Occurrence State and Distribution Law of Titanium in Titanium-containing Cryolite during Preparation of Titanium/Titanium-Aluminum Alloy Powder by Aluminothermic Reduction AITranslate
Abstract AITranslate
Using sodium fluorotitanate as raw material,titanium and titanium alloys were prepared by alu-minothermic reduction at 1150℃.Titanium-containing cryolite was the by-product in the distillation stage of aluminothermic reduction.Based on the diffusion path of titanium-containing cryolite vapor,sampling and analysis of titanium-containing cryolite at different positions in the crystallization zone were carried out.XRF analysis shows that according to the sequence of the flow location of titanium-containing cryolite vapor,the titanium content(calculated as TiO2) of the titanium-containing cryolite samples decreases sharply from 10.38%to 2.70%and then basically stabilizes at 0.16%.XPS analysis shows that titanium in the titanium-containing cryolite exists mainly in the form of TiO2 and TiOS,and the titanium in the two accounts for more than 70%of the total titanium.The titanium-containing cryolite also contains a small amount of titanium nitrides,fluorides and titanium aluminum alloys.The occurrence state of titanium in the titanium-containing cryolite obtained by XRD and SEM analysis is basically consistent with XPS results.
KeyWords AITranslate
1纪腾飞,赵斌,金跃峰,刘钊.钛在海水淡化领域中的应用[J].化工装备技术,2017,38(1):9-11. 被引量:6
2刘世锋,宋玺,薛彤,马宁,王岩,王立强.钛合金及钛基复合材料在航空航天的应用和发展[J].航空材料学报,2020,40(3):77-94. 被引量:91
3贾翃,逯福生,郝斌.2020年中国钛工业发展报告[J].钛工业进展,2021,38(2):34-41. 被引量:18
4梁舒然,王凡,周冬青,常荍,白玉兴.三维打印钛板支抗前方牵引治疗骨性Ⅲ类错(牙合)畸形的初步应用[J].中华口腔医学杂志,2017,52(12):753-755. 被引量:12
1郭佳明,梁精龙,李慧,徐正震.钛铝合金及其金属间化合物制备工艺研究进展[J].矿产综合利用,2022(3):1-5.
2李森,高锋,沈东东,龙文元,李新生,王开拓,王友彬,藤田丰久,韦悦周.铝热还原工艺条件对Al-Ti-Ce中间合金物相结构和合金元素浓度的影响[J].稀有金属材料与工程,2022,51(5):1805-1812. 被引量:1
3马晓卉,佡云,崔博程.碱熔试样-电感耦合等离子体原子发射光谱法测定铌铁中硅、磷、钛[J].中国有色冶金,2022,51(3):80-83.
4朱敏,熊维,李冠,徐海萍,王静荣,杨丹丹.钛酸钡纳米线的两步水热法制备及结构表征[J].上海第二工业大学学报,2022,39(2):118-127. 被引量:1
5王聪,王伟强,董旭峰,齐民.铝含量对钛铝二元合金MAO涂层结构及亲水性的影响[J].功能材料,2022,53(6):6014-6018.
6郑贵增.过氧化氢光度法快速测定新型合金包芯钛线中的钛[J].山东冶金,2022,44(3):37-38.
7许可,许德如.江南造山带黄金洞金矿蚀变岩型金矿化形成机制研究[J].黄金科学技术,2022,30(2):151-164.
8李小莉,邓赛文,王毅民,李松,徐进力,白金峰.X射线荧光光谱在碳酸盐类矿石分析中的应用文献评介[J].冶金分析,2022,42(3):33-46.
9杜伟,周存龙,赵敬伟.铌钛对铁素体不锈钢组织和成形性的影响[J].山东冶金,2022,44(3):22-26.
10李滨,臧甲忠,于海斌,王欢,李立青,陈铁红.空心鼓状多级孔钛硅氧化物的合成及氧化-吸附脱硫性能研究[J].无机盐工业,2022,54(7):135-140.
Basic Information:
DOI:
Chinese Library Classification Number:TF823[冶金工程—有色金属冶金]
Citation Information:
Using sodium fluorotitanate as raw material,titanium and titanium alloys were prepared by alu-minothermic reduction at 1150℃.Titanium-containing cryolite was the by-product in the distillation stage of aluminothermic reduction.Based on the diffusion path of titanium-containing cryolite vapor,sampling and analysis of titanium-containing cryolite at different positions in the crystallization zone were carried out.XRF analysis shows that according to the sequence of the flow location of titanium-containing cryolite vapor,the titanium content(calculated as TiO2) of the titanium-containing cryolite samples decreases sharply from 10.38%to 2.70%and then basically stabilizes at 0.16%.XPS analysis shows that titanium in the titanium-containing cryolite exists mainly in the form of TiO2 and TiOS,and the titanium in the two accounts for more than 70%of the total titanium.The titanium-containing cryolite also contains a small amount of titanium nitrides,fluorides and titanium aluminum alloys.The occurrence state of titanium in the titanium-containing cryolite obtained by XRD and SEM analysis is basically consistent with XPS results.
quote
| GB/T 7714-2015 | [1] SHEN Zi-qiang, DI Yue-zhong, PENG Jian-ping, et al. Occurrence State and Distribution Law of Titanium in Titanium-containing Cryolite during Preparation of Titanium/Titanium-Aluminum Alloy Powder by Aluminothermic Reduction[J]. Rare Metals and Cemented Carbides, 2022(3): 1-6. |
| MLA | [1] SHEN Zi-qiang, et al., "Occurrence State and Distribution Law of Titanium in Titanium-containing Cryolite during Preparation of Titanium/Titanium-Aluminum Alloy Powder by Aluminothermic Reduction." Rare Metals and Cemented Carbides, no. 3, 2022, pp. 1-6. |
| APA | [1] SHEN Zi-qiang, DI Yue-zhong, PENG Jian-ping, WANG Yao-wu, & FENG Nai-xiang. (2022). Occurrence State and Distribution Law of Titanium in Titanium-containing Cryolite during Preparation of Titanium/Titanium-Aluminum Alloy Powder by Aluminothermic Reduction. Rare Metals and Cemented Carbides(3), 1-6. |
| IEEE | [1] SHEN Zi-qiang, DI Yue-zhong, PENG Jian-ping, WANG Yao-wu, and FENG Nai-xiang, "Occurrence State and Distribution Law of Titanium in Titanium-containing Cryolite during Preparation of Titanium/Titanium-Aluminum Alloy Powder by Aluminothermic Reduction," Rare Metals and Cemented Carbides, no. 3, pp. 1-6, 2022. keywords: {titanium-containing cryolite;aluminothermic reduction;distillation;titanium;occurrence state;distribution law} |