daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Aluminum on Microstructure and Properties of As-Cast Nickel-Aluminum-Bronze Alloy AITranslate

1.State Key Laboratory of Nonferrous Metal Materials Preparation and Processing,GRIMAT Engineering Institute Co.,Ltd.,Beijing 101407,China
2.GRIMAT Engineering Institute Co.,Ltd.,Beijing 101407,China
3.General Research Institute for Nonferrous Metals,Beijing 100088,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nickel aluminum bronze (NAB)alloy has been widely used in marine propellers,seawater pumps,seawater pipes,and other components because of its good mechanical properties,excellent seawater corrosion resistance,welding performance,and marine microbial adhesion inhibition. It is the core material of marine engineering. However,there are many problems such as pore defects,component segregation,and uneven structure in casting NAB alloy,which have adverse effects on its mechanical properties and corrosion resistance,resulting in various corrosion problems of parts in highly corrosive marine environment. With the marine resources development and the implementation of the strategy of marine power,marine materials need to face the environment become more complicated,at this stage for the ascension of the corrosion resistance of NAB alloy,mainly concentrated in two aspects of foundry processing and surface modification,although in the above two aspects have clear process,However,the process and product of casting processing technology have poor controllability,and the surface modification has high requirements for operation. The existing methods all have certain disadvantages. The solution is to use different alloying elements to modify the properties of alloys,which is a method to fundamentally change the structure and properties of materials,and can solve the problems existing in the traditional method. Because there is no definite scope of the influence of alloy composition on the properties of NAB alloy,with the wide application of NAB,the composition and content of alloying elements need to be adjusted according to the actual demand,so the modification method of alloying elements has good extensibility and better application prospect. NAB alloys usually contain Cu,Al,Ni,Fe,and Mn elements. At present,the research on alloying elements mainly focuses on Ni and Fe elements,and the research on Al element is too little. Therefore,based on the composition of the commonly used cast NAB alloy (ZCuAl9-4-4-2),by changing the content of Al,two NAB alloys with different Al contents were prepared. Metallographic electron microscopy (OM),scanning electron microscopy (SEM),X-ray diffraction (XRD),tensile test,Vickers hardness test,uniform corrosion,and electrochemical impedance spectroscopy were used. The microstructure,mechanical properties, and corrosion behavior of as-cast NAB alloys with different Al content in 3.5% (mass fraction)NaCl solution were studied. The influence of Al content on microstructure and phase composition of the alloys was analyzed. The mechanical properties and static corrosion properties of the NAB alloys with different Al content were studied. To explore the relationship between Al content and microstructure and properties. The internal relationship between the microstructure change caused by the change of Al content and the mechanical and corrosion properties were systematically studied. The results showed that the morphology of α phase in matrix and κ phase of intermetallic compound changed with the increase of Al content in NAB alloy,showing distinct microstructure. With the increase of Al content,the morphology of α phase in matrix and intermetallic compound κ phase changed,which promoted the precipitation of a large amount of eutectoid κⅢ phase in α phase,and the κ phase was unevenly distributed from grain boundary to grain interior. As a result,the tensile strength,yield strength,and hardness of the alloy were improved. The elongation of the alloy decreases while the content of α phase decreased. With the increase of Al content in NAB alloy,the content of α phase in matrix with good plasticity decreased,and the hard phase with good strength increased. Therefore,the tensile strength,yield strength,and hardness all showed an upward trend,while the elongation significantly decreased. The static corrosion resistance of NAB alloy could be improved significantly with the decrease of Al content. After 30 days of soaking in 3.5% NaCl solution,the weight loss of 8Al alloy was about 54% lower than that of 10Al alloy,and the corrosion rate decreased from 0.0136 to 0.0068 mm·a−1. According to the results of electrochemical experiments,the corrosion resistance of the alloy was gradually improved with the increase of immersion time. After 30 days of immersion in 3.5% NaCl solution,the NAB alloy with lower Al content had higher polarization resistance and better corrosion resistance. The reduction of Al content could also reduce the local corrosion depth of NAB alloy. The surface film of Cu2O was generated in the initial stage,and the black CuO outer layer was further oxidized with the extension of soaking time. The outer layer of basic copper chloride was generated with the extension of soaking time,and the surface film of 8Al alloy was more dense and better protective. The low corrosion resistance of NAB alloy with increased Al content was mainly due to the formation of a large amount of α+κⅢ eutectoid structure,which increased the tendency of phase selection corrosion,and the α phase was more prone to corrosion. The addition of Al significantly promoted the formation of α+κⅢ eutectoid structure,so the NAB alloy with lower Al content had higher polarization resistance and better corrosion resistance.

