Development of RE Multiple Boride (La0.55Ba0.45)B6 and (La0.4Eu0.6)B6 Cathode Materials AITranslate
Abstract AITranslate
In view of more stringent requirement for better electric property of the relevant cathode material with the rapid development of the electron beam and ion beam technology, the paper describe the development of multiple RE boride(La0.55Ba0.45 )B6 and (La0.4 Eu0.6 )B6 cathode material. The testing results showed that its electric property is superior to that of LaB6 cathode material.
KeyWords AITranslate
1马汝广,刘丹敏,周身林,张久兴.放电等离子体烧结(SPS)制备多晶La_(0.4)Pr_(0.6)B_6块体及其发射性能研究[J].无机材料学报,2010,25(7):743-747. 被引量:5
2张宁,张久兴,包黎红,魏永峰,李晓娜.粉末粒度对SPS固相烧结La_(0.6)Eu_(0.4)B_6阴极材料的影响[J].稀有金属材料与工程,2013,42(2):311-315. 被引量:2
3张小琴,郝占忠,张海玲.稀土元素硼化物的研究进展[J].稀土,2013,34(2):74-80. 被引量:12
4包黎红,那仁格日乐,特古斯,张忻,张久兴.放电等离子烧结原位合成Lax Ce1-x B6化合物及性能研究[J].物理学报,2013(19):382-387. 被引量:6
5李录录,张忻,刘洪亮,张繁星,肖怡新,张久兴.La_(1-x)Nd_xB_6单晶的制备及热电子发射性能[J].材料导报,2017,31(18):21-24. 被引量:3
6余艺平,王松,李伟.多元镧基六硼化物固溶体材料研究进展[J].稀有金属材料与工程,2023,52(5):1954-1962.
1包黎红,张久兴,周身林.Ba掺杂对稀土硼化物GdB_6结构,晶粒取向和热发射性能的影响(英文)[J].无机材料学报,2011,26(10):1116-1120. 被引量:2
2张繁星,张忻,张久兴,梁超龙,黄颖凯.悬浮区域熔炼法制备Ce_(1-x)Pr_xB_6单晶体及其热发射性能研究[J].无机材料学报,2014,29(10):1073-1076. 被引量:7
3梁超龙,张忻,张久兴,张繁星,王杨.La_(1-x)Nd_xB_6阴极材料的制备及性能研究[J].无机材料学报,2015,30(4):363-368. 被引量:2
4成维,黄美松,苏正夫,王志坚,贾帅广,杨露辉.高纯高致密度LaB_6多晶体的制备[J].中国稀土学报,2015,33(3):323-327. 被引量:3
5李岳丽,王雯,王丽红,周青.环境中镧对水稻叶绿体功能元素的影响[J].稀土,2015,36(2):107-112. 被引量:7
6杨树颜,焦元启,骆伟新.纳米氧化镧掺杂PEO基SPEs的离子导电性能研究[J].稀土,2016,37(3):31-35.
7徐兰兰,孙丛婷,薛冬峰.稀土晶体研究进展[J].中国稀土学报,2018,36(1):1-17. 被引量:22
8许欢,王玺堂,王周福,马妍,刘浩.感应加热碳热还原合成LaB_6粉体[J].人工晶体学报,2018,47(2):354-358. 被引量:1
9陶如玉,包黎红,红莲,那仁格日乐,富泉.多元稀土硼化物Ce_xBa_(1-x)B_6的制备及表征[J].内蒙古师范大学学报:自然科学汉文版,2018,47(3):217-219. 被引量:1
10张飞鹏,施加利,张静文,包黎红,秦国强,张光磊,杨新宇,张久兴.稀土硼化物LaB_6晶体材料的弹性性质和力学性能[J].高压物理学报,2019,33(2):45-49. 被引量:1
1吴开明,徐世铮.不锈钢BaO-BaF_2渣系脱磷的试验研究[J].钢铁,1993(6):18-20. 被引量:4
2戴小平.160kA预焙铝电解槽“四低一高”电解工艺技术条件的选择[J].轻金属,2000(3):31-34. 被引量:10
3张朝晖,张彦睿,巨建涛,冯兵,蔡利勇.60t LF脱硫试验[J].炼钢,2006,22(6):38-40.
4李蒙姬,张烽,郑志良,朱永东.矿热炉碳热法生产硅基钙钡铝合金[J].铁合金,1995,26(6):19-21. 被引量:3
5Yucel BIROL.粉末冶金法制备Al-SrB_6复合材料(英文)[J].中国有色金属学报:英文版,2015,0(3):677-682.
6刘守平,唐萍.锰铁脱磷方法探讨[J].铁合金,2003,34(4):5-6. 被引量:4
7范士民,柴晓娜.烧结参数对(Ba_(0.6)Sr_(0.4))TiO_3-MgO复合陶瓷的影响[J].阜阳师范学院学报:自然科学版,2009,26(3):24-27.
8LIU Ning,YAN Guoqing,CAI Zhirang,GUO Huanyin,PENG Zhensheng,QU Zhe,ZHANG Yuheng.Charge order and spin orderof La_(0.3)Ca_(0.7)Mn_(1-x)W_(x)O_(3) system[J].科学通报:英文版,2006,51(7):770-776.
9郑树起,闵光辉,邹增大,王效志,韩建德.La_2O_3-B_4C系反应合成LaB_6粉末[J].金属学报,2001,37(4):419-422. 被引量:10
10麦克尔.科努鲁,杜游.高电压高电抗AC电弧炉的电气设计[J].宽厚板,1997,3(4):33-34.
Basic Information:
DOI:
Chinese Library Classification Number:TF304.3[冶金工程—冶金机械及自动化]
Citation Information:
In view of more stringent requirement for better electric property of the relevant cathode material with the rapid development of the electron beam and ion beam technology, the paper describe the development of multiple RE boride(La0.55Ba0.45 )B6 and (La0.4 Eu0.6 )B6 cathode material. The testing results showed that its electric property is superior to that of LaB6 cathode material.
quote
| GB/T 7714-2015 | [1] LIU Shu-ping, YANG Qing-shan, CHEN Wei-ping, et al. Development of RE Multiple Boride (La0.55Ba0.45)B6 and (La0.4Eu0.6)B6 Cathode Materials[J]. Rare Metals and Cemented Carbides, 2006(3): 8-11. |
| MLA | [1] LIU Shu-ping, et al., "Development of RE Multiple Boride (La0.55Ba0.45)B6 and (La0.4Eu0.6)B6 Cathode Materials." Rare Metals and Cemented Carbides, no. 3, 2006, pp. 8-11. |
| APA | [1] LIU Shu-ping, YANG Qing-shan, CHEN Wei-ping, LIU Jia-xiang, & LI Zhong-hua. (2006). Development of RE Multiple Boride (La0.55Ba0.45)B6 and (La0.4Eu0.6)B6 Cathode Materials. Rare Metals and Cemented Carbides(3), 8-11. |
| IEEE | [1] LIU Shu-ping, YANG Qing-shan, CHEN Wei-ping, LIU Jia-xiang, and LI Zhong-hua, "Development of RE Multiple Boride (La0.55Ba0.45)B6 and (La0.4Eu0.6)B6 Cathode Materials," Rare Metals and Cemented Carbides, no. 3, pp. 8-11, 2006. keywords: {multiple rare earth boride;cathode material;(La0. 55Ba0.45 ) B6;(La0. 4 Eu0. 6 ) B6;development} |