daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Analysis of Present Production and Latest Development of Cemented Carbide both at Home and Abroad AITranslate

Central South University Powder Metallurgical Factory;Central South University Powder Metallurgical Factory
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Brief analysis is made of the development of cemented carbides both at home and abroad and also the current production in China's cemented carbide industry. The paper describes the necessity for development of good quality cemented carbide materials. Analysis is also made of the latest development of cemented carbide for rock drilling.

KeyWords AITranslate

rock drilling cemented carbide present status development analysis

1李沐山.20世纪90年代世界硬质合金材料技术进展[M].株洲:硬质合金编辑部,2004.

2李沐山.国内外硬质合金现状与发展趋势[M].株洲:硬质合金厂,1994.

3周建华,孙宝琦,顾敏,赵少甫.真空热处理对矿用硬质合金组织性能的影响[J].金属热处理,1998(5):19-20. 被引量:6

4周建华,卢伟民.YJ2.1、YJ1.1矿山凿岩硬质合金的开发与应用[J].稀有金属与硬质合金,2001,29(4):10-12. 被引量:4

5曾日瓦诺夫BC.国外硬质合金技术发展的主要特点[J].国外硬质合金,1999,(2):28-28.

6Fischer,et al.Cemented carbide body used preferably for rock drilling and mineral cutting[P].US Pat:4743515,1988-05-10.

7Akerman,et al.Cemented carbide body with extra tough behavior[P].US Pat:5279901,1994-01-18.

8李沐山.梯度结构硬质合金的制取与应用[M].株洲:株洲硬质合金厂,1994.

9Hartzell,et al.Cemented carbide body with increased wear resistance[P].US Pat:5856626,1999-01-05.

10Fang zhigang,et al.Double cemented carbide composites[P].US Pat:5880382,1999-03-09.

1王进军.超细晶WC-Co硬质合金制备技术的研究[J].稀有金属与硬质合金,2015,43(2):50-53. 被引量:3

2高玉喜,郭志猛,张丽英,罗骥,刘祥庆.在还原过程中钒对纳米钨粉颗粒长大的抑制作用[J].粉末冶金工业,2007,17(5):29-33.

3戚正风,任瑞铭.国内外刀具材料发展现状[J].金属热处理,2008,33(1):15-20. 被引量:21

4李勇,谢淑华.WC粗晶硬质合金的研究进展[J].材料研究与应用,2009,3(2):77-80. 被引量:12

5李启厚,张程,王红军,刘志宏,刘智勇.超细镍粉的制备、应用现状及发展趋势[J].湿法冶金,2009,28(4):193-197. 被引量:4

6郭圣达,张正富,羊建高.钴盐沉淀法制备硬质合金混合料新工艺研究[J].硬质合金,2010,27(3):144-147. 被引量:2

7储开宇.硬质合金产业在我国的发展现状与展望[J].煤矿机械,2011,32(1):13-16. 被引量:6

8羊建高,戴煜.硬质合金的发展趋势及特殊粉末的制备技术[J].稀有金属与硬质合金,2011,39(1):48-51. 被引量:9

9储开宇.我国硬质合金产业的发展现状与展望[J].稀有金属与硬质合金,2011,39(1):52-56. 被引量:23

10刘海波,刘兆强.LWD电阻率新型耐磨带的研制[J].西部探矿工程,2011,23(9):61-62.

1郑清宏,刘江,时凯华,黄伟.粗细WC晶粒配比对双晶结构硬质合金力学性能与组织结构的影响[J].稀有金属与硬质合金,2020(1):75-79. 被引量:4

2邓四文.相同硬度的高钴和低钴含量硬质合金性能比较[J].理化检验:物理分册,2022,58(6):21-25.

3周永坤,赵先锐,王晓军.M2高速钢钻头热处理工艺及切削性能[J].金属热处理,2015,40(5):155-158. 被引量:4

4王进军.超细晶WC-Co硬质合金制备技术的研究[J].稀有金属与硬质合金,2015,43(2):50-53. 被引量:3

5杨胜,顾金宝,廖军,陈洪霞.烧结压力对WC-12%Co粗晶硬质合金组织及性能的影响[J].稀有金属与硬质合金,2015,43(2):54-58.

6潘金芝,任瑞铭,戚正风.国内外模具钢发展现状[J].金属热处理,2008,33(8):10-15. 被引量:34

7尹晓星.碳化钨、硬质合金文献调研[J].中国钨业,2008,23(5):7-10. 被引量:2

8陈明昕,雍岐龙,刘振宝,史庆南,亓海全,雍兮.有机物切割刀具用钢的研究和应用[J].金属热处理,2009,34(12):39-42. 被引量:2

9王弢,柯亚仕,周丹.硬质合金孔加工刀具的技术进展[J].工具技术,2011,45(5):9-12. 被引量:9

10沈志农,杨立.细WC配比对非均匀YG20C合金性能的影响[J].硬质合金,2011,28(3):163-165. 被引量:9

1周建华.矿用硬质合金发展动向分析[J].凿岩机械气动工具,2011,37(1):5-12. 被引量:4

2Deck.,RF,赵量.马氏体时效钢的近期发展[J].国外低合金钢:合金钢,1989(1):6-10.

3邹敦叙,贾天聪.Ti3Al基合金的近期发展[J].国外金属材料,1990(4):10-16. 被引量:1

4于影霞,何柏林,李力.国内外模具材料的现状及发展趋势[J].热加工工艺,2009,38(2):45-48. 被引量:26

5唐普林.略论我国硬质合金行业的技术引进方向[J].粉末冶金技术,1993,11(1):66-69.

6徐涛.中国硬质合金行业钴粉需求的技术经济分析[J].中国金属通报,2009(13):36-39.

7第十届铸铁科学与加工国际研讨会(SPCI10)[J].现代铸铁,2014(3):24-24.

8邱星武.激光技术在材料加工领域的发展及应用[J].稀有金属与硬质合金,2010,38(1):60-63. 被引量:13

9沈卓身,汪崧,黄震中.高耐蚀奥氏体合金的新进展[J].石油化工腐蚀与防护,1997,14(3):7-11. 被引量:10

10孙国雄.铸造技术的近期发展[J].国际学术动态,2001(2):19-20.

Basic Information:

DOI:

Chinese Library Classification Number:TG125.3[金属学及工艺—金属学]

Citation Information:

Brief analysis is made of the development of cemented carbides both at home and abroad and also the current production in China's cemented carbide industry. The paper describes the necessity for development of good quality cemented carbide materials. Analysis is also made of the latest development of cemented carbide for rock drilling.

quote

GB/T 7714-2015 [1] ZHOU Jian-hua, LU Wei-min. Analysis of Present Production and Latest Development of Cemented Carbide both at Home and Abroad[J]. Rare Metals and Cemented Carbides, 2006(1): 36-41.
MLA [1] ZHOU Jian-hua, and LU Wei-min. "Analysis of Present Production and Latest Development of Cemented Carbide both at Home and Abroad." Rare Metals and Cemented Carbides, no. 1, 2006, pp. 36-41.
APA [1] ZHOU Jian-hua, & LU Wei-min. (2006). Analysis of Present Production and Latest Development of Cemented Carbide both at Home and Abroad. Rare Metals and Cemented Carbides(1), 36-41.
IEEE [1] ZHOU Jian-hua and LU Wei-min, "Analysis of Present Production and Latest Development of Cemented Carbide both at Home and Abroad," Rare Metals and Cemented Carbides, no. 1, pp. 36-41, 2006. keywords: {rock drilling;cemented carbide;present status;development;analysis}