KeyWords AITranslate

nickel aluminum bronze aluminum corrosion resistance electrochemical impedance spectroscopy corrosion products

[1](聂薇,姚晓红,卢本才. 海洋工程重防腐技术 [J]. 造船技术,2016,21(6):82.)

W Nie,X H Yao,B C Lu. Technical of heavy-duty coatings for marine engineering [J]. Mar. Technol.,2016,21(6):82.

[2](祝儒飞,刘宇宁,张嘉凝,莫永达,王虎,娄花芬. 蚀刻与冲压用铜合金板带的分条变形及应力分布 [J]. 稀有金属,2023,47(7):995.)

R F Zhu,Y N Liu,J N Zhang,Y D Mo,H Wang,H F Lou. Slitting deformation and stress distribution of copper alloy strip for etching and stamping [J]. Chinese Journal of Rare Metals,2023,47(7):995.

[3](葛业豹,张春雨,缑瑞宾,于敏. 应变速率对T2紫铜热变形行为的影响[J].塑性工程学报,2023,30(11):106.)

Y B Ge,C Y Zhang,R B Gou,M Yu. Influence of strain rate on thermal deformation behavior of T2 pure copper [J].Journal of Plasticity Engineering,2023,30(11):106.

[4](侯保荣,路东柱. 我国腐蚀成本及其防控策略[J].中国科学院院刊,2018,33(6):601.)

B R Hou,D Z Lu. Corrosion cost and prevention strategies in China [J]. Bulletin of Chinese Academy of Sciences,2018,33(6):601.

[5](付利国,周铁柱,苑伟,马俊普,周振亚,王伟波. 大规格铜镍合金凸缘热挤压成形工艺 [J].锻压技术,2023,48(4):169.)

L G Fu,T Z Zhou,W Yuan,J P Ma,Z Y Zhou,W B Wang. Hot extrusion forming process of large-size copper-nickel alloy flange [J]. Forging & Stamping Technology,2023,48(4):169.

[6](丁阳. 镍铝青铜合金应力腐蚀开裂及腐蚀疲劳行为的微观机理研究 [D]. 上海:上海交通大学,2019.1.)

Y Ding. Study on Microstructure Mechanism of Stress Corrosion Cracking and Corrosion Fatigue Behavior of Ni-Al-Bronze Alloy [D]. Shanghai:Shanghai Jiao Tong University,2019. 1.

[7](潘一帆,郭桦,苑伟,刘乐乐,王军亮,马江南,郁炎. 海洋工程及船用ZCuAl9Fe4Ni4Mn2铜合金的腐蚀疲劳性能研究 [J].铜业工程,2023,(3):70.)

Y F Pan,H Guo,W Yuan,L L Liu,J L Wang,J N Ma,Y Yu. Corrosion fatigue properties of ZCuAl9Fe4Ni4Mn2 copper alloy for marine engineering[J].Copper Engineering,2023,(3):70.

[8](杨芬芬.镍铝青铜合金的成分优化与耐蚀机制 [D]. 大连:大连理工大学,2020.1.)

F F Yang. Composition Optimization and Corrosion Resistance Mechanism of Ni-Al-Bronze Alloy [D]. Dalian:Dalian University of Technology,2020.1.

[9]Meigh H J. Cast and wrought aluminum bronzes-properties,processes and structure [R]. London:Institute of Materials,2000. 1.

[10]Saud S N,Hamzah E,Abubakar T,Bakhsheshi-Rad H R,Zamri M,Tanemura M. Effects of Mnadditions the structure,mechanical properties,and corrosion behavior of Cu-Al-Ni shape memory alloys [J]. J. Mater. Eng. Perform.,2014,23(1):3619.

[11](秦真波. 镍铝青铜合金的腐蚀行为及其表面改性研究[D].上海:上海交通大学,2018. 1.)

Z B Qin. Study on Corrosion Behavior and Surface Modification of Ni-Al-Bronze Alloy [D]. Shanghai:Shanghai Jiao Tong University,2018. 1.

