Study on Extraction of Scandium from Sulphuric Acid Leaching Solution of Tungsten Residue AITranslate
Abstract AITranslate
The extraction of scandium from the leaching solution of tungsten residue was carried out by P204-TBP,sulfuric acid eluted the iron in the loaded organic phase and scandium was stripped in the eluted organic phase by sodium hydroxide.The results show that in the system of 5% P204+3% TBP+ kerosene, the extraction rate of scandium is 97.37% through five-stage counter current extraction with O/A ratio of 1∶10,temperature of 25 ℃,and time of 15min.Through five-stage counter current elution by 4 mol/L H2SO4,the elution rate of iron is 98.63%,while the scandium loss rate is less than 1%.The eluted organic phase was stripped with 3mol/L sodium hydroxide.The single-stage stripping rate of scandium reaches 98.31%.By using the method,the purity of crude scandium can reach more than 82%,and the total recovery rate of scandium is more than 95%.
KeyWords AITranslate
1李力,姜锋,李汉广.新世纪钪的应用开发和科技发展前景[J].稀有金属与硬质合金,2002,30(3):38-41. 被引量:21
2李汉广,尹志民.钪的发展动态和发展战略[J].稀有金属与硬质合金,1996,24(1):47-51. 被引量:21
3朱海玲,邓海波,吴承桧,何小民.钨渣的综合回收利用技术研究现状[J].中国钨业,2010,25(4):15-18. 被引量:25
4杨秀丽,王晓辉,向仕彪,孙青,魏昶,郑诗礼.盐酸法富集钨渣中的钽和铌[J].中国有色金属学报,2013,23(3):873-881. 被引量:21
5梁勇,王瑞祥,刘俊.高纯稀土化合物制备的现状与发展[J].上海有色金属,2004,25(4):188-191. 被引量:12
6廖春生,徐刚,贾江涛,张亚文,吴声,严纯华.新世纪的战略资源—钪的提取与应用[J].中国稀土学报,2001,19(4):289-297. 被引量:46
7王克勤,于永波,王皓,陈津.赤泥盐酸浸出提取钪的试验研究[J].稀土,2010,31(1):95-98. 被引量:51
8姜平国,廖春发.从赤泥盐酸浸出液中提取钪的工艺研究[J].中国有色冶金,2012,41(1):66-68. 被引量:13
9杨革.从钨渣中提取高纯氧化钪[J].湖南有色金属,2001,17(1):18-20. 被引量:33
10徐廷华,邓佐国,李伟,余腾海.从钨渣浸出液中提取钪的研究[J].江西有色金属,1997,11(4):32-36. 被引量:13
1朱心蕊,刘旭恒,陈星宇,李江涛,何利华,赵中伟.钨冶炼渣的综合利用及发展趋势[J].矿产保护与利用,2019,39(3):119-124. 被引量:9
2孙帅,孙宏骞,宋静,曲景奎,齐涛.钪资源现状及溶剂萃取在钪提取过程中的应用研究进展[J].过程工程学报,2020,20(8):877-886. 被引量:7
3龚丹丹,李祖怡,张勇,万林生,任嗣利.钨渣回收利用技术研究现状[J].稀有金属与硬质合金,2021,49(6):1-8. 被引量:2
4张金祥,罗教生,管建红,洪侃,黄叶钿,普建,李忠岐,陈远林,郭学益.我国钨渣处理现状与研究进展[J].中国钨业,2021,36(6):62-70.
5李祖怡,张勇,郑彬涛,侯志明,龚丹丹.碱分解钨渣硫酸浸出的正交试验研究[J].稀有金属与硬质合金,2023,51(1):1-4.
6李世春,池君洲,王丽萍,李超.从废弃物中回收稀土金属钪的研究进展[J].稀有金属与硬质合金,2023,51(1):10-16. 被引量:1
7刘观发,曾超聪,王泽凯,曾祥荣,黄万抚.钨冶炼渣制备高强烧结陶粒及其性能研究[J].无机盐工业,2023,55(8):132-139.
1葛阳阳,孟建卫,张凯熙,郭静粉.含氟助剂两段酸浸提取钒钛磁铁矿尾矿中的钪[J].稀土,2022,43(4):73-80. 被引量:2
2余春荣,黄亮,徐双,李跃海,陆晓晖.钨渣脱水过程中加压过滤机的应用实践[J].中国钨业,2019,34(6):43-47.
3刘国栋,付勇,何伟,唐波,龙珍,杨颖,龙克树.中国铝土岩系中伴生钪资源富集规律及富集机制初探[J].地质论评,2021,67(4):952-972. 被引量:2
4李望,王雯博,段理哲,朱晓波.伯胺7101萃取分离钒及有机相乳化分析[J].矿冶工程,2021,41(4):76-78.
5邱叶红,董惠,朱刘.钪回收提取技术发展现状[J].中国资源综合利用,2021,39(10):145-147. 被引量:1
6冯艳虎,庄故章,周平,李子豪,晋艳玲,张培.西昌三圆石材厂废料中高钪矿物的浮选试验[J].矿冶,2021,30(6):20-28.
