Study on the Cutting Property of the Coated Cemented Carbide Tips with Gradient Structure AITranslate
Abstract AITranslate
The cutting property of the coated cemented carbide with gradient structure and those without gradient structure was studied. The effect of cobalt on the cutting properties of graded cemented carbides was studied. The cutting tests demonstrate that the cutting property of the coated cemented carbide with gradient structure is much better than those without gradient structure. The cutting life of the former doubles that of the later at hB=0. 15 mm. Meanwhile,the larger cobalt content resulted in better cutting property.
KeyWords AITranslate
1Upadhyaya A,et al.Advances in sintering hard metals[J].Materials and Design,2001,22 (6):499.
2Tsuda,K,et al.Development of functionally graded sintered hard materials[J].Powder Metallurgy,1996,39(4):296.
3Rosso M,et al.Studies of graded cemented carbides components[J].International Journal of Refractory Metals &-Hard Materials,1999,17(1-3):187.
4Hans-Olof Andren.Microstructure development during sintering and heat-treatment of cemented carbides and cermets[J].Materials Chemistry and Physics,2001,67 (1-3):209.
5Walter Lengauer,et al.Functionally graded hardmetals[J].Journal of Alloys and Compounds,2002,338 (1-2):194.
6张伟.功能梯度材料的研究现状和前景[J].自然杂志,1995,17(4):216-216.
7程继贵,王华林,夏永红,蒋阳.功能梯度硬质合金和金属陶瓷材料研究的新进展[J].材料导报,2000,14(4):16-17. 被引量:19
8王辉平,尹志民.TiCN基金属陶瓷刀片的研究[J].硬质合金,2003,20(3):133-137. 被引量:18
1崔岩,王利成,董常青,董俐言,齐明慧.累积叠轧制备Ni/Al多层复合材料[J].热加工工艺,2019,0(24):78-80. 被引量:2
2李刘合,杨海健,陈五一,朱剑豪.用于加工Inconel718的切削刀具发展现状[J].工具技术,2010,44(5):3-12. 被引量:16
3唐思文,刘德顺,李鹏南,唐文波,唐德.TiCN基梯度功能金属陶瓷的制备及其切削性能[J].功能材料,2014,45(13):13126-13130. 被引量:10
4唐思文,苏闯南,肖雄,陈宇强,李鹏南,刘德顺.微波辅助氮化烧结制备TiCN基功能梯度金属陶瓷的组织与性能[J].热加工工艺,2015,44(18):103-106. 被引量:1
5魏恒生,沈金城,姚蕾,杨海涛.高速重载火车轮毂加工刀片的材质分析[J].硬质合金,2021,38(3):165-170.
1崔岩,王利成,董常青,董俐言,齐明慧.累积叠轧制备Ni/Al多层复合材料[J].热加工工艺,2019,0(24):78-80. 被引量:2
2詹春辉,计伟,李克强,岳彩旭,李玉甫.陶瓷圆刀片车削GH4169机理研究及工艺优化[J].航空制造技术,2011,0(14):89-92. 被引量:2
3张高峰,周山麒,陈三中,邸江顺.涂层硬质合金刀具切削Inconel718合金的有限元分析[J].装备制造技术,2012(2):13-15. 被引量:1
4王菊凤,赵先锋,何林,李长虹.高温合金GH4169铣削参数优化的研究[J].现代机械,2012(2):1-3. 被引量:2
5谷萌,李丽,王飞飞,孙浩.镍基合金IN718电火花线切割单脉冲放电温度场分析[J].机械设计与制造,2013(9):151-154. 被引量:9
6刘志林,严宏志.有限元仿真预测高温合金切槽刀具寿命的初步探讨[J].硬质合金,2014,31(1):37-43. 被引量:12
7沈汛,孙剑飞,陈五一.镍基高温合金高速切削加工性[J].工具技术,2014,48(12):3-10. 被引量:6
8张颖琳,孙剑飞,陈五一.PCBN刀具车削铸造高温合金的失效机理研究[J].工具技术,2015,49(1):11-16. 被引量:1
9唐思文,苏闯南,肖雄,陈宇强,李鹏南,刘德顺.微波辅助氮化烧结制备TiCN基功能梯度金属陶瓷的组织与性能[J].热加工工艺,2015,44(18):103-106. 被引量:1
10李凯,胡显军.几种牌号刀具对Inconel 625切削性能的对比研究[J].制造技术与机床,2016(2):107-110. 被引量:4
1廖诗兰.梯度结构硬质合金涂层刀片的金相观察[J].中国钨业,2009,24(6):35-38. 被引量:1
2张武装,刘咏,贺跃辉,羊建高,龙郑易.具有梯度结构的涂层硬质合金刀片[J].中国有色金属学报,2005,15(5):757-762. 被引量:18
3胡.山特维克可乐满新型铣刀[J].工具展望,2007(6):22-22.
4张武装,刘咏,贺跃辉,黄伯云.一种特殊烧结技术对梯度结构硬质合金性能影响的研究[J].功能材料,2007,38(2):292-294. 被引量:1
5张武装,刘咏,贺跃辉,王海兵.Co含量对硬质合金梯度结构和性能的影响[J].中国钨业,2004,19(6):34-37. 被引量:11
6王社权,陈康华,徐银超,祝昌军,谢灿强,陈响明.基体梯度结构对TiN涂层硬质合金力学和切削性能的影响[J].中国有色金属学报,2011,21(4):804-809. 被引量:6
7何开文.M42拉刀的裂纹原因分析报告[J].重庆钢研,2003(28):38-42.
8苗晋琦,张鬲君,王成彪,吕建国,唐伟忠,吕反修.酸浸+等离子体刻蚀YG6微米-纳米金刚石复合涂层工具研究[J].金刚石与磨料磨具工程,2005,25(5):18-23. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
The cutting property of the coated cemented carbide with gradient structure and those without gradient structure was studied. The effect of cobalt on the cutting properties of graded cemented carbides was studied. The cutting tests demonstrate that the cutting property of the coated cemented carbide with gradient structure is much better than those without gradient structure. The cutting life of the former doubles that of the later at hB=0. 15 mm. Meanwhile,the larger cobalt content resulted in better cutting property.
quote
| GB/T 7714-2015 | [1] ZHANG Wu-zhuang, LIU Yong, HE Yue-hui. Study on the Cutting Property of the Coated Cemented Carbide Tips with Gradient Structure[J]. Rare Metals and Cemented Carbides, 2006(3): 12-14. |
| MLA | [1] ZHANG Wu-zhuang, et al., "Study on the Cutting Property of the Coated Cemented Carbide Tips with Gradient Structure." Rare Metals and Cemented Carbides, no. 3, 2006, pp. 12-14. |
| APA | [1] ZHANG Wu-zhuang, LIU Yong, & HE Yue-hui. (2006). Study on the Cutting Property of the Coated Cemented Carbide Tips with Gradient Structure. Rare Metals and Cemented Carbides(3), 12-14. |
| IEEE | [1] ZHANG Wu-zhuang, LIU Yong, and HE Yue-hui, "Study on the Cutting Property of the Coated Cemented Carbide Tips with Gradient Structure," Rare Metals and Cemented Carbides, no. 3, pp. 12-14, 2006. keywords: {cemented carbide;gradient structure;coated tip;cutting property} |