[12](景媛,黄晓飞,杨荣,李明芳,辛钢. 铝含量对镍铝青铜合金耐盐水腐蚀的影响[J].腐蚀与防护,2020,41(11):43.)

Y Jing,X F Huang,R Yang,M F Li,G Xin. Effect of aluminum content on corrosion resistance of nickel-Al-bronze alloy with salt water [J]. Corrosion and Protection,2020,41(11):43.

[13]Hasan F,Jahana A,Lorimer G W. The morphology,crystallography,and chemistry of phases in as-cast nickel-aluminum bronze [J]. Metallurgical Transactions A,1982,13(8):1337.

[14]Ananta P J. Effect of hot working on microstructure evolution of as-cast nickel aluminum bronze alloy [J]. Materials and Design,2014,60(8):233.

[15]Xu X,Lv Y,Hu M. Influence of second phases on fatigue crack growth behavior of nickel aluminum bronze [J]. International Journal of Fatigue,2016,82(5):579.

[16](JB/T7901-2001. 金属材料实验室均匀腐蚀全浸试验方法[S].)

JB/T7901-2001. Metals materials-uniform corrosion-methods of laboratory immersion testing[S].

[17](韩靓,李周,王胜玉,李思,王永如. 时效处理对超高强Cu-Ti合金腐蚀行为的影响 [J]. 粉末冶金材料科学与工程,2016,21(6):931.)

L Han,Z Li,S Y Wang,S Li,Y R Wang. Effect of aging on corrosion behavior of ultra-high strength Cu-Ti alloy [J]. Powder Metallurgy Materials Science and Engineering,2016,21(6):931.

[18]Zhang B B,Wang J Z,Yan F Y. Load-dependent tribocorrosion behaviour of nickel-aluminium bronze in artificial seawater [J]. Corrosion Science,2018,131(11):252.

[19](曾彦华. 热轧工艺对镍铝青铜组织及性能的影响 [D]. 大连:大连理工大学,2020.1.)

Y H Zeng. Effect of Hot Rolling Process on Microstructure and Properties of Nickel-Aluminum Bronze [D]. Dalian:Dalian University of Technology,2020. 1.

[20](赵蓉. 腐蚀产物膜对镍铝青铜腐蚀行为的影响 [D]. 上海:上海交通大学,2018. 1.)

R Zhao. Effect of Corrosion Product Film on Corrosion Behavior of Nickel-Aluminum Bronze [D]. Shanghai:Shanghai Jiao Tong University,2018. 1.

[21]Sadawy M M,Ghanem M. Grain refinement of bronze alloy by equal-channel angular pressing (ECAP)and its effect on corrosion behaviour [J]. Defence Technology,2016,12(4):316.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY22030004

Chinese Library Classification Number:TG174.2

Citation Information:

