Self-immolative polymers (SIPs) allow a triggered depolymerization, which is an effective way to control the function of polymer-based systems. In this work, hydrophobic SIP segments and hydrophilic polyethylene glycol (PEG) are combined in diblock and triblock amphiphilic architectures, and the SIP-based blocks are made of polycaprolactone-like backbones with UV-sensitive nitrobenzene pendant groups. The depolymerization of the designed architectures in solution is monitored by NMR, UV–vis spectroscopy, and size exclusion chromatography, showing complete cleavage of the triggering units in the SIP parts after about 25 min under UV irradiation and depolymerization rates of the SIP backbones up to 60%. Self-assemblies are prepared from the diblock copolymers, their stability is verified by DLS, and the UV-triggered disintegration of the self-assemblies is demonstrated by SEM, Tindall effect, and by monitoring the derived count rate in DLS, showing a rapid disintegration (after 2 to 6 min under UV light). These SIP-based structures allow a fast, controlled, and on-demand disintegration of self-assemblies, with the ability to encapsulate and release on-demand the Nile red as a hydrophobic model molecule.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.3c01421
Chinese Library Classification Number:
Citation Information:
Self-immolative polymers (SIPs) allow a triggered depolymerization, which is an effective way to control the function of polymer-based systems. In this work, hydrophobic SIP segments and hydrophilic polyethylene glycol (PEG) are combined in diblock and triblock amphiphilic architectures, and the SIP-based blocks are made of polycaprolactone-like backbones with UV-sensitive nitrobenzene pendant groups. The depolymerization of the designed architectures in solution is monitored by NMR, UV–vis spectroscopy, and size exclusion chromatography, showing complete cleavage of the triggering units in the SIP parts after about 25 min under UV irradiation and depolymerization rates of the SIP backbones up to 60%. Self-assemblies are prepared from the diblock copolymers, their stability is verified by DLS, and the UV-triggered disintegration of the self-assemblies is demonstrated by SEM, Tindall effect, and by monitoring the derived count rate in DLS, showing a rapid disintegration (after 2 to 6 min under UV light). These SIP-based structures allow a fast, controlled, and on-demand disintegration of self-assemblies, with the ability to encapsulate and release on-demand the Nile red as a hydrophobic model molecule.
quote
| GB/T 7714-2015 | [1] Ádám Viktor Joó, Jonathan Potier, Nouzha Ouhssou, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.3c01421. |
| MLA | [1] Ádám Viktor Joó, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.3c01421. |
| APA | [1] Ádám Viktor Joó, Jonathan Potier, Nouzha Ouhssou, Bárbara Pepino Mendes, Gaëlle Le Fer, Patrice Woisel, & Kedafi Belkhir. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.3c01421 |
| IEEE | [1] Ádám Viktor Joó, Jonathan Potier, Nouzha Ouhssou, Bárbara Pepino Mendes, Gaëlle Le Fer, Patrice Woisel, and Kedafi Belkhir, ACS Applied Polymer Materials, no. 5, 2023, doi: 10.1021/acsapm.3c01421. keywords: {triggered depolymerization;selfimmolative polymers;UVresponsive polymers;selfassemblies} |