Development & Application of SP-700 Ti Alloy AITranslate

Northwest Nonferrous Metal Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

SP-700 Ti alloy features better forgeability, longer service life and lower cost than the conventional Ti alloy. It has found some applications in the fields of sports goods, hand tools and watch-making, etc. It is expected to extend its application to the steam turbine blades industry.

KeyWords AITranslate

SP-700 Ti alloy heat treatment microstructure mechanical performance superplastic formation

1付明杰,李继忠,曾元松.搅拌摩擦焊Ti-4.5Al-3V-2Fe-2Mo合金的超塑性变形行为研究[J].稀有金属,2020,0(1):1-8. 被引量:8

2邱仟,王克鲁,李鑫,王俊,张开铭,高鑫.变形工艺参数对SP700钛合金微观组织及显微硬度的影响[J].特种铸造及有色合金,2022,42(4):459-462.

3李梁,孙建科,孟祥军.钛合金超塑性研究及应用现状[J].材料开发与应用,2004,19(6):34-38. 被引量:28

4寇生中,昝斌.超塑性钛合金研究究开发概?[J].材料导报:网络版,2007(1):10-12. 被引量:1

5张绪虎,单群,陈永来,杜志惠.钛合金在航天飞行器上的应用和发展[J].中国材料进展,2011,30(6):28-32. 被引量:44

6曲选辉,钟伟,李益民,张健,钟孝贤.硬质合金注射成形制品中的缺陷控制[J].稀有金属材料与工程,2000,29(5):332-335. 被引量:6

7王智汉,高巍,张刚.SP-700钛合金的热处理工艺研究[J].石油化工建设,2016,38(1):61-64.

8王新,李蒙,张永强,王俭,徐哲,张平辉.退火温度对SP-700钛合金板材显微组织和力学性能的影响[J].材料热处理学报,2018,39(4):44-50. 被引量:5

9苏頔瑶,静永娟,岳喜山,陈林.SP700/TC4钛合金蜂窝夹层结构钎焊工艺分析[J].焊接学报,2018,39(4):119-123.

10陈锡源,陈俐,常明,何恩光.SP700钛合金激光焊的焊缝成形与性能分析[J].焊接学报,2018,39(6):121-125. 被引量:6

1白会涛,盛鹏,王晓,徐丽,李慧,薛晴.富钠普鲁士蓝的制备及其储钠性能研究[J].稀有金属,2021,45(12):1521-1528.

2邱仟,王克鲁,李鑫,王俊,张开铭,高鑫.变形工艺参数对SP700钛合金微观组织及显微硬度的影响[J].特种铸造及有色合金,2022,42(4):459-462.

3祝宝军,曲选辉,秦明礼,肖平安.硬质合金注射成形过程中的难点问题及解决方法[J].粉末冶金材料科学与工程,2001,6(3):173-178.

4李志希,范景莲,刘涛,肖琼.硬质合金注射工艺参数的研究[J].硬质合金,2005,22(1):32-35. 被引量:4

5张鹏省,毛小南,赵永庆,曾卫东,洪权,李辉.世界钛及钛合金产业现状及发展趋势[J].稀有金属快报,2007,26(10):1-6. 被引量:26

6李枫,陈明和,范平,王荣华,朱丽瑛,周兆峰.超塑成形/扩散焊接组合工艺的技术概况与应用[J].新技术新工艺,2008(4):70-73. 被引量:5

7王荣华,陈明和,陈国亮,范平,李枫,周兆锋.TC4钛合金盒形件超塑成形工艺[J].热加工工艺,2008,37(11):46-48. 被引量:9

8陈慧琴,邓文斌.TC11钛合金等轴组织热变形行为与组织演变[J].稀有金属,2009,33(2):147-152. 被引量:12

9吴晨刚,王高潮,董洪波,耿启冬.TA15钛合金的超塑性研究及组织变化[J].热加工工艺,2009,38(24):5-7. 被引量:1

10黄晓辉,左秀荣,刘凤芹,王齐伟,李勇.Ti6Al4V合金超塑性的研究进展及应用现状[J].材料研究与应用,2010,4(1):23-26. 被引量:7

1王智汉,高巍,张刚.SP-700钛合金的热处理工艺研究[J].石油化工建设,2016,38(1):61-64.

2陈石卿.强度高加工性好的SP—700钛合金[J].钛合金信息,1996(1):4-5.

3胡耀君.强度高成形性好的钛合金SP-700[J].钛工业进展,1993,10(2):54-55. 被引量:1

4劳金海.高强度高加工性SP—700钛合金的应用和发展[J].钛合金信息,1999(2):14-15.

5大内千秋,毛广湘.新型钛合金SP—700和表面硬化处理方法[J].国外稀有金属,1992(5):49-52.

6Thomas Schneider,杨春林.用铣床直接加工涡轮叶片[J].世界制造技术与装备市场,2003(2):142-143.

7李有观.易加工钛合金[J].世界有色金属,2005(3):68-68.

8黄虹.钛及其合金的非航空航天用途[J].稀有金属与硬质合金,2001,29(3):46-49. 被引量:8

9黄淑梅.SCS-6/SP-700复合材料的超塑性成形[J].稀有金属材料与工程,2003,32(8):620-620.

10付福兴.激光功率对透平叶片激光熔覆Ni基合金涂层裂纹的影响[J].热加工工艺,2016,45(10):173-174.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]

Citation Information:

SP-700 Ti alloy features better forgeability, longer service life and lower cost than the conventional Ti alloy. It has found some applications in the fields of sports goods, hand tools and watch-making, etc. It is expected to extend its application to the steam turbine blades industry.

quote

GB/T 7714-2015 [1] HUANG Jin-chang. Development & Application of SP-700 Ti Alloy[J]. Rare Metals and Cemented Carbides, 1998(3): 58-62.
MLA [1] HUANG Jin-chang. "Development & Application of SP-700 Ti Alloy." Rare Metals and Cemented Carbides, no. 3, 1998, pp. 58-62.
APA [1] HUANG Jin-chang. (1998). Development & Application of SP-700 Ti Alloy. Rare Metals and Cemented Carbides(3), 58-62.
IEEE [1] HUANG Jin-chang, "Development & Application of SP-700 Ti Alloy," Rare Metals and Cemented Carbides, no. 3, pp. 58-62, 1998. keywords: {SP-700 Ti alloy;heat treatment;microstructure;mechanical performance;superplastic formation}