The Latest Development of the Technologies to Treat APT Crystal Mother Liquor AITranslate

Kunming University of Technology Materials and Metallurgy Institute;Kunming University of Technology Materials and Metallurgy Institute;Kunming University of Technology Materials and Metallurgy Institute;Kunming University of Technology Materials and Metallurgy Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Some technologies for APT crystal mother liquor treatment are summarized, and the relatively reasonable and effective ones are emphatically introduced. The basic principle,process flowsheet and application effect of these technologies are reviewed, and their future development trends are also prospected.

KeyWords AITranslate

APT crystal mother liquor tungsten recovery ion exchange nanofiltration

1万林生,晏慧娟,肖学有,陈帮明,王辉.我国钨冶炼离子交换工艺的技术发展与工艺评价[J].中国钨业,2003,18(6):31-33. 被引量:20

2张全平.石灰直接沉淀法回收仲钨酸铵结晶母液中氧化钨方法的研究与工业实践.稀有金属,1981,(5):15-18.

3朱同浩.余碱分解法回收仲钨酸铵结晶母液中钨的工业实践[J].中国钨业,1991,0(7):14-16. 被引量:4

4徐迎春,姜萍.仲钨酸铵结晶母液的回收与利用[J].稀有金属与硬质合金,2004,32(3):29-31. 被引量:4

5张贵清,尚广浩,肖连生.纳滤法处理仲钨酸铵结晶母液的研究[J].稀有金属,2007,31(3):346-350. 被引量:7

6罗爱平,张启修.电渗析处理APT结晶母液的研究[J].中南矿冶学院学报,1994,25(1):44-48. 被引量:4

7孙培梅,李洪桂,李运姣,苏鹏抟,霍广生,赵中伟,刘茂盛.选择性沉淀法从钨酸盐溶液中除钼的工业试验[J].中国有色金属学报,2001,11(3):499-502. 被引量:22

8孙培梅,李洪桂,李运姣,苏鹏抟,赵中伟,霍广生,刘茂盛.APT结晶母液处理新工艺[J].中南工业大学学报,2000,31(1):27-29. 被引量:7

9陈启元,谭艳芝,胡慧萍,尹周澜.仲钨酸铵结晶制备进展[J].有色金属,2003,55(3):30-34. 被引量:10

10洪代琳.仲胺类萃取在我厂的应用[A].李正中.第七届全国钨钼学术交流会论文集[c].北京:中国钨业编辑部,1995.91-92.

1李义兵,刘开忠,张大增.钨冶炼工业工艺及装备述评[J].稀有金属与硬质合金,2015,43(3):1-4. 被引量:5

2卢勇甘.仲钨酸铵结晶母液处理技术的发展与工艺评价[J].中国钨业,2012,27(5):29-31. 被引量:1

3万林生,舒柳飞,赵立夫,谌勇明,李红超.黑钨矿与碳酸钙人工合成白钨的反应过程和机理[J].稀有金属与硬质合金,2014,42(2):1-4. 被引量:3

4万林生,黄小晶,杨亮,邓登飞,李红超,谌勇明.钨酸钠溶液氢氧化钙苛化-沉淀白钨的研究[J].有色金属科学与工程,2014,5(4):23-27. 被引量:3

5李义兵,罗鲲,肖超,孟征兵.从仲钨酸铵结晶母液中回收钨与氨的工艺研究[J].矿冶工程,2017,37(3):105-107.

1刘旭恒,胡芳,赵中伟.大孔型树脂处理高浓度钨酸钠溶液[J].中国有色金属学报,2014,24(7):1895-1900. 被引量:4

2万林生,潘明然,谌勇明,赵立夫,李红超.黑钨矿与碳酸钙人工合成白钨工艺研究[J].稀有金属与硬质合金,2014,42(6):1-3.

