daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Recent Developments in Chemical Vapor Deposition of 2D Magnetic Transition Metal Chalcogenides Recent Developments in Chemical Vapor Deposition of 2D Magnetic Transition Metal Chalcogenides AITranslate

Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University; Nanyang Technological University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In recent years, two-dimensional (2D) magnetic transition metal chalcogenides (TMCs) have attracted tremendous research interests thanks to their intriguing properties that are essential in developing future electronic and spintronic devices in this modernizing era. This review aims to introduce recent developments in the preparation of 2D magnetic TMCs, especially chromium and iron-based chalcogenides, their structures, as well as the related intriguing magnetic phenomena. First, the common crystal structures of magnetic TMCs including both layered and nonlayered structures are introduced. Various chemical vapor deposition strategies for synthesizing 2D magnetic TMCs are then introduced with emphasis on the key synthesis parameters. Moreover, the intriguing physical properties associated with 2D TMCs such as magnetic anisotropy, thickness, and phase-dependent magnetic response as well as stability are summarized. Last but not least, challenges and future research directions are briefly discussed in light of recent advances in the field.

KeyWords AITranslate

twodimensional material transition metal chalcogenides chemical vapor deposition magnetic property crystal structure stability
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00425

Chinese Library Classification Number:

Citation Information:

In recent years, two-dimensional (2D) magnetic transition metal chalcogenides (TMCs) have attracted tremendous research interests thanks to their intriguing properties that are essential in developing future electronic and spintronic devices in this modernizing era. This review aims to introduce recent developments in the preparation of 2D magnetic TMCs, especially chromium and iron-based chalcogenides, their structures, as well as the related intriguing magnetic phenomena. First, the common crystal structures of magnetic TMCs including both layered and nonlayered structures are introduced. Various chemical vapor deposition strategies for synthesizing 2D magnetic TMCs are then introduced with emphasis on the key synthesis parameters. Moreover, the intriguing physical properties associated with 2D TMCs such as magnetic anisotropy, thickness, and phase-dependent magnetic response as well as stability are summarized. Last but not least, challenges and future research directions are briefly discussed in light of recent advances in the field.

quote

GB/T 7714-2015 [1] Bijun Tang, Dianyi Hu, Xiaoxu Zhao, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00425.
MLA [1] Bijun Tang, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00425.
APA [1] Bijun Tang, Dianyi Hu, Xiaoxu Zhao, Xiaowei Wang, & Zheng Liu. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00425
IEEE [1] Bijun Tang, Dianyi Hu, Xiaoxu Zhao, Xiaowei Wang, and Zheng Liu, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00425. keywords: {twodimensional material transition metal chalcogenides chemical vapor deposition magnetic property crystal structure stability}