daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Low-Temperature-Toughened Polypropylene Blends with Highly Packed Elastomeric Domains AITranslate

Korea Electrotechnology Research Institute (KERI); Korea Electrotechnology Research Institute (KERI); Korea Electrotechnology Research Institute (KERI); Korea Electrotechnology Research Institute (KERI); Korea Electrotechnology Research Institute (KERI); University of Science and Technology (UST)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Despite its versatility, the use of polypropylene (PP) has been limited to subzero temperature applications owing to its inherent brittleness at low temperatures. Herein, we introduce a PP ternary blend toughened by tailoring the domains of ethylene-propylene rubber (EPR) and poly(ethylene-co-octene) (EOC) within a PP matrix. The PP ternary blend was fabricated by melt-blending a PP and EOC binary mixture; a PP copolymer (PPC) was used as an additive. The Izod impact strength of the PP ternary blends dramatically increased between −50–20 °C compared to that of the iPP/EOC binary blend. Particularly, PP ternary blends with specific compositions exhibited impact strengths above 70 kJ/m2 even at −40 °C. The retraction rate of these blends was similar to that of high-performance specialty rubbers. Moreover, the blends exhibited a low brittleness temperature of −72.9 °C and, hence, may replace the expensive rubber products currently used for various low-temperature applications.

KeyWords AITranslate

polypropylene elastomer blend toughening impact strength
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01221

Chinese Library Classification Number:

Citation Information:

Despite its versatility, the use of polypropylene (PP) has been limited to subzero temperature applications owing to its inherent brittleness at low temperatures. Herein, we introduce a PP ternary blend toughened by tailoring the domains of ethylene-propylene rubber (EPR) and poly(ethylene-co-octene) (EOC) within a PP matrix. The PP ternary blend was fabricated by melt-blending a PP and EOC binary mixture; a PP copolymer (PPC) was used as an additive. The Izod impact strength of the PP ternary blends dramatically increased between −50–20 °C compared to that of the iPP/EOC binary blend. Particularly, PP ternary blends with specific compositions exhibited impact strengths above 70 kJ/m2 even at −40 °C. The retraction rate of these blends was similar to that of high-performance specialty rubbers. Moreover, the blends exhibited a low brittleness temperature of −72.9 °C and, hence, may replace the expensive rubber products currently used for various low-temperature applications.

quote

GB/T 7714-2015 [1] DoKyun Kim, Seong Hwan Lee, ShinKi Hong, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01221.
MLA [1] DoKyun Kim, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01221.
APA [1] DoKyun Kim, Seong Hwan Lee, ShinKi Hong, Se Won Han, Dae Ho Lee, & Seunggun Yu. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01221
IEEE [1] DoKyun Kim, Seong Hwan Lee, ShinKi Hong, Se Won Han, Dae Ho Lee, and Seunggun Yu, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01221. keywords: {polypropylene;elastomer;blend;toughening;impact strength}