid ratio,leaching time and temperature for tungsten and vanadium leaching.The phases of spent SCR denitration catalyst were analyzed by XRD characterization before and after leaching.The results show that spent SCR denitration catalyst can be leached without roasting pretreatment,and the optimized experimental conditions are as follows:Na_2CO_3addition of 20%,NaOH addition of 8%,liquid-solid ratio of 2∶1,leaching time of 2hand leaching temperature of 230 ℃.Under the above conditions,the leaching rates of tungsten and vanadium reach 75.06% and 89.35%,respectively.In addition,the XRD analysis results show that titanium exists mainly in the form of anatase TiO_2 in spent SCR denitration catalyst,and high-temperature roasting can promote TiO_2 transition from anatase to rutile,inhibiting tungsten and vanadium leaching.Part of tungsten may exist in TiO_2 in the form of solid solution,and therefore the microstructure of TiO_2 should be destroyed by strengthening leaching conditions to further improve the leaching rate of tungsten.

KeyWords AITranslate

spent SCR denitration catalyst high pressure leaching with Na2CO3 tungsten recovery vanadium recovery

1谭青,冯雅晨.我国烟气脱硝行业现状与前景及SCR脱硝催化剂的研究进展[J].化工进展,2011,30(S1):709-713. 被引量:91

2华攀龙,李守信,于光喜,颜少云,许峰,华杰,周枫林.一种从废旧SCR脱硝催化剂中回收钛白粉的方法(P)中国专利:CN103130265A,

3汪德志, 吴刚, 肖雨亭, 等. 从选择性催化还原脱硝催化剂中回收钨组分的方法:中国, 103088217A[P]. 2013-05-08.

4肖雨亭, 赵建新, 汪德志, 等. 选择性催化还原脱硝催化剂钒组分回收的方法:中国, 102732730A[P]. 2012-10-17.

5李守信, 索平, 王亦亲, 等. 从SCR脱硝催化剂中回收三氧化钨和偏钒酸铵的方法:中国, 102557142A[P]. 2012-07-11.

6朱跃, 何胜, 张扬. 从废烟气脱硝催化剂中回收金属氧化物的方法:中国, 101921916A[P]. 2010-12-22.

7孙玉龙,刘永浩,蔡明哲.从SCR脱硝废触媒中回收金属氧化物的方法(P)中国专利:CN103160690A,

8霍怡廷,常志东,董彬,李文军.一种SCR废烟气脱硝催化剂的回收方法(P)中国专利:CN103526031A,

9云端,宋蔷,姚强.V_2O_5-WO_3/TiO_2 SCR催化剂的失活机理及分析[J].煤炭转化,2009,32(1):91-96. 被引量:49

10Li Qi-chao,Liu Zhen-yu,Liu Qing-ya.Kinetics of vanadium leaching from a spent industrial V2O5/TiO2catalyst by sulfuric acid. Industrial&Engineering Chemistry Research . 2014

1辛玥,赵亮,王海旭.废催化剂中贵金属钒的浸出工艺[J].产业与科技论坛,2018,17(18):80-81. 被引量:1

2郑怡琳,戴世金,赵由才,牛冬杰,张超洋,代宇轩.废SCR催化剂中钒和钨的有机酸浸出[J].化工环保,2020,40(2):162-168. 被引量:4

3李强,陈铁军,李奇勇,王明珠,李士龙.废弃SCR脱硝催化剂资源化利用研究进展[J].中国冶金,2020,30(5):1-10. 被引量:5

4贾秀敏,陈天宝,黄永,刘会武,刘忠臣,李培佑,向秋林.钠化焙烧法从SCR废脱硝催化剂中回收钛[J].钢铁钒钛,2020,41(6):1-5. 被引量:3

5侯学军,章小明,程文博,王馨,王春霞,徐盛明,黄国勇.废钒钛基SCR催化剂的处置方法研究进展[J].化工进展,2021,40(10):5313-5324. 被引量:4

6韩桂洪,王旱雨,苏胜鹏,黄艳芳,刘兵兵.溶解态钨钒选择性分离技术研究进展及探讨[J].中国有色金属学报,2021,31(11):3380-3395. 被引量:3

7张新远,张柏林,张深根.废钒钛系脱硝催化剂碱法回收研究进展[J].化工进展,2022,41(S01):580-594. 被引量:1

8庞君保,周朝辉,许伟,余宇航.硫酸镁磷渣中钒的浸出研究[J].石化技术,2023,30(4):53-55.

1张涛,陈晓利,孙超,袁冬冬.废钒钛系SCR催化剂有价金属回收与再利用研究进展[J].现代化工,2021,41(S01):67-72. 被引量:4

2王海北.我国二次资源循环利用技术现状与发展趋势[J].有色金属:冶炼部分,2019,0(9):1-11. 被引量:21

3汪胡根,程厚德,单宏伟,李雄浩,马士新,曹宝辰,陈逸伦.废弃脱硝催化剂的回收现状[J].广东化工,2020,47(17):145-147. 被引量:1

4张文志.升温法SCR脱硝结构流场优化设计[J].中国冶金,2021,31(1):68-74. 被引量:1

5张振全,赵备备,李兰杰,董自慧,白瑞国,王海旭.废SCR脱硝催化剂钒、钛、钨选择性分离研究[J].钢铁钒钛,2021,42(1):24-31. 被引量:4

6林政隆,宋浩,吴卫红,刘少俊,郑成航,高翔.季铵盐N263萃取分离废SCR催化剂碱浸液中的钒[J].化工环保,2021,41(5):571-575.

