Measuring of Ni in Mixed Material by Atomic Absorption AITranslate

Jinan Institute of Metallurgical Sciences;Jinan Institute of Metallurgical Sciences
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made of the conditions for the determination of Ni in the reclaimed cemented carbide by atomic absorption.The results showed that the use of the operating conditions indicated in the paper can result in the 98%~105% measured recovery and relative inaccuracy ≤17%,the measured results basically conforming to the standard value.When Co content in the mixed material is ≤13%,Co will not interfere with the measurement,as can satisfy the production measurement.

KeyWords AITranslate

atomic absorption cemented carbide scrap Ni measurement

1李俊义 等.分析化学[M].辽宁:大连工学院出版社,1998..

1张力.原子吸收法测定锌熔混合料中的锌[J].硬质合金,1999,16(2):114-116.

2李慧玲,张林.混合料中钒、铬分量测定方法的研究[J].四川有色金属,2007(2):37-39. 被引量:3

3孙媚华,陈迁,陈泽智,宋亭,宋光泉.紫外-可见分光光度法测定单质碘含量[J].仲恺农业工程学院学报,2012,25(2):37-41. 被引量:3

4郑一新,黄文川,程新胜,陈高昌,郑根武.一种快速测定一元弱酸pK_a的方法[J].化学教育,2005,26(10):55-56. 被引量:1

5晋霞,刘世斌.铋膜电极阳极溶出伏安法测定人发中锌的含量[J].太原理工大学学报,2008,39(2):199-202. 被引量:3

6曾波,付韬,贺铀,付志军.库仑滴定在锰矿石中硫的分析应用[J].中国锰业,2003,21(3):41-42. 被引量:2

7李侠,李晓艳.非水滴定法快速测定食品中的糖精钠[J].中国酿造,2006,25(5):65-66. 被引量:2

8汪耀明,陶玉贵,叶连斌,万宗飞.毛细管电泳仪测定土壤中氧化乐果的含量[J].安徽工程科技学院学报:自然科学版,2007,22(4):38-41. 被引量:3

9李令,朱云勤,张菊,刘凯萍,孟铁宏,江鸥.邻二氮菲分光光度法测定赤泥和石灰石混匀度[J].岩矿测试,2009,28(4):394-396. 被引量:1

10郭振华,刘波.粉煤灰/海泡石纤维复合沥青混合料的制备与性能研究[J].功能材料,2007,38(A09):3453-3457. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:O657.31[理学—分析化学]

Citation Information:

Study is made of the conditions for the determination of Ni in the reclaimed cemented carbide by atomic absorption.The results showed that the use of the operating conditions indicated in the paper can result in the 98%~105% measured recovery and relative inaccuracy ≤17%,the measured results basically conforming to the standard value.When Co content in the mixed material is ≤13%,Co will not interfere with the measurement,as can satisfy the production measurement.

quote

GB/T 7714-2015 [1] ZHANG Li, CHAO Yue-qian. Measuring of Ni in Mixed Material by Atomic Absorption[J]. Rare Metals and Cemented Carbides, 2003(3): 15-17.
MLA [1] ZHANG Li, and CHAO Yue-qian. "Measuring of Ni in Mixed Material by Atomic Absorption." Rare Metals and Cemented Carbides, no. 3, 2003, pp. 15-17.
APA [1] ZHANG Li, & CHAO Yue-qian. (2003). Measuring of Ni in Mixed Material by Atomic Absorption. Rare Metals and Cemented Carbides(3), 15-17.
IEEE [1] ZHANG Li and CHAO Yue-qian, "Measuring of Ni in Mixed Material by Atomic Absorption," Rare Metals and Cemented Carbides, no. 3, pp. 15-17, 2003. keywords: {atomic absorption;cemented carbide scrap;Ni;measurement}