Study on the Sintering Process of NdFeB Magnet AITranslate
Abstract AITranslate
The effects of sintering in vacuum and Ar atmosphere on the magnetic performance and microstructure of NdFeB magnet were studied. The results show that there is a great individual difference of magnetic performance among vacuum sintered samples,but the Ar sintered samples are almost of uniform magnetic performance. The average remanence and magnetic energy product of the magnet by Ar atmosphere sintering are about 0.05-0.09 T and 40 kJ/m^3 higher than that by vacuum sintering,respectively. The SEM photos indicate that the microstructure of Ar-atmosphere sintered magnet is much more homogeneous,but vacuum sintered magnet is of many defects.
KeyWords AITranslate
1解振林,田薇,陈连生.钕铁硼永磁合金烧结过程中的晶粒聚集长大及对磁性能的影响[J].稀有金属材料与工程,2003,32(4):264-267. 被引量:10
2谭春林,白书欣,张虹,高艳丽,张家春,蔡珣.回火处理对烧结钕铁硼永磁材料组织和磁性能的影响[J].中国有色金属学报,2002,12(z1):64-66. 被引量:17
3Tenaud P, Lemaire H, Vial F. Recent improvements in NdFeB sintered magnets [J]. Magn and Magn Mater, 1991,101:328-332.
4于旭光,秦茶,赵田臣,杨惠芳,徐良,赵金伶,田藏韬.烧结钕铁硼微观组织对磁性能的影响[J].特殊钢,2003,24(5):16-18. 被引量:12
1唐杰,王晓军,杨梨容,张林,魏成富.烧结Nd-Fe-B合金断裂机制和增韧方法[J].材料导报,2016,30(17):97-101.
2利荣森,唐焱,徐晋勇,甘家毅.烧结钕铁硼永磁体制备工艺的研究进展[J].热加工工艺,2019,48(4):10-14. 被引量:6
1江英英,甘正明.高性能粘结钕铁硼磁性材料生产工艺环境影响分析[J].绿色科技,2019,0(24):151-153. 被引量:2
2张葆华.钕铁硼生产中烧结挥发物的相关研究[J].中国金属通报,2019,0(11):264-265.
3付利雯,汪金良,雷翔,王厚庆.钕铁硼废料资源化回收利用研究进展[J].有色金属科学与工程,2020,11(1):92-97. 被引量:9
4刘义伦,曾洋.不同成型工艺下钕铁硼模压成型过程的力学行为分析[J].粉末冶金技术,2020,38(4):262-268. 被引量:1
5常凯曦,吉琳,吝怡,樊茜,李露新,刘建华,马锋,吕毅,严小鹏.基于磁驱动技术的空肠营养管的设计[J].现代生物医学进展,2020,20(17):3217-3220. 被引量:3
6赵导文,唐杰,邓盛贤,杨梨容,刘畅.回火对高矫顽力烧结Nd-Fe-B磁体微结构及磁性能的影响[J].磁性材料及器件,2022,53(3):38-41.
1柴庆冕,杨双锁,马春生.变电站蓄电池组电压均衡策略研究[J].电气工程学报,2016,11(12):45-49.
2董博,李永东.蓄电池容量均衡方法概述[J].电源学报,2011,9(5):32-36. 被引量:5
3高卫星.300MW机组锅炉燃烧调整及优化[J].科技创新与应用,2012,2(6):46-46. 被引量:1
4言小艾.手机电池的使用与保养[J].大众用电,2011(6):44-44.
5谭晓慧.分层教学法在电工学课程中的应用[J].科技创新与应用,2012,2(07Z):256-256.
6曹阳,彭秀英,杨桃月.小型风光互补电源的蓄电池智能充电装置设计[J].电源技术,2011,35(2):213-214. 被引量:7
7沈金波,李宏文,王景凯.小型断路器接线端子温度特性的试验研究[J].建筑电气,2009,28(1):11-14. 被引量:1
8王晓.标准化作业在基层点检班组的应用[J].设备管理与维修,2016(6):16-18.
9黎康康,王志勇,靳国忠,吴刚.基于统计分析的风电齿轮箱试验温度评价标准[J].风能,2015,0(7):70-72.
10叶笑冬,陆宇,王子健,李劲.从工业4.0看储能系统锂电池寿命的预测[J].上海电气技术,2015,8(1):1-3. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TM273[一般工业技术—材料科学与工程]
Citation Information:
The effects of sintering in vacuum and Ar atmosphere on the magnetic performance and microstructure of NdFeB magnet were studied. The results show that there is a great individual difference of magnetic performance among vacuum sintered samples,but the Ar sintered samples are almost of uniform magnetic performance. The average remanence and magnetic energy product of the magnet by Ar atmosphere sintering are about 0.05-0.09 T and 40 kJ/m^3 higher than that by vacuum sintering,respectively. The SEM photos indicate that the microstructure of Ar-atmosphere sintered magnet is much more homogeneous,but vacuum sintered magnet is of many defects.
quote
| GB/T 7714-2015 | [1] TANG Jie, WEI Cheng-fu, ZHAO Dao-wen, et al. Study on the Sintering Process of NdFeB Magnet[J]. Rare Metals and Cemented Carbides, 2009(2): 1-3. |
| MLA | [1] TANG Jie, et al., "Study on the Sintering Process of NdFeB Magnet." Rare Metals and Cemented Carbides, no. 2, 2009, pp. 1-3. |
| APA | [1] TANG Jie, WEI Cheng-fu, ZHAO Dao-wen, LIN Hong, & DENG Sheng-xian. (2009). Study on the Sintering Process of NdFeB Magnet. Rare Metals and Cemented Carbides(2), 1-3. |
| IEEE | [1] TANG Jie, WEI Cheng-fu, ZHAO Dao-wen, LIN Hong, and DENG Sheng-xian, "Study on the Sintering Process of NdFeB Magnet," Rare Metals and Cemented Carbides, no. 2, pp. 1-3, 2009. keywords: {NdFeB magnet;vacuum sintering;Ar atmosphere sintering} |