daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Flexible High-Energy-Density 4.3 V Supercapacitor Based on a Trimetallic Sulfide Cathode and a Bimetallic Sulfide-Polypyrrole Anode with an Ionic Liquid Gel Polymer Electrolyte AITranslate

School of Nano Science and Technology, IIT Kharagpur;Department of Physics, IIT Kharagpur;Electronics and Electrical Communication Engineering, IIT Kharagpur
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Battery-type electrode materials have recently been explored as an exclusive class of high-capacity cathode materials for the advancement of hybrid supercapacitors. The electrode materials’ higher specific energy, long-term cycle stability, and faster ion transportation are commendable attributes that have prompted researchers to envisage high-performance cathode materials. The hierarchically structured electrodes provide optimal redox sites and channels for accelerating the transit of ions and electrons between the electrodes and electrolytes. Electropolymerization and a facile hydrothermal procedure followed by calcination were used to concoct Cu–Fe–Co-based trimetallic sulfide and Ni–Fe-based bimetallic sulfide with the polypyrrole composite over carbon cloth for the development of a flexible asymmetric supercapacitor. The hierarchical core–shell Cu4Fe2Co2S4 hybrid composite on carbon cloth was used as a high-performance cathode material for solid-state supercapacitors. The Cu4Fe2Co2S4 electrode exhibits a capacitance retention of 84.87% after 10,000 cycles and a specific capacitance of 334 mAh/g at 4 mA/cm2. In addition, the electropolymerized Ni2FeS4-Ppy on carbon cloth was initially reported as the recent anode, with a retention of the capacitance of 92.32% after 10,000 cycles, a specific capacitance of 1228 mAh/g at 8 mA/cm2, and a significantly increased specific energy of 790 Wh/kg. The ionic liquid polymer-based electrolyte gel assembled flexible all-solid-state asymmetric supercapacitor Ni2FeS4-Ppy/PVA-DMSO-EMIM-BF4/Cu4Fe2Co2S4 has a specific energy of 756.7 Wh/kg and specific power of 10750 W/kg, indicating a specific capacity of 352 mAh/g and remarkable retention of the capacitance of 96% after 10,000 cycles. These unrivaled inorganic–organic amalgamation systems strengthen the synergistic development of innovative functional electrode materials for energy storage applications with improved cyclic stability and rate capability.

KeyWords AITranslate

binary metal sulfide ternary metal sulfide polypyrrole pseudocapacitance ionic liquid gel polymer asymmetric Supercapacitor
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.3c01230

Chinese Library Classification Number:

Citation Information:

Battery-type electrode materials have recently been explored as an exclusive class of high-capacity cathode materials for the advancement of hybrid supercapacitors. The electrode materials’ higher specific energy, long-term cycle stability, and faster ion transportation are commendable attributes that have prompted researchers to envisage high-performance cathode materials. The hierarchically structured electrodes provide optimal redox sites and channels for accelerating the transit of ions and electrons between the electrodes and electrolytes. Electropolymerization and a facile hydrothermal procedure followed by calcination were used to concoct Cu–Fe–Co-based trimetallic sulfide and Ni–Fe-based bimetallic sulfide with the polypyrrole composite over carbon cloth for the development of a flexible asymmetric supercapacitor. The hierarchical core–shell Cu4Fe2Co2S4 hybrid composite on carbon cloth was used as a high-performance cathode material for solid-state supercapacitors. The Cu4Fe2Co2S4 electrode exhibits a capacitance retention of 84.87% after 10,000 cycles and a specific capacitance of 334 mAh/g at 4 mA/cm2. In addition, the electropolymerized Ni2FeS4-Ppy on carbon cloth was initially reported as the recent anode, with a retention of the capacitance of 92.32% after 10,000 cycles, a specific capacitance of 1228 mAh/g at 8 mA/cm2, and a significantly increased specific energy of 790 Wh/kg. The ionic liquid polymer-based electrolyte gel assembled flexible all-solid-state asymmetric supercapacitor Ni2FeS4-Ppy/PVA-DMSO-EMIM-BF4/Cu4Fe2Co2S4 has a specific energy of 756.7 Wh/kg and specific power of 10750 W/kg, indicating a specific capacity of 352 mAh/g and remarkable retention of the capacitance of 96% after 10,000 cycles. These unrivaled inorganic–organic amalgamation systems strengthen the synergistic development of innovative functional electrode materials for energy storage applications with improved cyclic stability and rate capability.

quote

GB/T 7714-2015 [1] Monojit Mondal, Dipak Kumar Goswami, Tarun Kanti Bhattacharyya. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c01230.
MLA [1] Monojit Mondal, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c01230.
APA [1] Monojit Mondal, Dipak Kumar Goswami, & Tarun Kanti Bhattacharyya. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c01230
IEEE [1] Monojit Mondal, Dipak Kumar Goswami, and Tarun Kanti Bhattacharyya, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c01230. keywords: {binary metal sulfide ternary metal sulfide polypyrrole pseudocapacitance ionic liquid gel polymer asymmetric Supercapacitor}