7Xu Wang,Xiao‑Dong Ma,Kun Su,Chun‑Fa Liao,Bao‑Jun Zhao.Fundamental studies for high temperature processing of tungsten leaching residues for alloy formation[J].钨科技(英文),2020,2(4):362-370.
8匡兵,余泽全.中国再生钨资源回收利用现状及建议[J].中国钨业,2021,36(4):1-5. 被引量:5
9王秋银,张国莹,赵煜,贾开程.湿法炼锌中废渣的综合回收利用技术研究[J].中国金属通报,2021(21):13-14.
10李仲泽.中国钨产业高质量发展的思考[J].中国钨业,2021,36(5):1-10. 被引量:5
1吴希桃,王志坚.锆渣洗水中Sc与P的萃取分离工艺及其机理研究[J].稀有金属与硬质合金,2018,46(3):1-5. 被引量:1
2郑汝伟,包申旭,张一敏.P204-TBP浸渍树脂的制备及对钒(Ⅳ)的吸附研究[J].有色金属:冶炼部分,2018(1):39-43. 被引量:3
3马朝扬,谭海翔,姚骥,黄静,虞萍,孙立贤,胡振光.P350萃取分离稀土草酸沉淀母液中草酸和盐酸的试验研究[J].湖南有色金属,2018,34(6):30-33. 被引量:3
4何艺,徐双,靳晓勤,林晓,陶莉,许海青.中国钨渣产生特性及资源化利用技术研究现状[J].中国钨业,2018,33(5):51-56. 被引量:8
5张雪凯,周康根,陈伟,雷清源,黄颖,彭长宏.酸浸-分步萃取法从赤泥中回收铁和稀土(英文)[J].中南大学学报:英文版,2019,26(2):458-466. 被引量:26
6孙振,曾理,关文娟,张贵清,王应松.P204/4PC协萃体系在酸性硫酸盐溶液中选择性萃取镍的机理研究[J].稀有金属与硬质合金,2018,46(6):25-31. 被引量:2
7曹海欧,李惠艳.某大学附属医院护士多点执业认知调查[J].解放军医院管理杂志,2018,25(12):1177-1181. 被引量:7
8万建新,任学昌,蒋煜峰,郭效军,彭波.P204-熔融石蜡固液萃取废水中铜、钴、镍[J].环境化学,2018,37(12):2688-2693.
9陈硕,王立久.酸浸法提取粉煤灰中铝铁及纳米氧化铁的制备[J].材料科学与工程学报,2018,36(6):1003-1009. 被引量:6
10周超,李勇,薛向欣.利用吡啶类离子液体萃取分离电镀污泥中的Cr^(6+)与Fe^(3+)[J].电镀与精饰,2019,41(1):41-46. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF845.1[冶金工程—有色金属冶金]
Citation Information:
The extraction of scandium from the leaching solution of tungsten residue was carried out by P204-TBP,sulfuric acid eluted the iron in the loaded organic phase and scandium was stripped in the eluted organic phase by sodium hydroxide.The results show that in the system of 5% P204+3% TBP+ kerosene, the extraction rate of scandium is 97.37% through five-stage counter current extraction with O/A ratio of 1∶10,temperature of 25 ℃,and time of 15min.Through five-stage counter current elution by 4 mol/L H2SO4,the elution rate of iron is 98.63%,while the scandium loss rate is less than 1%.The eluted organic phase was stripped with 3mol/L sodium hydroxide.The single-stage stripping rate of scandium reaches 98.31%.By using the method,the purity of crude scandium can reach more than 82%,and the total recovery rate of scandium is more than 95%.
quote
| GB/T 7714-2015 | [1] ZHOU Guo-tao, LI Qing-gang, LIU Yong-chang, et al. Study on Extraction of Scandium from Sulphuric Acid Leaching Solution of Tungsten Residue[J]. Rare Metals and Cemented Carbides, 2018(6): 1-9. |
| MLA | [1] ZHOU Guo-tao, et al., "Study on Extraction of Scandium from Sulphuric Acid Leaching Solution of Tungsten Residue." Rare Metals and Cemented Carbides, no. 6, 2018, pp. 1-9. |
| APA | [1] ZHOU Guo-tao, LI Qing-gang, LIU Yong-chang, ZHANG Gui-qing, CAO Zuo-ying, ZENG Li, & GUAN Wen-juan. (2018). Study on Extraction of Scandium from Sulphuric Acid Leaching Solution of Tungsten Residue. Rare Metals and Cemented Carbides(6), 1-9. |
| IEEE | [1] ZHOU Guo-tao, LI Qing-gang, LIU Yong-chang, ZHANG Gui-qing, CAO Zuo-ying, ZENG Li, and GUAN Wen-juan, "Study on Extraction of Scandium from Sulphuric Acid Leaching Solution of Tungsten Residue," Rare Metals and Cemented Carbides, no. 6, pp. 1-9, 2018. keywords: {tungsten residue;scandium;P204-TBP extraction;H2SO4 elution,NaOH stipping;recycle} |