Process Research on Vanadium Extraction from Stone Coal by High Temperature Curing and Column Leaching AITranslate

Xi'an Northwest Nonferrous Geological Research Institute Co.,LTD.;Xi'an Northwest Nonferrous Geological Research Institute Co.,LTD.;Xi'an Northwest Nonferrous Geological Research Institute Co.,LTD.;Xi'an Northwest Nonferrous Geological Research Institute Co.,LTD.;Xi'an Northwest Nonferrous Geological Research Institute Co.,LTD.;Xi'an Northwest Nonferrous Geological Research Institute Co.,LTD.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The extraction of vanadium from stone coal was carried out by the process of acid mixing pelleting,high temperature curing and column leaching.Also,the study discussed the leaching effect of vanadium from raw ore affected by process conditions such as the amount of sulfuric acid,the amount of water supplement for curing,the binder dosage,the curing temperature,the curing time,the particle size of the cured material and the spraying intensity.The results show that the leaching rate is 76.99%when the conditions of the process are as follows:The particle size of the raw ore is less than 12 mm;the water content of the raw ore is 10%;the amount of sulfuric acid is 20%;the binder dosage is 0.05%;the curing temperature is 135 C;the curing time is 10 h;the particle size of the cured material is less than 8 cm;the liquid-solid ratio of leaching section is 1.5:1;the spraying intensity is 15 L/(m2·h).After the leaching residue is washed four times(the liquid-solid ratio of washing section is 1.5:1),the leaching rate of vanadium can be increased to 87.48%,and the content of V2O5,in the tailings can be reduced to 0.11%.The research can provide important reference for the industrial production of the heap-leaching of vanadium ore.

KeyWords AITranslate

stone coal vanadium high temperature curing column leaching process condition

1申亚芳,张文,郝百川,王乐,李慧.湿法冶金过程中除铁工艺研究进展[J].矿产综合利用,2021(3):114-119. 被引量:2

2温永忠,魏巧生.浅析离子交换树脂中毒现象及解决对策[J].过滤与分离,2014,24(4):26-28. 被引量:7

3尹升华,陈勋.堆浸体系含水率的影响因素[J].中国有色金属学报,2015,25(7):1961-1968. 被引量:3

4梁建龙,刘慧娟,王清良,史文革,胡凯光,胡鄂明,李会娟.预处理—堆浸—石煤湿法冶金提钒新工艺[J].现代矿业,2013(1):111-113. 被引量:3

5万洪强,宁顺明,佘宗华,邢学永,王文娟,吴江华.石煤钒矿浓酸熟化浸出工艺优化[J].稀有金属,2014,38(5):880-886. 被引量:6

6万洪强,宁顺明,佘宗华,邢学永,封志敏.石煤钒矿拌酸熟化浸出新工艺[J].过程工程学报,2013,13(2):202-206. 被引量:13

7王明,程倩,齐建云,李洁,宁新霞,靳建平.石煤钒矿硫酸低温熟化—柱浸提钒工艺[J].矿冶,2020,29(3):62-67. 被引量:5

8叶国华,谢禹,胡艺博,左琪,乔吉波,童雄.低品位石煤钒矿低温硫酸化焙烧-水浸提钒研究[J].稀有金属,2020,44(7):753-761. 被引量:16

9程倩,王明,宁新霞,李洁,曹欢,郭金玉.从某低品位炭质钒矿石中酸浸-萃取-氨沉淀提钒实验研究[J].矿产综合利用,2021(3):17-21. 被引量:6

10蒋京航,叶国华,张世民,张爽.石煤直接酸浸提钒工艺研究进展[J].矿冶,2016,25(6):35-39. 被引量:12

1王东良,佘雪峰,魏秀泉.褐铁矿的磁化焙烧—磁选工艺解析[J].冶金管理,2022(7):19-21.

2张聪,王清良,周龙,胡鄂明,胡芳,雷治武,王红强.难溶含铀碱渣氧化焙烧酸浸试验研究[J].矿冶工程,2022,42(4):116-119.

3姜海,牛聪聪,夏瑜,方科.赞比亚卢安夏盆地巴鲁巴铜氧化矿石工艺矿物学特征及对比研究[J].世界有色金属,2022(12):99-103.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

The extraction of vanadium from stone coal was carried out by the process of acid mixing pelleting,high temperature curing and column leaching.Also,the study discussed the leaching effect of vanadium from raw ore affected by process conditions such as the amount of sulfuric acid,the amount of water supplement for curing,the binder dosage,the curing temperature,the curing time,the particle size of the cured material and the spraying intensity.The results show that the leaching rate is 76.99%when the conditions of the process are as follows:The particle size of the raw ore is less than 12 mm;the water content of the raw ore is 10%;the amount of sulfuric acid is 20%;the binder dosage is 0.05%;the curing temperature is 135 C;the curing time is 10 h;the particle size of the cured material is less than 8 cm;the liquid-solid ratio of leaching section is 1.5:1;the spraying intensity is 15 L/(m2·h).After the leaching residue is washed four times(the liquid-solid ratio of washing section is 1.5:1),the leaching rate of vanadium can be increased to 87.48%,and the content of V2O5,in the tailings can be reduced to 0.11%.The research can provide important reference for the industrial production of the heap-leaching of vanadium ore.

quote

GB/T 7714-2015 [1] ZHAO Xiao-yi, WANG Wang-bo, CHENG Qian, et al. Process Research on Vanadium Extraction from Stone Coal by High Temperature Curing and Column Leaching[J]. Rare Metals and Cemented Carbides, 2022(4): 1-6.
MLA [1] ZHAO Xiao-yi, et al., "Process Research on Vanadium Extraction from Stone Coal by High Temperature Curing and Column Leaching." Rare Metals and Cemented Carbides, no. 4, 2022, pp. 1-6.
APA [1] ZHAO Xiao-yi, WANG Wang-bo, CHENG Qian, WANG Yong, NING Xin-xia, & WANG Si-ying. (2022). Process Research on Vanadium Extraction from Stone Coal by High Temperature Curing and Column Leaching. Rare Metals and Cemented Carbides(4), 1-6.
IEEE [1] ZHAO Xiao-yi, WANG Wang-bo, CHENG Qian, WANG Yong, NING Xin-xia, and WANG Si-ying, "Process Research on Vanadium Extraction from Stone Coal by High Temperature Curing and Column Leaching," Rare Metals and Cemented Carbides, no. 4, pp. 1-6, 2022. keywords: {stone coal;vanadium;high temperature curing;column leaching;process condition}