Effect of Ru Addition on Microstructure of WC-Co Cemented Carbides AITranslate
Abstract AITranslate
The effect of ruthenium addition on the microstructure of WC-Co cemented carbides was discussed.The results show that ruthenium addition has a significant effect on the growth and average size of WC grains in WC-Co cemented carbides.With the increase of ruthenium content, the phenomenon of abnormal growth of WC grains in the cemented carbides gradually decreases until it disappears, the average grain size of WC decreases to a certain extent, but WC grain growth orientation does not show a clear tendency.After ruthenium element is added to WC-Co cemented carbides, it is mainly dissolved in the Co phase, and ruthenium grains significantly grow up by sintering.
KeyWords AITranslate
1林春芳,杜玉国,孙丹,陈蓓瑾,刘莹华.WC-(7-9)Ni-(1-2)Cr硬质合金耐蚀性能的研究[J].硬质合金,2010,27(4):224-229. 被引量:12
2刘书祯.超细晶硬质合金晶粒长大抑制剂的研究[J].稀有金属与硬质合金,2007,35(4):51-56. 被引量:21
3时凯华,昝秀颀,廖军,舒军.配碳量与碳化温度对(W,Mo)C粉末成分与结构的影响[J].中国钨业,2021,36(2):53-59. 被引量:1
1余碧荷,金永中,苏伟,钟健,赵建涛,曾守君.(V,Cr,W)C复合粉末对WC-11Ni硬质合金微观组织及力学性能的影响[J].稀有金属与硬质合金,2023,51(1):34-39.
1唐彦渊,钟志强,羊求民,王红云,徐国钻.碳含量对WC-10Co硬质合金微观组织及力学性能的影响[J].稀有金属与硬质合金,2021,49(6):73-78. 被引量:6
2冯可桃,吕健,阚高辉,郑铮辉,李莎,魏剑磊,李亚军.烧结过程氮气分压对(Ti, Nb)(C,N)基金属陶瓷组织和性能的影响[J].稀有金属与硬质合金,2021,49(6):47-54. 被引量:1
3周光杰,刘晓玮,杨文志,陈钊,金韬.含Nb或V的Q390钢板的组织与性能研究[J].热加工工艺,2021,50(23):103-106.
4肖双,罗有华,牟海川,王瑞斌,贾钧麟.热蒸发法制备以有机小分子-无机钙钛矿复合薄膜为发光层的白光PeLED[J].科学通报,2022,67(2):193-203.
5刘艳艳,肖猛,高雪松,吕非.FGH95/GH4169异质材料激光增材修复再制造界面的组织与性能研究[J].热加工工艺,2021,50(23):22-25. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
The effect of ruthenium addition on the microstructure of WC-Co cemented carbides was discussed.The results show that ruthenium addition has a significant effect on the growth and average size of WC grains in WC-Co cemented carbides.With the increase of ruthenium content, the phenomenon of abnormal growth of WC grains in the cemented carbides gradually decreases until it disappears, the average grain size of WC decreases to a certain extent, but WC grain growth orientation does not show a clear tendency.After ruthenium element is added to WC-Co cemented carbides, it is mainly dissolved in the Co phase, and ruthenium grains significantly grow up by sintering.
quote
| GB/T 7714-2015 | [1] SHI Kai-hua, ZAN Xiu-qi, SHU Jun, et al. Effect of Ru Addition on Microstructure of WC-Co Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2021(6): 79-84. |
| MLA | [1] SHI Kai-hua, et al., "Effect of Ru Addition on Microstructure of WC-Co Cemented Carbides." Rare Metals and Cemented Carbides, no. 6, 2021, pp. 79-84. |
| APA | [1] SHI Kai-hua, ZAN Xiu-qi, SHU Jun, & LIAO Jun. (2021). Effect of Ru Addition on Microstructure of WC-Co Cemented Carbides. Rare Metals and Cemented Carbides(6), 79-84. |
| IEEE | [1] SHI Kai-hua, ZAN Xiu-qi, SHU Jun, and LIAO Jun, "Effect of Ru Addition on Microstructure of WC-Co Cemented Carbides," Rare Metals and Cemented Carbides, no. 6, pp. 79-84, 2021. keywords: {WC-Co cemented carbide;Ru addition;microstructure;grain size;crystal orientation} |