Research Progress of Lithium Extraction Technology from Fly Ash AITranslate
Abstract AITranslate
There are a lot of metal elements in fly ash,which has a certain extraction value.In this paper,the existing state of lithium in fly ash and the economical efficiency of lithium extraction are analyzed.Also,the research progress of lithium leaching technology from fly ash and the separation extraction technology of lithium from the leaching solution is reviewed.The key nodes of lithium extraction from fly ash are briefly discussed,giving reasonable suggestions and research directions.
KeyWords AITranslate
1SUN Yuzhuang,ZHAO Cunliang,LI Yanheng,WANG Jinxi,ZHANG Jianya,JIN Zhe,LIN Mingyue,Wolfgang KALKREUTH.Further Information of the Associated Li Deposits in the No.6 Coal Seam at Jungar Coalfield, Inner Mongolia, Northern China[J].地质学报:英文版,2013,87(4):1097-1108. 被引量:32
2刘向磊,钟辉,唐中杰.盐湖卤水提锂工艺技术现状及存在的问题[J].无机盐工业,2009,41(6):4-6. 被引量:35
3张玲,林德松.我国稀有金属资源现状分析[J].地质与勘探,2004,40(1):26-30. 被引量:37
4薛宇飞,蒋开喜,王海北,谢铿,周起帆.盐湖卤水锂萃取体系的性能研究[J].有色金属:冶炼部分,2018(6):28-32. 被引量:8
5祝茂忠.溶剂萃取法提取盐湖卤水中锂的研究[J].化工矿物与加工,2016,45(8):27-30. 被引量:6
6曾小毛,樊磊.高镁锂比盐湖老卤萃取提锂工艺研究[J].矿冶工程,2017,37(6):95-96. 被引量:7
7侯永茹,李彦恒,代红,侯晓琪.用吸附法从粉煤灰碱性溶液里提取锂[J].粉煤灰综合利用,2015,29(3):10-11. 被引量:20
8徐徽,许良,陈白珍,石西昌,杨鑫.高镁锂比盐湖卤水镁锂分离工艺[J].中南大学学报:自然科学版,2009,40(1):36-40. 被引量:30
9陈东,李超.氯化铝溶液中分离、制取碳酸锂新技术研究[J].轻金属,2018(2):14-17. 被引量:2
10侯晓琪,李彦恒,代红,侯永茹.从粉煤灰中浸出锂的工艺研究[J].河北工程大学学报:自然科学版,2015,23(1):58-61. 被引量:9
1韩海军,黄珊珊,符宝怡,高乙情,陈烽雄,李家乐.粉煤灰中提取锂的研究进展[J].当代化工研究,2022(15):16-18.
2李淑雅,王晓,马玉军,张付康,李娟.共存离子浓度对[BMIM]PF_(6)-TBP体系萃取提锂的影响[J].有色金属工程,2022,12(8):77-81.
3刘庆生,喻修远,肖浩,刘嘉铭,邱廷省.磷酸铁锂电池废料提锂尾渣的回收及磷酸铁的制备[J].稀有金属与硬质合金,2022,50(4):17-23. 被引量:2
4王平.量化分析锂供需与锂价格的联动关系[J].无机盐工业,2022,54(9):1-13. 被引量:2
5李强.盐湖卤水提锂工艺中萃取法的应用[J].石化技术,2022,29(8):197-199. 被引量:1
6张果泰,漆贵财,海春喜,周园.球形MnO_(2)·0.5H_(2)O提锂性能及其机理研究[J].盐湖研究,2022,30(3):21-33. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF826.3[冶金工程—有色金属冶金]
Citation Information:
There are a lot of metal elements in fly ash,which has a certain extraction value.In this paper,the existing state of lithium in fly ash and the economical efficiency of lithium extraction are analyzed.Also,the research progress of lithium leaching technology from fly ash and the separation extraction technology of lithium from the leaching solution is reviewed.The key nodes of lithium extraction from fly ash are briefly discussed,giving reasonable suggestions and research directions.
quote
| GB/T 7714-2015 | [1] XU Lijun, LIU Rui-ping, ZHANG Yun-feng, et al. Research Progress of Lithium Extraction Technology from Fly Ash[J]. Rare Metals and Cemented Carbides, 2022(4): 12-16. |
| MLA | [1] XU Lijun, et al., "Research Progress of Lithium Extraction Technology from Fly Ash." Rare Metals and Cemented Carbides, no. 4, 2022, pp. 12-16. |
| APA | [1] XU Lijun, LIU Rui-ping, ZHANG Yun-feng, CHI Jun-zhou, & CHEN Dong. (2022). Research Progress of Lithium Extraction Technology from Fly Ash. Rare Metals and Cemented Carbides(4), 12-16. |
| IEEE | [1] XU Lijun, LIU Rui-ping, ZHANG Yun-feng, CHI Jun-zhou, and CHEN Dong, "Research Progress of Lithium Extraction Technology from Fly Ash," Rare Metals and Cemented Carbides, no. 4, pp. 12-16, 2022. keywords: {fly ash;lithium;leaching;separation extraction;research progress} |