Nickel aluminum bronze (NAB)alloy has been widely used in marine propellers,seawater pumps,seawater pipes,and other components because of its good mechanical properties,excellent seawater corrosion resistance,welding performance,and marine microbial adhesion inhibition. It is the core material of marine engineering. However,there are many problems such as pore defects,component segregation,and uneven structure in casting NAB alloy,which have adverse effects on its mechanical properties and corrosion resistance,resulting in various corrosion problems of parts in highly corrosive marine environment. With the marine resources development and the implementation of the strategy of marine power,marine materials need to face the environment become more complicated,at this stage for the ascension of the corrosion resistance of NAB alloy,mainly concentrated in two aspects of foundry processing and surface modification,although in the above two aspects have clear process,However,the process and product of casting processing technology have poor controllability,and the surface modification has high requirements for operation. The existing methods all have certain disadvantages. The solution is to use different alloying elements to modify the properties of alloys,which is a method to fundamentally change the structure and properties of materials,and can solve the problems existing in the traditional method. Because there is no definite scope of the influence of alloy composition on the properties of NAB alloy,with the wide application of NAB,the composition and content of alloying elements need to be adjusted according to the actual demand,so the modification method of alloying elements has good extensibility and better application prospect. NAB alloys usually contain Cu,Al,Ni,Fe,and Mn elements. At present,the research on alloying elements mainly focuses on Ni and Fe elements,and the research on Al element is too little. Therefore,based on the composition of the commonly used cast NAB alloy (ZCuAl9-4-4-2),by changing the content of Al,two NAB alloys with different Al contents were prepared. Metallographic electron microscopy (OM),scanning electron microscopy (SEM),X-ray diffraction (XRD),tensile test,Vickers hardness test,uniform corrosion,and electrochemical impedance spectroscopy were used. The microstructure,mechanical properties, and corrosion behavior of as-cast NAB alloys with different Al content in 3.5% (mass fraction)NaCl solution were studied. The influence of Al content on microstructure and phase composition of the alloys was analyzed. The mechanical properties and static corrosion properties of the NAB alloys with different Al content were studied. To explore the relationship between Al content and microstructure and properties. The internal relationship between the microstructure change caused by the change of Al content and the mechanical and corrosion properties were systematically studied. The results showed that the morphology of α phase in matrix and κ phase of intermetallic compound changed with the increase of Al content in NAB alloy,showing distinct microstructure. With the increase of Al content,the morphology of α phase in matrix and intermetallic compound κ phase changed,which promoted the precipitation of a large amount of eutectoid κⅢ phase in α phase,and the κ phase was unevenly distributed from grain boundary to grain interior. As a result,the tensile strength,yield strength,and hardness of the alloy were improved. The elongation of the alloy decreases while the content of α phase decreased. With the increase of Al content in NAB alloy,the content of α phase in matrix with good plasticity decreased,and the hard phase with good strength increased. Therefore,the tensile strength,yield strength,and hardness all showed an upward trend,while the elongation significantly decreased. The static corrosion resistance of NAB alloy could be improved significantly with the decrease of Al content. After 30 days of soaking in 3.5% NaCl solution,the weight loss of 8Al alloy was about 54% lower than that of 10Al alloy,and the corrosion rate decreased from 0.0136 to 0.0068 mm·a−1. According to the results of electrochemical experiments,the corrosion resistance of the alloy was gradually improved with the increase of immersion time. After 30 days of immersion in 3.5% NaCl solution,the NAB alloy with lower Al content had higher polarization resistance and better corrosion resistance. The reduction of Al content could also reduce the local corrosion depth of NAB alloy. The surface film of Cu2O was generated in the initial stage,and the black CuO outer layer was further oxidized with the extension of soaking time. The outer layer of basic copper chloride was generated with the extension of soaking time,and the surface film of 8Al alloy was more dense and better protective. The low corrosion resistance of NAB alloy with increased Al content was mainly due to the formation of a large amount of α+κⅢ eutectoid structure,which increased the tendency of phase selection corrosion,and the α phase was more prone to corrosion. The addition of Al significantly promoted the formation of α+κⅢ eutectoid structure,so the NAB alloy with lower Al content had higher polarization resistance and better corrosion resistance.

quote

GB/T 7714-2015 [1] Huiyuan Deng, Haofeng Xie, Shuhui Huang, et al. Aluminum on Microstructure and Properties of As-Cast Nickel-Aluminum-Bronze Alloy[J]. Chinese Journal of Rare Metals, 2025, 49(6): 795-806. DOI:10.13373/j.cnki.cjrm.XY22030004.
MLA [1] Huiyuan Deng, et al., "Aluminum on Microstructure and Properties of As-Cast Nickel-Aluminum-Bronze Alloy." Chinese Journal of Rare Metals, vol. 49, no. 6, 2025, pp. 795-806, https://doi.org/10.13373/j.cnki.cjrm.XY22030004.
APA [1] Huiyuan Deng, Haofeng Xie, Shuhui Huang, & Xujun Mi. (2025). Aluminum on Microstructure and Properties of As-Cast Nickel-Aluminum-Bronze Alloy. Chinese Journal of Rare Metals, 49(6), 795-806. https://doi.org/10.13373/j.cnki.cjrm.XY22030004
IEEE [1] Huiyuan Deng, Haofeng Xie, Shuhui Huang, and Xujun Mi, "Aluminum on Microstructure and Properties of As-Cast Nickel-Aluminum-Bronze Alloy," Chinese Journal of Rare Metals, vol. 49, no. 6, pp. 795-806, 2025, doi: 10.13373/j.cnki.cjrm.XY22030004. keywords: {nickel aluminum bronze;aluminum;corrosion resistance;electrochemical impedance spectroscopy;corrosion products}