Abstract AITranslate
Microstructure and dislocation behavior of the aluminium magnesium alloy containing scandium in the process of superplastic deformation were investigated by transmission electron microscope.The results show that four processes will take place in sequence during superplastic deformation, i.e., dynamic recrystallization;dislocations come from grain boundaries;motion of the dislocations within the grains is prohibited by the secondary phase Al3Sc as well as dislocations climb up and go over the dispersed particles;dislocations are annihilated in grain boundaries.It is found that dynamic recrystallization is the microstructure effect of the alloy and play a role in inducing microfine grain superplasticity during superplastic deformation. The dominant mechanism of superplastic deformation is that grain boundary sliding process will be accompanied by intergrainular dislocations.
KeyWords AITranslate
1林肇琦.新一代铝合金——铝钪合金的发展概况[J].材料导报,1992(3):10-16. 被引量:49
2蒋晓军,李依依,桂全红,马禄铭,梁国军,师昌绪.Sc对Al-Li-Cu-Mg-Zr合金组织与性能的影响[J].金属学报,1994,30(8). 被引量:23
3杨磊.高强高韧含钪铝合金研究,中南工业大学硕士研究论文[M].,1999..
4潘青林,高拥政,尹志民,左铁镛.Sc对Al-Mg合金组织与性能的影响[J].材料科学与工艺,1997,5(4):9-13. 被引量:15
1侯贤华,高英俊,秦平力.微量元素对Al—Mg合金微结构及合金性能的影响[J].汕头大学学报:自然科学版,2005,20(3):35-40. 被引量:1
1周琦,臧树俊,安亮,孟倩.燃烧合成Al/Mg_2Si复合材料的热力学分析[J].材料热处理学报,2010,31(3):25-29. 被引量:2
1周善佑,唐燕.扫描电镜定量研究Zn-5%Al-0.05%Mg合金的超塑变形机制[J].分析测试通报,1991,10(1):44-47.
2王斌,易丹青,罗文海,周玲伶,方西亚.微量Sc元素对AZ91镁合金组织性能的影响[J].铸造,2005,54(5):459-461. 被引量:11
3谭澄宇,陈准,郑子樵.Al-Mg-Sc合金的拉伸性能和显微组织研究[J].铝加工,2002,25(4):1-3. 被引量:7
4周琦.形变强化对疲劳裂纹萌生的组织效应[J].甘肃工业大学学报,1999,25(2):22-27. 被引量:1
5徐国富,金头男,邹景霞,尹志民,聂祚仁.微量Sc元素对Al-Cu合金组织与性能的影响[J].材料热处理学报,2004,25(2):15-18. 被引量:11
6张雪飞,周天国.连续铸挤成形Al-Mg-Sc合金的再结晶[J].轻合金加工技术,2010,38(9):49-51. 被引量:2
7王瑞杰,徐永波,王中光,周敬,张静华,胡壮麒.Ni基高温合金单晶裂尖位错行为的动态研究——Ⅰ.DFZ 的形成及微裂纹的扩展[J].材料科学进展,1992,6(2):103-108. 被引量:1
8崔建忠,马龙翔.超塑变形机制[J].金属科学与工艺,1991,10(1):68-76. 被引量:3
9徐国富,牟申周,尹志民.Sc含量对Al-2%Cu合金固溶处理行为的影响[J].湖南有色金属,2006,22(1):38-41. 被引量:2
10杨磊,潘青林,高拥政,尹志民.退火工艺对含Sc铝镁合金组织与性能的影响[J].铝加工,1998,21(6):41-44. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG146.21[金属学及工艺—金属材料]
Citation Information:
Microstructure and dislocation behavior of the aluminium magnesium alloy containing scandium in the process of superplastic deformation were investigated by transmission electron microscope.The results show that four processes will take place in sequence during superplastic deformation, i.e., dynamic recrystallization;dislocations come from grain boundaries;motion of the dislocations within the grains is prohibited by the secondary phase Al3Sc as well as dislocations climb up and go over the dispersed particles;dislocations are annihilated in grain boundaries.It is found that dynamic recrystallization is the microstructure effect of the alloy and play a role in inducing microfine grain superplasticity during superplastic deformation. The dominant mechanism of superplastic deformation is that grain boundary sliding process will be accompanied by intergrainular dislocations.
quote
| GB/T 7714-2015 | [1] PAN Qing-lin, YIN Zhi-min, YANG Lei, et al. Mechanism of Superplastic Deformation in AlMg Alloy Containing Scandium[J]. Rare Metals and Cemented Carbides, 1999(2): 4-6. |
| MLA | [1] PAN Qing-lin, et al., "Mechanism of Superplastic Deformation in AlMg Alloy Containing Scandium." Rare Metals and Cemented Carbides, no. 2, 1999, pp. 4-6. |
| APA | [1] PAN Qing-lin, YIN Zhi-min, YANG Lei, & ZUO Tie-yong. (1999). Mechanism of Superplastic Deformation in AlMg Alloy Containing Scandium. Rare Metals and Cemented Carbides(2), 4-6. |
| IEEE | [1] PAN Qing-lin, YIN Zhi-min, YANG Lei, and ZUO Tie-yong, "Mechanism of Superplastic Deformation in AlMg Alloy Containing Scandium," Rare Metals and Cemented Carbides, no. 2, pp. 4-6, 1999. keywords: {aluminium alloy containing scandium;superplastic deformation;grain boundary sliding} |