daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Interfacial Molecular Lock: A Universal Strategy for Hydrogel Adhesion AITranslate

China University of Geosciences; China University of Geosciences; China University of Geosciences; China University of Geosciences
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Hydrogel adhesion is fundamental to a large number of established and emerging fields. The existing adhesion methods have some problems, such as the limited penetration ability of polymers in hydrogels, the interface hardening caused by in situ monomer polymerization, the secondary damage caused by covalent strong bonding during detachment, the need for complementary techniques to induce adhesion, and the complex and impractical operation. Inspired by the adhesion mechanism of mussels, we propose a universal strategy of interfacial molecular lock (IML) for hydrogel adhesion, which is simple to operate. IML is composed of organic (low-molecular-weight) molecules containing catechol groups, which are easy to penetrate into hydrogels. The principle of IML relies on the combination of a dynamic covalent bond, coordination bond, hydrogen bond, π–π interaction, and cation-π interaction. IML can adapt to interfacial chemistry of hydrogels on different substrates and achieve reversible adhesion without external regulation. The molecular micro-polymerization further enhances the stability and strength of hydrogel adhesion. IML is expected to expand hydrogel adhesion in various applications, especially tissue adhesives, wound sealants, wearable devices, and hydrogel-on-metal protection.

KeyWords AITranslate

hydrogel adhesion interfacial molecular lock mussel tannic acid micropolymerization
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.2c01990

Chinese Library Classification Number:

Citation Information:

Hydrogel adhesion is fundamental to a large number of established and emerging fields. The existing adhesion methods have some problems, such as the limited penetration ability of polymers in hydrogels, the interface hardening caused by in situ monomer polymerization, the secondary damage caused by covalent strong bonding during detachment, the need for complementary techniques to induce adhesion, and the complex and impractical operation. Inspired by the adhesion mechanism of mussels, we propose a universal strategy of interfacial molecular lock (IML) for hydrogel adhesion, which is simple to operate. IML is composed of organic (low-molecular-weight) molecules containing catechol groups, which are easy to penetrate into hydrogels. The principle of IML relies on the combination of a dynamic covalent bond, coordination bond, hydrogen bond, π–π interaction, and cation-π interaction. IML can adapt to interfacial chemistry of hydrogels on different substrates and achieve reversible adhesion without external regulation. The molecular micro-polymerization further enhances the stability and strength of hydrogel adhesion. IML is expected to expand hydrogel adhesion in various applications, especially tissue adhesives, wound sealants, wearable devices, and hydrogel-on-metal protection.

quote

GB/T 7714-2015 [1] Wanglong Zhang, Yu Dai, Fan Xia, et al. ACS Applied Polymer Materials, 2023(5). DOI:10.1021/acsapm.2c01990.
MLA [1] Wanglong Zhang, et al., ACS Applied Polymer Materials, no. 5, 2023, https://doi.org/10.1021/acsapm.2c01990.
APA [1] Wanglong Zhang, Yu Dai, Fan Xia, & Xiaojin Zhang. (2023). ACS Applied Polymer Materials(5). https://doi.org/10.1021/acsapm.2c01990