Effects of Ce Modification on NH3-SCR Denitration Performance of Activated Rare Earth Tailings Catalyst AITranslate

Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Bayan Obo rare earth tailings are composed of hematite,bastnasite,fluorite,quartz and magnetite,in which rare earth element Ce and transition metals Fe,Mn are the active elements required for catalyst.In this paper,activated rare earth tailings were modified by Ce using impregnation method,and the effects of Ce modification on the performance of activated rare earth tailings catalyst were investigated by SEM-EDS,XRD,BET,NH3-TPD,H2-TPR and XPS.The results show that the Ce-modified activated rare earth tailings catalyst is dominated by mesoporous structure and Ce element is highly dispersed on the catalyst surface.There is a synergistic effect between Ce and Fe,and the existence of a redox couple between them promotes the transformation between different valence states of Ce and Fe ions,enhances the redox ability of the catalyst and increases the number of acid sites,which provides favorable environment for the adsorption and activation of NH3,improving the denitration efficiency of the catalyst.After being modified by 15%Ce,the denitration efficiency of the activated rare earth tailings increases from 70%to 82%,the N2selectivity is above 90%,and the reaction temperature window is widened to 275~450℃.

KeyWords AITranslate

rare earth tailings denitration catalyst activation Ce modification impregnation NH3-SCR

1梁文俊,李庆磊,任思达.酸预处理对整体式催化剂载体性能的影响研究[J].中国环境科学,2020,40(12):5237-5245. 被引量:5

2夏岩,詹望成,郭耘,郭杨龙,卢冠忠.Fe-Beta分子筛催化剂在选择催化还原氮氧化物反应中的活性:Fe含量的影响(英文)[J].催化学报(英文),2016,37(12):2069-2078. 被引量:9

3陈亮,李俊华,葛茂发,马磊,常化振.CeO2-WO3复合氧化物催化剂的NH_3-SCR反应机理(英文)[J].催化学报(英文),2011,32(5):836-841. 被引量:18

4边雪,肖坤宇,王书豪,邱保龙.Fe、Ce改性锰钛催化剂的制备及其低温脱硝性能研究[J].功能材料,2019,0(7):7079-7084. 被引量:8

5赵毅,孙中豪,曾韵洁.低温SCR脱硝催化剂的研究进展[J].化工环保,2019,39(1):1-5. 被引量:18

1杨建军.加氢催化剂及其产物中Mo元素含量测定[J].石化技术,2023,30(2):42-44.

2尹传辉,李康,陈诚.“铁及其重要化合物”微项目教学——贫血该怎么办[J].中学化学教学参考,2023(9):25-29.

3阎清华,王爱斌,高洁,刘国成,辛言君.Ce_(2)/Cu_(4)Al_(1)O_(x)催化剂的脱硝性能及PbCl_(2)耐受性[J].化工环保,2023,43(2):241-246.

4李秋,朱翔,耿海宁,李宗刚,马浩森,陈伟.地聚合物基多相陶瓷高放废液固化体固化机理与浸出性能[J].硅酸盐通报,2023,42(4):1437-1447. 被引量:1

5周怡璇,马丹丹,石建稳.铜离子价态对铜基催化剂光/电催化CO_(2)还原性能影响的研究进展[J].材料工程,2023,51(4):15-28.

6李延吉,赵明,李明泽,宋瑞雯.改性HZSM-5催化玉米秸秆与HDPE共热解制轻质芳烃[J].太阳能学报,2023,44(4):238-246.

7杨华,杨幸川,徐丽,曹春梅,刘国际.不同A位取代Co基尖晶石纳米线阵列的合成及其催化碳烟消除的研究[J].现代化工,2023,43(3):98-105.

8王永强,王勇,唐菊兴,贺传凯,王海勇,闫鹏刚,冯翼鹏.西藏帮布勒矽卡岩型铅锌矿床闪锌矿化学成分特征及其地质意义[J].地球学报,2023,44(3):485-497.

9徐春生,李雨清,刘威,周彬,程传,陆冠旗,姚欢.CuCe双金属氧化物催化剂催化氧化丙烯腈废气的性能研究[J].合成材料老化与应用,2022,51(6):34-37.

10张家宇,孙娜,凌丽霞,章日光,贾丽涛,李德宝,王宝俊.不同价态金属掺杂对La_(2)O_(3)(001)表面上甲烷活化影响的研究[J].燃料化学学报(中英文),2023,51(5):673-683.

Basic Information:

DOI:

Chinese Library Classification Number:TD983[矿业工程—选矿]

Citation Information:

Bayan Obo rare earth tailings are composed of hematite,bastnasite,fluorite,quartz and magnetite,in which rare earth element Ce and transition metals Fe,Mn are the active elements required for catalyst.In this paper,activated rare earth tailings were modified by Ce using impregnation method,and the effects of Ce modification on the performance of activated rare earth tailings catalyst were investigated by SEM-EDS,XRD,BET,NH3-TPD,H2-TPR and XPS.The results show that the Ce-modified activated rare earth tailings catalyst is dominated by mesoporous structure and Ce element is highly dispersed on the catalyst surface.There is a synergistic effect between Ce and Fe,and the existence of a redox couple between them promotes the transformation between different valence states of Ce and Fe ions,enhances the redox ability of the catalyst and increases the number of acid sites,which provides favorable environment for the adsorption and activation of NH3,improving the denitration efficiency of the catalyst.After being modified by 15%Ce,the denitration efficiency of the activated rare earth tailings increases from 70%to 82%,the N2selectivity is above 90%,and the reaction temperature window is widened to 275~450℃.

quote

GB/T 7714-2015 [1] HOU Li-min, XU Jie, WANG Tian-tian, et al. Effects of Ce Modification on NH3-SCR Denitration Performance of Activated Rare Earth Tailings Catalyst[J]. Rare Metals and Cemented Carbides, 2023(2): 60-67.
MLA [1] HOU Li-min, et al., "Effects of Ce Modification on NH3-SCR Denitration Performance of Activated Rare Earth Tailings Catalyst." Rare Metals and Cemented Carbides, no. 2, 2023, pp. 60-67.
APA [1] HOU Li-min, XU Jie, WANG Tian-tian, QIAO Chao-yue, CHEN Han, FU Shan-cong, & WU Wen-fei. (2023). Effects of Ce Modification on NH3-SCR Denitration Performance of Activated Rare Earth Tailings Catalyst. Rare Metals and Cemented Carbides(2), 60-67.
IEEE [1] HOU Li-min, XU Jie, WANG Tian-tian, QIAO Chao-yue, CHEN Han, FU Shan-cong, and WU Wen-fei, "Effects of Ce Modification on NH3-SCR Denitration Performance of Activated Rare Earth Tailings Catalyst," Rare Metals and Cemented Carbides, no. 2, pp. 60-67, 2023. keywords: {rare earth tailings;denitration catalyst;activation;Ce modification;impregnation;NH-SCR}