Effect of Fluorinated Substituents on Solubility and Dielectric Properties of the Liquid Crystalline Poly(ester imides) AITranslate

South China University of Technology;Kingfa Science and Technology, Company, Ltd.; PR China|Key Laboratory of Polymer Processing Engineering (South China University of Technology); PR China|Key Laboratory of Polymer Processing Engineering (South China University of Technology); PR China|Key Laboratory of Polymer Processing Engineering (South China University of Technology)
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

With the rapid advancement of 5G communication technology, much attention has been paid on high-performance polymers with a low dielectric constant (Dk), a low dielectric loss (Df) and good processability. In order to further research and improve dielectric properties of the liquid crystalline poly(ester imide)s (LCPEIs), four imide dicarboxylic acids (IAs) with fluorinated groups are designed and synthesized. They are then copolymerized with 1,3-phthalic acid (IPA), p-hydroxybenzoic acid (HBA), and bisphenol monomers via solution polycondensation to obtain fluorinated PEIs, whose fluorine content, position of the fluorinated group, and LC behavior are tunable by using different IAs and bisphenol monomers. These PEIs with the highest Tg of 238 °C are soluble in general organic solvents, such as m-cresol, N-methyl-2-pyrrolidone (NMP), chloroform, and so on. PEI-6F25AF exhibits the lowest Dk of 2.60, while LCPEI-6FD shows the lowest Df of 0.0053 at 10 GHz. It is found that high fluorine content and large pendent group can reduce the Dk, while the fluorinated group grafted close to the nitrogen atom and the LC rigid rod-like conformation lead to low Df. We devoutly expect that this research offers some reference for structure design of LCPEIs with both low Dk and Df at high frequency.

KeyWords AITranslate

poly(ester imide)s fluorinated polymers liquid crystalline polymers dielectric constant (Dk) dielectric loss (Df)
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01358

Chinese Library Classification Number:

Citation Information:

With the rapid advancement of 5G communication technology, much attention has been paid on high-performance polymers with a low dielectric constant (Dk), a low dielectric loss (Df) and good processability. In order to further research and improve dielectric properties of the liquid crystalline poly(ester imide)s (LCPEIs), four imide dicarboxylic acids (IAs) with fluorinated groups are designed and synthesized. They are then copolymerized with 1,3-phthalic acid (IPA), p-hydroxybenzoic acid (HBA), and bisphenol monomers via solution polycondensation to obtain fluorinated PEIs, whose fluorine content, position of the fluorinated group, and LC behavior are tunable by using different IAs and bisphenol monomers. These PEIs with the highest Tg of 238 °C are soluble in general organic solvents, such as m-cresol, N-methyl-2-pyrrolidone (NMP), chloroform, and so on. PEI-6F25AF exhibits the lowest Dk of 2.60, while LCPEI-6FD shows the lowest Df of 0.0053 at 10 GHz. It is found that high fluorine content and large pendent group can reduce the Dk, while the fluorinated group grafted close to the nitrogen atom and the LC rigid rod-like conformation lead to low Df. We devoutly expect that this research offers some reference for structure design of LCPEIs with both low Dk and Df at high frequency.

quote

GB/T 7714-2015 [1] Wenxiang Zhang, Zhongquan Peng, Qiwei Pan, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01358.
MLA [1] Wenxiang Zhang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01358.
APA [1] Wenxiang Zhang, Zhongquan Peng, Qiwei Pan, Shumei Liu, & Jianqing Zhao. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01358
IEEE [1] Wenxiang Zhang, Zhongquan Peng, Qiwei Pan, Shumei Liu, and Jianqing Zhao, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.2c01358. keywords: {poly(ester imide)s;fluorinated polymers;liquid crystalline polymers;dielectric constant (Dk);dielectric loss (Df)}