Network Topology of the Interphase between Cross-Linked Polyurethane/Ethylene Propylene Diene Terpolymer Elastomers for Adhesion Applications AITranslate

ArianeGroup, Centre de Recherches du Bouchet;ArianeGroup, Centre de Recherches du Bouchet; Sorbonne Université
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Understanding the interfacial phenomena involved in the adhesion between elastomer layers on a molecular basis is an important topic from both fundamental and applied aspects. Nevertheless, this topic has been poorly addressed experimentally. This report aims at rationalizing differences in the adhesion behavior of polyurethane (PU) elastomers cured on an ethylene–propylene–diene terpolymer (EPDM) substrate, based on a detailed description of their local network-like topology, determined thanks to 1H solid-state nuclear magnetic resonance (NMR) spectroscopy. The polyurethanes, composed of the same fraction of hydroxy-terminated poly(butadiene) and isophorone diisocyanate, were cured under different reaction conditions: nature and concentration of the catalyst as well as the cross-linking temperature. The rigid domains formed by the hard segments, the proportion of elastically active chains, and the distribution of the topological constraints in the soft domains were investigated by 1H solid-state NMR, taking advantage of the magic sandwich echoes and double quantum-based experiments. The PU network topology within 20 μm thick slices collected near the interface with the EPDM layer was systematically compared to the one observed for 60 μm thick slices, located 500 μm from the interface, corresponding to the bulk regions. Curing at a low temperature (30 °C) with a low amount of catalyst (0.02 wt %) leads to elastically active poly(butadiene) chains close to the interface with, on average, higher molecular weights between topological constraints than the ones in the bulk. Such differences between interfacial and bulk regions are not observed any longer as the catalyst concentration is increased to 0.2 wt %. These variations of the local PU network topology, occurring over several tens of micrometers, allow one to account for the adhesion testing results.

KeyWords AITranslate

polyurethane network topology interfaces elastomer bonding solidstate NMR
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.3c01458

Chinese Library Classification Number:

Citation Information:

Understanding the interfacial phenomena involved in the adhesion between elastomer layers on a molecular basis is an important topic from both fundamental and applied aspects. Nevertheless, this topic has been poorly addressed experimentally. This report aims at rationalizing differences in the adhesion behavior of polyurethane (PU) elastomers cured on an ethylene–propylene–diene terpolymer (EPDM) substrate, based on a detailed description of their local network-like topology, determined thanks to 1H solid-state nuclear magnetic resonance (NMR) spectroscopy. The polyurethanes, composed of the same fraction of hydroxy-terminated poly(butadiene) and isophorone diisocyanate, were cured under different reaction conditions: nature and concentration of the catalyst as well as the cross-linking temperature. The rigid domains formed by the hard segments, the proportion of elastically active chains, and the distribution of the topological constraints in the soft domains were investigated by 1H solid-state NMR, taking advantage of the magic sandwich echoes and double quantum-based experiments. The PU network topology within 20 μm thick slices collected near the interface with the EPDM layer was systematically compared to the one observed for 60 μm thick slices, located 500 μm from the interface, corresponding to the bulk regions. Curing at a low temperature (30 °C) with a low amount of catalyst (0.02 wt %) leads to elastically active poly(butadiene) chains close to the interface with, on average, higher molecular weights between topological constraints than the ones in the bulk. Such differences between interfacial and bulk regions are not observed any longer as the catalyst concentration is increased to 0.2 wt %. These variations of the local PU network topology, occurring over several tens of micrometers, allow one to account for the adhesion testing results.

quote

GB/T 7714-2015 [1] Nancy Desgardin, Agnès Aymonier, Cédric Lorthioir. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01458.
MLA [1] Nancy Desgardin, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01458.
APA [1] Nancy Desgardin, Agnès Aymonier, & Cédric Lorthioir. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01458
IEEE [1] Nancy Desgardin, Agnès Aymonier, and Cédric Lorthioir, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01458. keywords: {polyurethane;network topology;interfaces;elastomer bonding;solidstate NMR}