Development of W Ion-exchange New Technology AITranslate

Xiamen Tungsten Industry Co., Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

W ion exchange new technology is based on the different absorption power of strongly basic-anion exchange resin for different ions in the sodium tungstate and based on the characteristics that the ions with high affinity can be replaced by distinct increase of concentration of ions with low affinity for resin for the purpose of impurity separation and W purification.Through over 20 years of continuous improvement,this technology has become a perfect ion exchange technology for W.

KeyWords AITranslate

ion exchange resin sodium tungstate solution purification by ion exchange technological progress

1胡兆瑞.离子交换法在钨冶炼中的应用[J].中国钨业,1994,0(5):1-4. 被引量:9

2肖连生,张启修,龚柏藩,黄芍英.密实移动床——流化床离子交换除钼技术在工业上的应用[J].中国钨业,2001,16(2):26-29. 被引量:21

3胡兆瑞.离子交换法冶炼钨工艺的诞生和发展[J].中国钨业,1997,0(Z1):42-44. 被引量:11

1宋阜,朱宾权.离子交换法分离富集钨酸钠溶液中的钒[J].稀有金属与硬质合金,2006,34(3):5-7. 被引量:14

2关文娟,张贵清.用季铵盐从模拟钨矿苏打浸出液中直接萃取钨[J].中国有色金属学报,2011,21(7):1756-1762. 被引量:22

3李会强,唐忠阳,何利华,陈星宇.离子交换技术在钨冶金中的应用与进展[J].中国钨业,2014,29(5):34-39. 被引量:13

4陈世梁,张贵清,肖连生,关文娟.采用HCO_3^--CO_3^(2-)混合型季铵盐从模拟钨矿苏打高压浸出液中萃取钨[J].中国有色金属学报,2014,24(12):3155-3161. 被引量:10

5黄万抚,李新冬,文金磊,陈园园,梁娟.HD325树脂从低浓度稀土矿浸出液中回收稀土的研究[J].稀有金属,2015,39(8):727-734. 被引量:17

6李嘉豪,曹佐英,李嘉,张贵清,肖连生,李青刚.新型胺类萃取剂N1633萃取钨的研究[J].矿冶工程,2018,38(2):74-78.

7业界首个90毫微米CMOS设计平台面市[J].电子工程师,2002,28(10):9-9.

1刘黎慧,周朝昕,杨洪升,杨笑松,陈文忠.FeSO4还原混凝法处理奥里油电厂含钒废水[J].安全与环境工程,2009,16(3):45-49. 被引量:3

2赵卓,李小斌,赵清杰.树脂离子交换提取拜耳法流程中钒的动力学[J].过程工程学报,2009(3):462-467. 被引量:7

3ZHAO Zhuo,LI Xiaobin,ZHAO Qingjie.Recovery of V_2O_5 from Bayer liquor by ion exchange[J].稀有金属:英文版,2010,0(2):115-120. 被引量:3

4柯兆华,张贵清,关文娟,尚广浩.季铵盐从碱性钨酸钠溶液中萃取钨的研究[J].稀有金属与硬质合金,2012,40(6):1-4. 被引量:10

5关文娟,张贵清,高从堦.蒸发脱氨络合法制备的双氧水络合萃取分离钨钼前驱体料液(英文)[J].中国有色金属学报:英文版,2013,23(4):1139-1146. 被引量:5

6关文娟,张贵清,高从堦,尚广浩.双氧水络合萃取分离钨钼的前驱体料液的制备[J].中南大学学报:自然科学版,2013,44(5):1766-1774. 被引量:4

7曾之琪,肖连生,张贵清.碱性钨萃余液返回高压浸出的试验研究[J].稀有金属与硬质合金,2013,41(6):1-6. 被引量:1

8张魁芳,曹佐英,张贵清,肖连生,周小舟.甲基碳酸酯季铵盐的合成、转型及萃取性能[J].中国有色金属学报,2013,23(12):3529-3536. 被引量:1

9赵长多,杨晓博,范美玲,胡文斌,夏启斌.纳米零价铁对水溶液中钒离子的吸附性能[J].过程工程学报,2018,18(6):1253-1260.

10李嘉豪,曹佐英,李嘉,张贵清,李青刚,曾理,关文娟.高级脂肪胺类萃取剂在稀有金属溶剂萃取中的应用[J].稀有金属与硬质合金,2018,46(6):10-18. 被引量:1

1离子交换法净化三价铬镀液[J].国际表面处理,2000(4):66-67.

2陈修海,侯巧荣.论三聚氰胺生产工艺技术的改进措施[J].中国石油和化工标准与质量,2011,31(10):74-75.

3刘伟,乔聪震,张兆麟.纯盐酸生产中离子交换除铁工艺研究[J].河南化工,1995,14(10):10-11. 被引量:7

4张萍,蒋馥华.苛化泥为焙烧添加剂从石煤提取五氧化二钒[J].稀有金属,2000,24(2):115-118. 被引量:15

5杨守生.沉淀法从高铁锰的钴溶液中分离杂质[J].山东化工,1999,28(5):5-7.

6尹国强,崔英德,廖列文,崔亦华.氯化胆碱合成工艺研究[J].广州化工,2000,28(4):56-58. 被引量:5

7陈英.硫酸锰中钙镁的测定[J].饲料工业,2006,27(1):49-49. 被引量:3

8胡祖福.常州一步混合设备深受好评[J].机电信息,2017,0(11):57-57.

9谢祖芳,朱万仁,陈渊,晏全,周振,何雪玲.强碱性阴离子交换树脂对苦味酸的吸附与解吸性能[J].化工环保,2011,31(2):104-109. 被引量:2

10杨彩娟,邵利,许春建,周明.浆料催化精馏酯交换合成碳酸二甲酯[J].石油化工,2006,35(2):132-135. 被引量:10

Basic Information:

DOI:

Chinese Library Classification Number:TQ028.37[化学工程]

Citation Information:

W ion exchange new technology is based on the different absorption power of strongly basic-anion exchange resin for different ions in the sodium tungstate and based on the characteristics that the ions with high affinity can be replaced by distinct increase of concentration of ions with low affinity for resin for the purpose of impurity separation and W purification.Through over 20 years of continuous improvement,this technology has become a perfect ion exchange technology for W.

quote

GB/T 7714-2015 [1] HUANG Cheng-tong. Development of W Ion-exchange New Technology[J]. Rare Metals and Cemented Carbides, 2003(3): 37-41.
MLA [1] HUANG Cheng-tong. "Development of W Ion-exchange New Technology." Rare Metals and Cemented Carbides, no. 3, 2003, pp. 37-41.
APA [1] HUANG Cheng-tong. (2003). Development of W Ion-exchange New Technology. Rare Metals and Cemented Carbides(3), 37-41.
IEEE [1] HUANG Cheng-tong, "Development of W Ion-exchange New Technology," Rare Metals and Cemented Carbides, no. 3, pp. 37-41, 2003. keywords: {ion exchange resin;sodium tungstate solution;purification by ion exchange;technological progress}