daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Triazine and Thiophene-Containing Conjugated Polymer Network Emitter-Based Solution-Processable Stable Blue Organic LEDs AITranslate

Banaras Hindu University; National Tsing Hua University; Banaras Hindu University; National Tsing Hua University; Banaras Hindu University; National Tsing Hua University; Banaras Hindu University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The development of solution-processable fluorescent materials with blue electroluminescence has recently attracted considerable research interest for organic light-emitting diode (OLED) applications. Whereas, conjugated polymer frameworks (CPFs) or networks (CPNs) have attained tremendous research interest due to their vast potential in a variety of cutting-edge applications including photocatalysis, sensing, gas storage, energy storage, and so on. These framework/network materials without side chains or functional groups on their backbone are generally insoluble in common organic solvents and less solution-processable for electronic device applications. Herein, we have reported two triazine-based highly fluorescent and wide-band gap donor–acceptor conjugated polymer networks (CPNs) by coupling a 3-substituted thiophene (donor) unit with a triazine ring (acceptor) through a phenyl ring spacer. Two different side chains, alkyl and oligoethylene glycol, are rationally introduced into the 3-position of thiophene in the polymer network to make them solution-processable. Further physicochemical and optoelectronic characterizations of these emitters are performed in detail, and the effects of the side chain functionality and polarity on the above-mentioned properties are also thoroughly investigated. OLEDs based on these CPNs as emitters show a maximum external quantum efficiency of 2.3% with a maximum brightness of 2541 cd/m2 and a maximum current efficiency of 2.8 cd/A with blue emission [Commission Internationale de l’éclairage (CIE) coordinates of (0.17, 0.19)]. To the best of our knowledge, this may be the first example of conjugated polymer network material emitters being successfully designed, fabricated, and tested for solution-processable blue OLEDs. These results also demonstrate the high potential of the conjugated polymer network emitters for future blue or other color OLED applications.

KeyWords AITranslate

conjugated polymer network emissive materials organic semiconductor organic lightemitting diode photoluminescence
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01337

Chinese Library Classification Number:

Citation Information:

The development of solution-processable fluorescent materials with blue electroluminescence has recently attracted considerable research interest for organic light-emitting diode (OLED) applications. Whereas, conjugated polymer frameworks (CPFs) or networks (CPNs) have attained tremendous research interest due to their vast potential in a variety of cutting-edge applications including photocatalysis, sensing, gas storage, energy storage, and so on. These framework/network materials without side chains or functional groups on their backbone are generally insoluble in common organic solvents and less solution-processable for electronic device applications. Herein, we have reported two triazine-based highly fluorescent and wide-band gap donor–acceptor conjugated polymer networks (CPNs) by coupling a 3-substituted thiophene (donor) unit with a triazine ring (acceptor) through a phenyl ring spacer. Two different side chains, alkyl and oligoethylene glycol, are rationally introduced into the 3-position of thiophene in the polymer network to make them solution-processable. Further physicochemical and optoelectronic characterizations of these emitters are performed in detail, and the effects of the side chain functionality and polarity on the above-mentioned properties are also thoroughly investigated. OLEDs based on these CPNs as emitters show a maximum external quantum efficiency of 2.3% with a maximum brightness of 2541 cd/m2 and a maximum current efficiency of 2.8 cd/A with blue emission [Commission Internationale de l’éclairage (CIE) coordinates of (0.17, 0.19)]. To the best of our knowledge, this may be the first example of conjugated polymer network material emitters being successfully designed, fabricated, and tested for solution-processable blue OLEDs. These results also demonstrate the high potential of the conjugated polymer network emitters for future blue or other color OLED applications.

quote

GB/T 7714-2015 [1] Neelam Gupta, Mangey Ram Nagar, Anamika, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01337.
MLA [1] Neelam Gupta, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01337.
APA [1] Neelam Gupta, Mangey Ram Nagar, Anamika, Prakalp Gautam, Biswajit Maiti, JwoHuei Jou, & Biplab Kumar Kuila. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01337
IEEE [1] Neelam Gupta, Mangey Ram Nagar, Anamika, Prakalp Gautam, Biswajit Maiti, JwoHuei Jou, and Biplab Kumar Kuila, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01337. keywords: {conjugated polymer network;emissive materials;organic semiconductor;organic lightemitting diode;photoluminescence}