daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Emergent Phenomena in Magnetic Two-Dimensional Materials and van der Waals Heterostructures Emergent Phenomena in Magnetic Two-Dimensional Materials and van der Waals Heterostructures AITranslate

Beijing Computational Science Research Center, Beijing 100193;Beijing Computational Science Research Center, Beijing 100193; Tsinghua University; Beijing Normal University; Tsinghua University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Two-dimensional (2D) materials and their van der Waals (vdW) heterostructures provide powerful platforms for exploring fascinating physical phenomena and implementing intriguing applications. The recent discovery of 2D magnetic materials opens up many exciting topics in the research of 2D materials. 2D magnetic materials not only exhibit diverse properties on their own, which can be effectively controlled via external stimuli, but also can serve as a part of vdW heterostructures, creating a variety of unprecedented properties and functionalities. The field of 2D magnetism has grown rapidly in the past few years. In this review, we summarize the recent progress on the emergent phenomena in this active field. We review the well-established understanding of typical 2D magnetic materials and the vdW heterostructures and introduce the manipulations of their magnetic properties. In addition, we discuss the interplay between magnetism and topology in some recently discovered 2D materials. Moreover, we also address the valley relevant physics and the topological spin textures in 2D magnetic materials. Finally, we highlight some future interests in this promising field.

KeyWords AITranslate

2D magnetic materials magnetic topological materials valleytronics topological spin textures van der Waals heterostructures
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.2c00419

Chinese Library Classification Number:

Citation Information:

Two-dimensional (2D) materials and their van der Waals (vdW) heterostructures provide powerful platforms for exploring fascinating physical phenomena and implementing intriguing applications. The recent discovery of 2D magnetic materials opens up many exciting topics in the research of 2D materials. 2D magnetic materials not only exhibit diverse properties on their own, which can be effectively controlled via external stimuli, but also can serve as a part of vdW heterostructures, creating a variety of unprecedented properties and functionalities. The field of 2D magnetism has grown rapidly in the past few years. In this review, we summarize the recent progress on the emergent phenomena in this active field. We review the well-established understanding of typical 2D magnetic materials and the vdW heterostructures and introduce the manipulations of their magnetic properties. In addition, we discuss the interplay between magnetism and topology in some recently discovered 2D materials. Moreover, we also address the valley relevant physics and the topological spin textures in 2D magnetic materials. Finally, we highlight some future interests in this promising field.

quote

GB/T 7714-2015 [1] Yang Li, Baishun Yang, Shengnan Xu, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.2c00419.
MLA [1] Yang Li, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.2c00419.
APA [1] Yang Li, Baishun Yang, Shengnan Xu, Bing Huang, & Wenhui Duan. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.2c00419
IEEE [1] Yang Li, Baishun Yang, Shengnan Xu, Bing Huang, and Wenhui Duan, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.2c00419. keywords: {2D magnetic materials magnetic topological materials valleytronics topological spin textures van der Waals heterostructures}