Fractionated Crystallization Behavior of Low-Molecular-Weight Polyethylene Grafted onto SiO2 Nanoparticles AITranslate

China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; China|University of Chinese Academy of Sciences; University of the Basque Country UPV/EHU; China|University of Chinese Academy of Sciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The synthesis of polymer-grafted nanoparticles is crucial for the development of polymer nanocomposites with excellent properties, but the synthesis of polyethylene (PE)-grafted SiO2 nanoparticles (PE-g-SiO2 NPs) remains a significant challenge due to the chemical inertia of PE. In this study, PE-g-SiO2 NPs with different grafting densities and molecular weights were successfully synthesized by a simple “grafting to” method, and differential scanning calorimetry was used to study the crystallization behavior of grafted PE. Some PE-g-SiO2 samples exhibited three crystallization peaks in the cooling curve (i.e., fractionated crystallization phenomena). Self-nucleation (SN) and successive SN and annealing (SSA) results reveal that the nanoparticles in PE-g-SiO2 samples provoke both confinement and nucleation effects on the grafted PE chains. For PE-g-SiO2 NPs with higher grafting density and molecular weight, the PE chains are more stretched and the interfacial chain segmental dynamics are less suppressed, which enhance the nucleation effect and weaken the confinement effect.

KeyWords AITranslate

polyethylene polymergrafted nanoparticles fractionated crystallization nucleation effect confinement effect
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01394

Chinese Library Classification Number:

Citation Information:

The synthesis of polymer-grafted nanoparticles is crucial for the development of polymer nanocomposites with excellent properties, but the synthesis of polyethylene (PE)-grafted SiO2 nanoparticles (PE-g-SiO2 NPs) remains a significant challenge due to the chemical inertia of PE. In this study, PE-g-SiO2 NPs with different grafting densities and molecular weights were successfully synthesized by a simple “grafting to” method, and differential scanning calorimetry was used to study the crystallization behavior of grafted PE. Some PE-g-SiO2 samples exhibited three crystallization peaks in the cooling curve (i.e., fractionated crystallization phenomena). Self-nucleation (SN) and successive SN and annealing (SSA) results reveal that the nanoparticles in PE-g-SiO2 samples provoke both confinement and nucleation effects on the grafted PE chains. For PE-g-SiO2 NPs with higher grafting density and molecular weight, the PE chains are more stretched and the interfacial chain segmental dynamics are less suppressed, which enhance the nucleation effect and weaken the confinement effect.

quote

GB/T 7714-2015 [1] Shaofan Li, Weilong Ju, Wenhua Sun, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.2c01394.
MLA [1] Shaofan Li, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.2c01394.
APA [1] Shaofan Li, Weilong Ju, Wenhua Sun, Yunlan Su, Alejandro J. Müller, & Dujin Wang. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.2c01394
IEEE [1] Shaofan Li, Weilong Ju, Wenhua Sun, Yunlan Su, Alejandro J. Müller, and Dujin Wang, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.2c01394. keywords: {polyethylene;polymergrafted nanoparticles;fractionated crystallization;nucleation effect;confinement effect}