Rare Metal-containing Ceramic Pigment and Glaze──Study of Rare Metal Fine Chemicals(Ⅱ) AITranslate

Beijing Normal University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper briefly describes the recent research and development of rare metalcontaining ceramic pigments and glazes. Some related literatures are presented for reference.

KeyWords AITranslate

rare metal fine chemicals ceramics pigment glaze.

1张文丽.色料的呈色机理、生产及应用[J].中国陶瓷工业,1997,4(2):10-16. 被引量:21

2邵明梁.硫硒化镉大红釉的研究[J].江苏陶瓷,1997,30(2):3-5. 被引量:3

3杨萍,赵宗昱.硫化锌基颜料的研究[J].陶瓷研究,1997,12(1):7-11. 被引量:1

4李国栋,吴伯麟,吕林女.高温型硫硒化镉红色釉的研制[J].中国陶瓷,1997,33(1):6-8. 被引量:4

5俞康泰.对我国陶瓷色釉料工业生产发展的几点建议[J].中国陶瓷工业,1996,3(4):4-6. 被引量:3

6司志胜,马桂红.低温快烧无光釉的研制[J].山东陶瓷,1996,19(3):23-26. 被引量:6

7常传平,孙岩,马明川,赵翠萍.硅酸锆超细微粉及工艺研究[J].山东陶瓷,1996,19(3):27-28. 被引量:1

8陈建国,唐绍裘.碳酸锂对瓷釉性能影响的研究[J].山东陶瓷,1996,19(2):3-9. 被引量:2

9王登其.还原焰高温釉下颜料的研制[J].中国陶瓷,1995,31(6):30-32. 被引量:2

10董麒,叶大年,张振禹.瓷釉化学成分之总观[J].中国陶瓷,1995,31(6):43-45. 被引量:2

1张文朴.稀有金属精细化学品研究与开发进展(Ⅱ)──无机非金属材料[J].稀有金属与硬质合金,1995,23(2):37-41.

2山内昭.日本电渗析技术研究与开发进展[J].水处理技术,1995,21(4):203-207. 被引量:1

3陈旭峰.“八五”期间陶瓷窑用耐火材料的新进展[J].硅酸盐通报,1997,16(1):15-20. 被引量:1

4王强,陈铁亮,周鑫.新型玻璃金水的研制[J].河北陶瓷,1999,27(4):3-8.

5姜伟,姚勇,杨缤维,鲁伟员,张书霞,寇自力.两面顶金刚石杂质的中子活化分析[J].人工晶体学报,2005,34(6):1100-1104. 被引量:2

6王杰曾,袁林.新形势下水泥窑用耐火材料的研究与开发进展[J].硅酸盐通报,2016,35(10):3219-3223. 被引量:4

7彭新战,胡道和.磷石膏分解炉的研究与开发进展[J].硫酸工业,1993(5):43-48. 被引量:4

8王存文,张俊峰,孙炜.液相甲醇合成新工艺的工业化研究与开发进展[J].湖北化工,2001,18(1):13-15.

9李春利,孙玉春,王志英,方静.新型立体传质塔板CTST的研究与开发进展[J].河北工业大学学报,2004,33(2):155-162. 被引量:13

10任叶果,黄明智,侯仲轲.四氢酞酰亚胺类除草剂的研究与开发进展[J].精细化工中间体,2004,34(6):7-9. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TQ174.4[化学工程—陶瓷工业]

Citation Information:

This paper briefly describes the recent research and development of rare metalcontaining ceramic pigments and glazes. Some related literatures are presented for reference.

quote

GB/T 7714-2015 [1] ZHANG Wen-pu. Rare Metal-containing Ceramic Pigment and Glaze──Study of Rare Metal Fine Chemicals(Ⅱ)[J]. Rare Metals and Cemented Carbides, 1998(3): 52-58.
MLA [1] ZHANG Wen-pu. "Rare Metal-containing Ceramic Pigment and Glaze──Study of Rare Metal Fine Chemicals(Ⅱ)." Rare Metals and Cemented Carbides, no. 3, 1998, pp. 52-58.
APA [1] ZHANG Wen-pu. (1998). Rare Metal-containing Ceramic Pigment and Glaze──Study of Rare Metal Fine Chemicals(Ⅱ). Rare Metals and Cemented Carbides(3), 52-58.
IEEE [1] ZHANG Wen-pu, "Rare Metal-containing Ceramic Pigment and Glaze──Study of Rare Metal Fine Chemicals(Ⅱ)," Rare Metals and Cemented Carbides, no. 3, pp. 52-58, 1998. keywords: {rare metal;fine chemicals;ceramics pigment;glaze.}