Research on Recovery Treatment Process of Beryllium Copper Waste Slag and Application of the Recycled Materials AITranslate
Abstract AITranslate
The technology of recovering beryllium and useful resources from the waste slag produced in the melting and casting process of beryllium-copper alloy was studied.Using ESR waste slag as a covering agent,beryllium-copper waste slag was refined and purified in a vacuum induction furnace under the protection of a molten slag layer.The Yuanbao ingots obtained after refining and casting can be used as interalloys for producing beryllium-copper alloy ingots to replace expensive beryllium-copper master alloys.The recovered ESR waste slag can be recycled for the recovery treatment of beryllium-copper waste slag,and can also be used as a flux for the manufacture of ceramics,glass,etc.after impurity removal and purification.The experimental results show that adjusting the slag viscosity to about 0.09 Pa·s under the optimal mass ratio of ESR waste slag to CaF2 is beneficial to the improvement of metal yield and Be yield.When the vacuum degree is below 0.07 MPa,the Yuanbao ingots with no pores and uniform internal microstructure are obtained by vacuum refining.The successful research and development of this technology not only enables the comprehensive utilization of beryllium-copper waste slag as resources,turns waste into treasure,greatly reduces production costs and increases metal recovery rate,but also solves the environmental problems caused by long-term storage of beryllium-copper waste slag.
KeyWords AITranslate
1陈艳梅,赵俊学,樊君,崔雅茹,李小明,路晓涛.电渣重熔过程中渣成分变化的研究[J].特殊钢,2010,31(6):7-9. 被引量:15
2吴少鹏,李万明,尹彬,臧喜民,李德军.电渣重熔过程中熔渣成分变化的研究[J].材料与冶金学报,2018,17(3):191-197. 被引量:2
1杨荣林.钢液真空精炼用全干式真空泵系统的设计及应用[J].大型铸锻件,2022(5):37-41.
2王媛.工程机械用钢35MnBH的开发生产实践[J].天津冶金,2022(4):18-21.
3徐慧宁,王浩达,冀卫东,石浩,韦赟豪,谭忆秋.路面低温变色复配物的制备及热色特性[J].中国公路学报,2022,35(7):55-66.
Basic Information:
DOI:
Chinese Library Classification Number:X758[环境科学与工程—环境工程]
Citation Information:
The technology of recovering beryllium and useful resources from the waste slag produced in the melting and casting process of beryllium-copper alloy was studied.Using ESR waste slag as a covering agent,beryllium-copper waste slag was refined and purified in a vacuum induction furnace under the protection of a molten slag layer.The Yuanbao ingots obtained after refining and casting can be used as interalloys for producing beryllium-copper alloy ingots to replace expensive beryllium-copper master alloys.The recovered ESR waste slag can be recycled for the recovery treatment of beryllium-copper waste slag,and can also be used as a flux for the manufacture of ceramics,glass,etc.after impurity removal and purification.The experimental results show that adjusting the slag viscosity to about 0.09 Pa·s under the optimal mass ratio of ESR waste slag to CaF2 is beneficial to the improvement of metal yield and Be yield.When the vacuum degree is below 0.07 MPa,the Yuanbao ingots with no pores and uniform internal microstructure are obtained by vacuum refining.The successful research and development of this technology not only enables the comprehensive utilization of beryllium-copper waste slag as resources,turns waste into treasure,greatly reduces production costs and increases metal recovery rate,but also solves the environmental problems caused by long-term storage of beryllium-copper waste slag.
quote
| GB/T 7714-2015 | [1] ZHANG Jin-shan, REN Hai-qiang, GE Da-ming. Research on Recovery Treatment Process of Beryllium Copper Waste Slag and Application of the Recycled Materials[J]. Rare Metals and Cemented Carbides, 2022(4): 7-11. |
| MLA | [1] ZHANG Jin-shan, et al., "Research on Recovery Treatment Process of Beryllium Copper Waste Slag and Application of the Recycled Materials." Rare Metals and Cemented Carbides, no. 4, 2022, pp. 7-11. |
| APA | [1] ZHANG Jin-shan, REN Hai-qiang, & GE Da-ming. (2022). Research on Recovery Treatment Process of Beryllium Copper Waste Slag and Application of the Recycled Materials. Rare Metals and Cemented Carbides(4), 7-11. |
| IEEE | [1] ZHANG Jin-shan, REN Hai-qiang, and GE Da-ming, "Research on Recovery Treatment Process of Beryllium Copper Waste Slag and Application of the Recycled Materials," Rare Metals and Cemented Carbides, no. 4, pp. 7-11, 2022. keywords: {beryllium-copper waste slag;beryllium recovery;refining;Yuanbao ingot;CaF2;slag viscosity;vacuumdegree} |