Application of Advanced Aliphatic Amine Extractants in Solvent Extraction of Rare Metals AITranslate
Abstract AITranslate
Advanced aliphatic amine extractant are widely used in the metallurgical industry.This paper focuses on several commonly used advanced aliphatic amine extractant and its application in the rare metals solvent extraction process.
KeyWords AITranslate
1周岚,邵建中,柴丽琴.阳离子改性剂在棉纤维天然染料染色中的应用[J].纺织学报,2009,30(10):95-100. 被引量:32
2蔡水洪,苏元复.从盐酸溶液中萃取铟[J].华东化工学院学报,1992,18(1):6-12. 被引量:6
3张明杰,郭清富.21世纪的能源金属——锂的冶金现状及发展[J].盐湖研究,2001,9(3):52-60. 被引量:47
4李菁华.N263萃取分离钼钨的硫代盐[J].稀有金属,1989,13(4):296-300. 被引量:14
5张贵清,张启修,周康根.N1923萃取回收钛白水解废酸中的钛——反萃取参数的研究[J].矿冶工程,2003,23(2):66-68. 被引量:7
6刘公召,隋智通.萃取法从废催化剂中提取V_2O_5的研究[J].矿产综合利用,2001(6):41-44. 被引量:12
7林春生.萃取法从钼、铼溶液中回收铼[J].中国钼业,2005,29(1):41-43. 被引量:21
8李园,张治国,沈大娲,马清林.钢铁及铁质文物有机缓蚀剂的研究进展[J].化工技术与开发,2008,37(10):17-19. 被引量:10
9周小舟,曹佐英,肖连生,刘劭钢,张贵清,李青刚,曾理,关文娟,白兰.新型三叔胺萃取剂的合成及其萃取性能[J].中南大学学报:自然科学版,2017,48(3):562-569. 被引量:2
10梁建生.季铵盐类消毒剂及其应用[J].中国消毒学杂志,2012,29(2):129-131. 被引量:27
1宋强,童雄,谢贤,张文杰,许宝松,范培强,彭世文.溶剂萃取法分离提取镍和钴的研究现状及展望[J].中国有色金属学报,2023,33(6):1957-1971.
1Lei Fu.Member of Editorial Board of Rising Stars[J].中国化学:英文版,2018,36(6):555-555.
2马丽伊,徐志强,田振峰,赵爱侠,淦五二.LC-MS/MS法测定烟草中7种高级脂肪酸[J].中国烟草学报,2018,24(6):1-8. 被引量:2
3坚一明,李显,朱贤青,芦田隆一,WORASUWANNARAK Nakorn,胡振中,罗光前,姚洪,钟梅,刘景梅,马凤云,三浦孝一.低阶煤与生物质在热溶剂提质萃取过程中的相互作用(英文)[J].燃料化学学报,2019,47(1):14-22. 被引量:6
4朱建勇,张旭乾,杨辉,陆荣秀.单光照条件变化的镨/钕元素组分含量软测量[J].化工学报,2019,70(2):780-788. 被引量:4
5毛雪华,刘代俊.磷酸三丁酯—正癸醇对盐酸介质中钛的萃取[J].钢铁钒钛,2018,39(5):9-15. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TF804.2[冶金工程—有色金属冶金]
Citation Information:
Advanced aliphatic amine extractant are widely used in the metallurgical industry.This paper focuses on several commonly used advanced aliphatic amine extractant and its application in the rare metals solvent extraction process.
quote
| GB/T 7714-2015 | [1] LI Jia-hao, CAO Zuo-ying, LI Jia, et al. Application of Advanced Aliphatic Amine Extractants in Solvent Extraction of Rare Metals[J]. Rare Metals and Cemented Carbides, 2018(6): 10-18. |
| MLA | [1] LI Jia-hao, et al., "Application of Advanced Aliphatic Amine Extractants in Solvent Extraction of Rare Metals." Rare Metals and Cemented Carbides, no. 6, 2018, pp. 10-18. |
| APA | [1] LI Jia-hao, CAO Zuo-ying, LI Jia, ZHANG Gui-qing, LI Qing-gang, ZENG Li, & GUAN Wen-juan. (2018). Application of Advanced Aliphatic Amine Extractants in Solvent Extraction of Rare Metals. Rare Metals and Cemented Carbides(6), 10-18. |
| IEEE | [1] LI Jia-hao, CAO Zuo-ying, LI Jia, ZHANG Gui-qing, LI Qing-gang, ZENG Li, and GUAN Wen-juan, "Application of Advanced Aliphatic Amine Extractants in Solvent Extraction of Rare Metals," Rare Metals and Cemented Carbides, no. 6, pp. 10-18, 2018. keywords: {amine extractant;rare metals;solvent extraction} |