Abstract AITranslate
Analysis is made of the influence factors of the tunsten wire low-temperatare ductility in respect of the raw matcrial purity,additive content and technological conditions,Corresponding improvement measures are presented.
KeyWords AITranslate
1刘光耀.掺杂钨丝生产工艺的改进研究[J].稀有金属与硬质合金,1997,25(2):26-29. 被引量:3
2白淑文 等.钨铝丝加工原理[M].北京:轻工业出版社,1983..
1侯玉柏,丁舜,解峰,丁尉骑,刘山宇.微量SiO_2对钍钨合金烧结性能的影响[J].矿冶,2018,27(4):55-60.
1蒋显亮,左铁镛.掺杂钨丝再结晶机理的研究[J].中南矿冶学院学报,1989,20(3):276-280.
2张存信,张树格,田华,林勇.加热温度对掺杂钨丝再结晶组织及性能的影响[J].热处理技术与装备,2007,28(1):15-17.
3张存信,张树格,田华,林勇.加热温度对掺杂钨丝再结晶组织和性能的影响[J].兵器材料科学与工程,2005,28(6):37-39.
4钟伯明,魏嘉荃,贺杰,李其.《低温延性断裂韧度J_(IC)测试技术》J=J_(IC)的工程应用[J].大庆石油学院学报,1990,14(4):122-132.
5钟伯明,魏嘉荃,贺杰.《低温延性断裂韧度J_(IC)测试技术》J=J_(IC)的理论基础[J].大庆石油学院学报,1990,14(4):114-121. 被引量:1
6板垣孟彦,陈润甫.掺杂钨丝中镍诱发再结晶和镍的扩散渗透[J].钨钼材料,1992(4):30-34.
7范荣奎,陈安庆.掺杂钨丝性能与拉伸工艺的关系[J].钨钼材料,1993(3):36-44.
8陈中春,周美玲,左铁镛.掺杂钨丝的再结晶[J].中南矿冶学院学报,1989,20(4):421-427.
9王龙滨,朱恩科,王增民.掺杂钨丝抗拉强度对其绕丝性能的影响[J].中国钨业,2003,18(3):21-23. 被引量:2
10殷为宏,郑汉,张德尧.钨和钨合金的新发展(Ⅱ)——钨合金和高纯钨[J].稀有金属材料与工程,1990(3):2-11. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TG111.91[金属学及工艺—物理冶金]
Citation Information:
Analysis is made of the influence factors of the tunsten wire low-temperatare ductility in respect of the raw matcrial purity,additive content and technological conditions,Corresponding improvement measures are presented.
quote
| GB/T 7714-2015 | [1] FAN Jun-xian. Influence Factors and Improvement of Low-temperature Ductility of Doped Tungsten Wire[J]. Rare Metals and Cemented Carbides, 2003(3): 42-44. |
| MLA | [1] FAN Jun-xian. "Influence Factors and Improvement of Low-temperature Ductility of Doped Tungsten Wire." Rare Metals and Cemented Carbides, no. 3, 2003, pp. 42-44. |
| APA | [1] FAN Jun-xian. (2003). Influence Factors and Improvement of Low-temperature Ductility of Doped Tungsten Wire. Rare Metals and Cemented Carbides(3), 42-44. |
| IEEE | [1] FAN Jun-xian, "Influence Factors and Improvement of Low-temperature Ductility of Doped Tungsten Wire," Rare Metals and Cemented Carbides, no. 3, pp. 42-44, 2003. keywords: {doped tungsten wire;low-temperatare ductility;influence factors;improvement measure} |