7侯学军,章小明,程文博,王馨,王春霞,徐盛明,黄国勇.废钒钛基SCR催化剂的处置方法研究进展[J].化工进展,2021,40(10):5313-5324. 被引量:4

8韩桂洪,王旱雨,苏胜鹏,黄艳芳,刘兵兵.溶解态钨钒选择性分离技术研究进展及探讨[J].中国有色金属学报,2021,31(11):3380-3395. 被引量:3

9韩桂洪,王静雯,刘兵兵,孙虎,黄艳芳.湿法炼锌净化钴渣回收钴技术进展及展望[J].贵州大学学报:自然科学版,2022,39(2):1-6. 被引量:1

10范晓慧,朱渊,甘敏,季志云,孙增青,武钰丰.氧化球团烟气中SO_(2)和H_(2)O(g)对SCR脱硝的影响[J].钢铁研究学报,2022,34(5):429-437.

1王君,赵刚,张朝红,张向东,张冠,马腾,姜岳峰,张鹏.处理温度对锐钛型TiO_2光催化活性的影响及利用可见光降解甲基紫[J].染料与染色,2006,43(5):46-49. 被引量:3

2李春荣,杨胜科,段磊,刘江.二氧化钛光催化降解硝基苯废水[J].应用化工,2007,36(8):748-750. 被引量:7

3蒋应平,赵磊,王海北,蒋训雄.从高压浸出镓锗液中回收镓锗的试验研究[J].中国资源综合利用,2012,30(6):25-27. 被引量:10

4吕坤.废水中硝基苯的光催化降解实验研究[J].山西建筑,2010,36(11):183-184. 被引量:2

5谈军,余振泉,张一兵.锐钛型掺铁TiO_2可见光催化降解苯胺的研究[J].电子元件与材料,2012,31(3):61-63.

6刘洋,谭军,尹周澜,刘常青,陈启元,张平民,廖舟,王心皞.湿法炼锌沉铁渣和浸锌渣的焙烧预处理[J].中国有色金属学报,2016,26(1):212-222. 被引量:12

7陈娴,陆金,殷燕,唐雪弢,程洁红.电镀污泥的焙烧预处理及其浸出动力学[J].电镀与环保,2014,34(3):43-46. 被引量:2

8刘增超,郭霄.镧硫共掺杂纳米TiO_2可见光催化性能研究[J].西安工业大学学报,2014,34(10):830-835. 被引量:3

9专利文摘[J].化工环保,2013,33(5):389-389.

10张丽霞(译).从废锂离子电池中回收金属钻和锂[J].有色金属再生与利用,2006(1):39-39.

Basic Information:

DOI:

Chinese Library Classification Number:X773[环境科学与工程—环境工程]

Citation Information:

Tungsten and vanadium were recovered from spent SCR denitration catalyst by high pressure leaching with Na2CO3.The effects were investigated of roasting pretreatment temperature,type and dosage of the leaching additive,Na_2CO_3 dosage,liquid-solid ratio,leaching time and temperature for tungsten and vanadium leaching.The phases of spent SCR denitration catalyst were analyzed by XRD characterization before and after leaching.The results show that spent SCR denitration catalyst can be leached without roasting pretreatment,and the optimized experimental conditions are as follows:Na_2CO_3addition of 20%,NaOH addition of 8%,liquid-solid ratio of 2∶1,leaching time of 2hand leaching temperature of 230 ℃.Under the above conditions,the leaching rates of tungsten and vanadium reach 75.06% and 89.35%,respectively.In addition,the XRD analysis results show that titanium exists mainly in the form of anatase TiO_2 in spent SCR denitration catalyst,and high-temperature roasting can promote TiO_2 transition from anatase to rutile,inhibiting tungsten and vanadium leaching.Part of tungsten may exist in TiO_2 in the form of solid solution,and therefore the microstructure of TiO_2 should be destroyed by strengthening leaching conditions to further improve the leaching rate of tungsten.

quote

GB/T 7714-2015 [1] LUO Jun, GUAN Wen-juan, ZHANG Gui-qing, et al. High Pressure Leaching of Tungsten and Vanadium with Sodium Carbonate from Spent SCR Denitration Catalyst[J]. Rare Metals and Cemented Carbides, 2015(6): 1-6.
MLA [1] LUO Jun, et al., "High Pressure Leaching of Tungsten and Vanadium with Sodium Carbonate from Spent SCR Denitration Catalyst." Rare Metals and Cemented Carbides, no. 6, 2015, pp. 1-6.
APA [1] LUO Jun, GUAN Wen-juan, ZHANG Gui-qing, LI Zhi-hua, XUE Fei, ZHAO Hong, & HAN Zhang-min. (2015). High Pressure Leaching of Tungsten and Vanadium with Sodium Carbonate from Spent SCR Denitration Catalyst. Rare Metals and Cemented Carbides(6), 1-6.
IEEE [1] LUO Jun, GUAN Wen-juan, ZHANG Gui-qing, LI Zhi-hua, XUE Fei, ZHAO Hong, and HAN Zhang-min, "High Pressure Leaching of Tungsten and Vanadium with Sodium Carbonate from Spent SCR Denitration Catalyst," Rare Metals and Cemented Carbides, no. 6, pp. 1-6, 2015. keywords: {spent SCR denitration catalyst;high pressure leaching with Na2CO3;tungsten recovery;vanadium recovery}