3罗小燕,于孟,陈斌,蒙鹏宇.基于模糊自适应PID控制的反应釜系统的设计与仿真[J].有色金属科学与工程,2015,6(5):129-134. 被引量:6

4杨亮,万林生,舒柳飞.(NH_4)_3PO_4-NH_3·H_2O-H_2O体系中磷酸铵溶解度[J].有色金属科学与工程,2016,7(2):39-42. 被引量:1

5黄志红.论科技期刊编辑与作者的合作[J].编辑学报,2016,28(5):418-420. 被引量:9

6易贤荣,徐双.高纯仲钨酸铵萃取法清洁生产工艺应用研究[J].中国钨业,2016,31(6):54-59. 被引量:3

7张平,赵珊,苏仕军,孙维义,丁桑岚.碳酸锰热解—酸洗制备高纯化学二氧化锰试验研究[J].湿法冶金,2019,38(3):239-242. 被引量:3

8杨运光,万林生,龚丹丹.粗钨酸钠溶液深度脱磷工业试验研究[J].稀有金属与硬质合金,2019,47(4):1-6. 被引量:3

9叶田田,刘立,谌建宇,刘钢,王振兴.钨冶炼行业清洁生产评价指标体系探讨[J].中国钨业,2020,35(4):45-51.

10赖星任,张龙辉,周加坤,张忠堂.钨酸钠浓料铝盐除氟工艺探讨[J].中国冶金,2021,31(4):118-121. 被引量:3

1张贵清,尚广浩,肖连生.纳滤法处理仲钨酸铵结晶母液的研究[J].稀有金属,2007,31(3):346-350. 被引量:7

2卢勇甘.仲钨酸铵结晶母液处理技术的发展与工艺评价[J].中国钨业,2012,27(5):29-31. 被引量:1

3徐迎春,姜萍.仲钨酸铵结晶母液的回收与利用[J].稀有金属与硬质合金,2004,32(3):29-31. 被引量:4

4梅东海.由仲钨酸铵结晶母液提钨的工艺方法[J].中国钨业,1990(10):18-20. 被引量:1

5一种从仲钨酸铵结晶母液中回收钨和氯化铵的方法[J].化学试剂,2008,30(1):76-76.

6邓解德.离子交换法回收仲钨酸铵结晶母液中的钨[J].中国钨业,1999,14(1):29-32. 被引量:7

7朱同浩.余碱分解法回收仲钨酸铵结晶母液中钨的工业实践[J].中国钨业,1991,0(7):14-16. 被引量:4

8万林生,龚丹丹,付赞辉,李红超,孙丽.仲钨酸铵结晶母液深度脱除氨氮的研究[J].稀有金属与硬质合金,2011,39(4):4-7. 被引量:1

9陈树茂,郭永忠.离子交换法处理仲钨酸铵结晶母液试验与实践[J].中国钨业,2001,16(3):22-24. 被引量:14

10韩曙祥.用离子交换处理仲钨酸铵结晶母液工艺探讨[J].中国钨业,1993,0(5):10-13.

Basic Information:

DOI:

Chinese Library Classification Number:TF803.2[冶金工程—有色金属冶金]

Citation Information:

Some technologies for APT crystal mother liquor treatment are summarized, and the relatively reasonable and effective ones are emphatically introduced. The basic principle,process flowsheet and application effect of these technologies are reviewed, and their future development trends are also prospected.

quote

GB/T 7714-2015 [1] LU Hui, XIE Gang, YU Xiao-hua, et al. The Latest Development of the Technologies to Treat APT Crystal Mother Liquor[J]. Rare Metals and Cemented Carbides, 2009(4): 44-47.
MLA [1] LU Hui, et al., "The Latest Development of the Technologies to Treat APT Crystal Mother Liquor." Rare Metals and Cemented Carbides, no. 4, 2009, pp. 44-47.
APA [1] LU Hui, XIE Gang, YU Xiao-hua, & LI Rong-xing. (2009). The Latest Development of the Technologies to Treat APT Crystal Mother Liquor. Rare Metals and Cemented Carbides(4), 44-47.
IEEE [1] LU Hui, XIE Gang, YU Xiao-hua, and LI Rong-xing, "The Latest Development of the Technologies to Treat APT Crystal Mother Liquor," Rare Metals and Cemented Carbides, no. 4, pp. 44-47, 2009. keywords: {APT;crystal mother liquor;tungsten recovery;ion exchange;nanofiltration}