Large Sign Reversal of Tunneling Magnetoresistance in an Epitaxial Fe/MgAlOx/Fe4N Magnetic Tunnel Junction Large Sign Reversal of Tunneling Magnetoresistance in an Epitaxial Fe/MgAlOx/Fe4N Magnetic Tunnel Junction AITranslate
Abstract AITranslate
A sign-reversible tunneling magnetoresistance (TMR) bestows an extra control freedom to design TMR-based spintronic devices for developing spin-logic applications. Here, we demonstrate a large sign reversal of TMR in an epitaxial Fe/MgAlOx/Fe4N magnetic tunnel junction (MTJ) controlled by the bias voltage. At room temperature (RT), the TMR is measured as large as −26.7% (−38% under optimistic definition) at V = +0.45 V, and it changes the sign to be +3.2% at V = −0.6 V. The TMR sign-reversal effect is doubled compared to those of the Fe/MgO/Fe4N MTJs, which is attributed to the better lattice mismatch between Fe4N and MgAlOx as well as less N diffusion inside the tunneling barrier. First-principles calculations reveal that the change of the TMR sign originates from different symmetry-dependent tunneling channels between Fe and Fe4N electrodes under opposite bias voltages. The Fe/MgAlOx/Fe4N MTJ with voltage-controllable TMR signs and relatively large TMR ratios at RT will promote the development of versatile and reprogrammable spin-logic applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.3c00937
Chinese Library Classification Number:
Citation Information:
A sign-reversible tunneling magnetoresistance (TMR) bestows an extra control freedom to design TMR-based spintronic devices for developing spin-logic applications. Here, we demonstrate a large sign reversal of TMR in an epitaxial Fe/MgAlOx/Fe4N magnetic tunnel junction (MTJ) controlled by the bias voltage. At room temperature (RT), the TMR is measured as large as −26.7% (−38% under optimistic definition) at V = +0.45 V, and it changes the sign to be +3.2% at V = −0.6 V. The TMR sign-reversal effect is doubled compared to those of the Fe/MgO/Fe4N MTJs, which is attributed to the better lattice mismatch between Fe4N and MgAlOx as well as less N diffusion inside the tunneling barrier. First-principles calculations reveal that the change of the TMR sign originates from different symmetry-dependent tunneling channels between Fe and Fe4N electrodes under opposite bias voltages. The Fe/MgAlOx/Fe4N MTJ with voltage-controllable TMR signs and relatively large TMR ratios at RT will promote the development of versatile and reprogrammable spin-logic applications.
quote
| GB/T 7714-2015 | [1] Tianyi Ma, Yu Zhu, Pambiang Abel Dainone, et al. ACS Applied Electronic Materials, 2023(5). DOI:10.1021/acsaelm.3c00937. |
| MLA | [1] Tianyi Ma, et al., ACS Applied Electronic Materials, no. 5, 2023, https://doi.org/10.1021/acsaelm.3c00937. |
| APA | [1] Tianyi Ma, Yu Zhu, Pambiang Abel Dainone, Tongxin Chen, Xavier Devaux, Caihua Wan, Sylvie Migot, Gwladys Lengaigne, Michel Vergnat, Yu Yan, Xiufeng Han, & Yuan Lu. (2023). ACS Applied Electronic Materials(5). https://doi.org/10.1021/acsaelm.3c00937 |
| IEEE | [1] Tianyi Ma, Yu Zhu, Pambiang Abel Dainone, Tongxin Chen, Xavier Devaux, Caihua Wan, Sylvie Migot, Gwladys Lengaigne, Michel Vergnat, Yu Yan, Xiufeng Han, and Yuan Lu, ACS Applied Electronic Materials, no. 5, 2023, doi: 10.1021/acsaelm.3c00937. keywords: {magnetic tunnel junction inverse magnetoresistance symmetrydependent tunneling magnetic randomaccess memoriesShow More} |