daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Boosting Piezoelectricity via a Bimodal Pore Distribution: The Role of Small Pores Boosting Piezoelectricity via a Bimodal Pore Distribution: The Role of Small Pores AITranslate

Polymer Research Institute of Sichuan University; Polymer Research Institute of Sichuan University; Polymer Research Institute of Sichuan University;Baosheng Science and Technology Innovation Company, Ltd.;Baosheng Science and Technology Innovation Company, Ltd.
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Structural elements play an important role for improving mechanical-to-electrical energy conversion of piezoelectric devices with a hierarchical configuration. However, the state-of-the-art manufacturing method fails to ensure plenty of structural elements for better piezoelectricity. In this work, piezoelectric poly(vinylidene fluoride) (PVDF) foam with an extremely high content of structural elements was fabricated by applying bimodal pore distributions via supercritical carbon dioxide foaming and template-leaching methods, and the mechanisms for improved piezoelectricity were systematically researched. By removal of the preadded templates, the structural element density can be modulated from ∼187 to ∼2.6 × 106 cells/mm2. It was found that the small pores in a foam with bimodal pore distributions can diminish small or medium stress and convert it to high stress in the rest area of the large pores, thus greatly enlarging the ratio of stress concentration. Impressively, the stress concentration degree is improved from 0.19 of bulk PVDF to 5.3 and 13.3 of PVDF foam with unimodal and bimodal pore distributions, respectively. As a result, the piezoelectric outputs increase correspondingly from ∼5 V to ∼8.5 and ∼13 V. This work reveals the strain–charge correlations by applying structural elements and can be extended widely for studies on a three-dimensional piezoelectric device.

KeyWords AITranslate

piezoelectric energy harvesting PVDF composites SCCO2 foaming bimodal pore distribution
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01223

Chinese Library Classification Number:

Citation Information:

Structural elements play an important role for improving mechanical-to-electrical energy conversion of piezoelectric devices with a hierarchical configuration. However, the state-of-the-art manufacturing method fails to ensure plenty of structural elements for better piezoelectricity. In this work, piezoelectric poly(vinylidene fluoride) (PVDF) foam with an extremely high content of structural elements was fabricated by applying bimodal pore distributions via supercritical carbon dioxide foaming and template-leaching methods, and the mechanisms for improved piezoelectricity were systematically researched. By removal of the preadded templates, the structural element density can be modulated from ∼187 to ∼2.6 × 106 cells/mm2. It was found that the small pores in a foam with bimodal pore distributions can diminish small or medium stress and convert it to high stress in the rest area of the large pores, thus greatly enlarging the ratio of stress concentration. Impressively, the stress concentration degree is improved from 0.19 of bulk PVDF to 5.3 and 13.3 of PVDF foam with unimodal and bimodal pore distributions, respectively. As a result, the piezoelectric outputs increase correspondingly from ∼5 V to ∼8.5 and ∼13 V. This work reveals the strain–charge correlations by applying structural elements and can be extended widely for studies on a three-dimensional piezoelectric device.

quote

GB/T 7714-2015 [1] Qingquan Jiang, Jiajun Guo, Min Nie, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01223.
MLA [1] Qingquan Jiang, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01223.
APA [1] Qingquan Jiang, Jiajun Guo, Min Nie, Xu Zhu, & Huarong Zhang. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01223
IEEE [1] Qingquan Jiang, Jiajun Guo, Min Nie, Xu Zhu, and Huarong Zhang, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01223. keywords: {piezoelectric energy harvesting PVDF composites SCCO2 foaming bimodal pore distribution}