Effect of RE on the Properties and the Microstructure of CuNiZn Alloy AITranslate
Abstract AITranslate
Effect of RE on the properties and the microstructure of CuNiZn alloy has been studied by SEM, metallographic microscope and XRay. Results show that the RE has effect both on the mechanical properties and the microstructure of the alloy. The casting structure and recrystallization structure has become fine, the fensile strength and hardness have been increased and the elongation has been decreased; but with RE addition of over 1.0%, the hot plastisity of the alloy has become bad, thus the alloy is difficult to form.
KeyWords AITranslate
1郭晓梅,赵友昌.稀土元素对Al-Zn-Mg合金动态再结晶行为的影响[J].稀土,1991,12(2):38-42. 被引量:2
2邱聿成,叶英宁,李革.稀土在銅合金中的应用現状[J]稀土,1980(04).
1袁宜耀,孙勇,张秀兰,许磊.微量稀土元素对Sn-Ag-Sb系合金组织及焊料/Cu界面组织的影响[J].金属功能材料,2008,15(2):33-36. 被引量:9
2曾秋莲,章爱生,魏秀琴,周浪.微量稀土和硼在铜及其合金中的作用[J].特种铸造及有色合金,2002(3):55-57. 被引量:43
3孟祥锋,周丹,赵轩,康枭.微量钕对纯晶粒大小及铜硬度的影响[J].科技创新导报,2014,11(28):103-103.
4邵晴,吴敏.镧对Sn3.0Ag0.5Cu钎料组织及微米压痕性能影响[J].金属功能材料,2015,22(2):33-36. 被引量:3
1沈艳兰,顾小龙,徐时清,金霞.Ce的添加对SnAgCu系钎料组织和性能的影响[J].中国计量学院学报,2011,22(2):194-197. 被引量:4
2潘君益,金霞,沈艳兰.稀土元素对SnAgCu系无铅钎料合金组织与性能的影响[J].焊接技术,2013,42(3):31-34.
3郭淑梅,王永朝,刘月梅.加B冷凝管合金HSn70-1B熔铸特点[J].特种铸造及有色合金,2004(4):68-69.
4涂芳,何柏林.点焊电极强化工艺的研究进展[J].机械工程材料,2005,29(1):23-26. 被引量:9
5刘靖,韩静涛,符定梅,王江.小变形扩散-轧制生产蜂窝复合板中的助复剂[J].北京科技大学学报,2005,27(1):65-67. 被引量:4
6刘勇,刘平,李伟,田保红.Cu-Cr-Zr-Y合金时效析出行为研究[J].功能材料,2005,36(3):377-379. 被引量:20
7李伟,刘平,刘勇,田保红.微量稀土元素对Cu-Cr-Zr合金接触线抗软化性能的影响[J].金属热处理,2005,30(2):38-40. 被引量:11
8陈小红,李炎,田保红,张毅.Cu-Al-Y合金表面渗铝研究[J].特种铸造及有色合金,2005,25(11):656-657. 被引量:3
9刘喜波,刘平,贾淑果,田保红.微量Ce和Cr对Cu-0.1Ag合金性能的影响[J].金属热处理,2005,30(C00):238-241. 被引量:1
10张胜华,黄政权.稀土铈对冷凝管用锡黄铜组织及性能的影响[J].材料保护,2006,39(3):62-64. 被引量:12
1付博,王勇围,刘建华,刘龙玉,沈金龙,桂美文,马党参.V和N微合金化对77B钢组织和性能的影响[J].热处理,2009,24(6):31-33. 被引量:3
2张友寿,赵昌旭,夏露,黄晋.锑对蠕铁组织和性能的影响[J].热加工工艺,2005,34(6):15-16.
3刘政军,屈佳兴,苏允海.T4处理后AZ91镁合金焊接接头组织演变规律[J].沈阳工业大学学报,2014,36(6):642-646. 被引量:2
4熊仲明,张锁梅,石东崖,宋维锡.稀土、锑对灰铸铁的作用[J].中国稀土学报,1994,12(2):150-153. 被引量:2
5刘东,王永霞,向红亮,杨彩萍.时效温度对含Cu抗菌双相不锈钢力学及耐蚀性能的影响[J].金属热处理,2015,40(10):127-131. 被引量:3
6蔡璐,赵秀明,朱金华.1300MPa级高强度螺栓的研制[J].机械工程材料,2003,27(6):21-24. 被引量:2
7史鉴开,史小雨,吴宵三.微锑灰铸铁的生产[J].现代铸铁,2003,23(5):54-55. 被引量:3
8房洪杰,孙杰,刘慧,纪仁龙,尹登峰.复合添加Cr、Mn、Ti对7136铝合金组织及力学性能的影响[J].金属热处理,2017,42(4):53-57. 被引量:16
9张旭鹏,扈广麒,杨磊,马文治,杨林.过滤技术在大型铸钢件铸造中的应用[J].中国铸造装备与技术,2014,49(4):19-21.
10潘利文,罗涛,林覃贵,谭怡佳,唐侍琦,胡治流.稀土铝合金最新研究进展[J].轻合金加工技术,2016,44(9):12-16. 被引量:22
Basic Information:
DOI:
Chinese Library Classification Number:TG146.11[金属学及工艺—金属材料]
Citation Information:
Effect of RE on the properties and the microstructure of CuNiZn alloy has been studied by SEM, metallographic microscope and XRay. Results show that the RE has effect both on the mechanical properties and the microstructure of the alloy. The casting structure and recrystallization structure has become fine, the fensile strength and hardness have been increased and the elongation has been decreased; but with RE addition of over 1.0%, the hot plastisity of the alloy has become bad, thus the alloy is difficult to form.
quote
| GB/T 7714-2015 | [1] HUANG Yi-hong, TAN Xin-chang, ZHANG Jian-an. Effect of RE on the Properties and the Microstructure of CuNiZn Alloy[J]. Rare Metals and Cemented Carbides, 1999(2): 1-3. |
| MLA | [1] HUANG Yi-hong, et al., "Effect of RE on the Properties and the Microstructure of CuNiZn Alloy." Rare Metals and Cemented Carbides, no. 2, 1999, pp. 1-3. |
| APA | [1] HUANG Yi-hong, TAN Xin-chang, & ZHANG Jian-an. (1999). Effect of RE on the Properties and the Microstructure of CuNiZn Alloy. Rare Metals and Cemented Carbides(2), 1-3. |
| IEEE | [1] HUANG Yi-hong, TAN Xin-chang, and ZHANG Jian-an, "Effect of RE on the Properties and the Microstructure of CuNiZn Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 1-3, 1999. keywords: {RE, CuNiZn alloy, property, microstructure} |