The Prepration and Sintering Characteristics of Nanocrystalline WC-Co Composites AITranslate

National Key Laboratory of Metal Precision Hot Processing of Harbin University of Technology;National Key Laboratory of Metal Precision Hot Processing of Harbin University of Technology;National Key Laboratory of Metal Precision Hot Processing of Harbin University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

This paper reviewed the development of the synthesis techniques of nanocrystalline WC-Co composite powders,summarized the sintering characteristics of nanocrystalline WC-Co cemented carbide.The present reaesach status is analyzed,the problems and research tendency are also discussed in the paper.

KeyWords AITranslate

nanocrystalline WC-Co composite powders sintering

1周益明,忻新泉.低热固相合成化学[J].无机化学学报,1999,15(3):273-292. 被引量:247

2邵刚勤,吴伯麟,魏明坤,袁润章.超细晶粒WC硬质合金的研制动态[J].武汉工业大学学报,1999,21(6):18-20. 被引量:37

3印红羽,盛挺,汪海宽.硬质合金低压热等静压烧结工艺[J].粉末冶金技术,1997,15(4):299-303. 被引量:16

4高勇,唐振方,黄景清,郑家概,凌育远,钟红海.纳米WC-Co复合材料制备及其烧结过程[J].硬质合金,2000,17(1):18-20. 被引量:35

5毛昌辉.高能机械研磨纳米结构WC-Co复合粉末的研究[J].稀有金属,1999,23(3):185-188. 被引量:22

6黎樵燊,谢致薇,李瑜煜,陈海燕,邓爱国.纳米硬质合金粉末压制过程的研究[J].粉末冶金技术,1999,17(2):94-98. 被引量:4

7胡茂中.2010年我国硬质合金产品质量改进的思考[J].硬质合金,1997,14(3):171-176. 被引量:2

8黄忠耿.研制和生产粒度小于0.6μm碳化钨粉的工艺技术发展动态[J].稀有金属与硬质合金,1998,26(4):51-56. 被引量:8

9仝建峰,陈大明,陈宇航,雷景轩.热压工艺参数对纳米SiC-Al_2O_3/TiC新型陶瓷刀具材料力学性能的影响[J].粉末冶金技术,2000,18(2):102-105. 被引量:5

10张立,黄伯云,吴恩熙.纳米WC—Co复合粉的烧结特征[J].硬质合金,2001,18(2):65-68. 被引量:12

1林信平,曹顺华,李炯义.现代烧结技术在制备超细和纳米硬质合金中的应用[J].粉末冶金材料科学与工程,2004,9(2):126-133. 被引量:7

2马运柱,黄伯云,范景莲,熊翔,汪登龙.纳米级(晶)钨基合金复合粉末的制备[J].粉末冶金材料科学与工程,2004,9(3):204-211. 被引量:3

3李长案,孙兰,熊计,贾成厂.球磨WC-8Co粉末的放电等离子烧结[J].四川大学学报:工程科学版,2012,44(S1):285-290. 被引量:4

4白佳声,杨慧敏,候克忠,陆明炯.微纳米硬质合金的制备及应用[J].材料导报,2004,18(8):84-88. 被引量:3

5范景莲,艾宪平,马运柱.高能球磨和放电等离子体烧结制备超细WC-8Co硬质合金[J].稀有金属,2005,29(2):129-132. 被引量:4

6史晓亮,邵刚勤,段兴龙,张卫丰,袁润章.纳米复合WC-6Co粉末的快速烧结[J].稀有金属材料与工程,2005,34(8):1283-1286. 被引量:7

7陈玮.纳米WC-Co硬质合金研究现状[J].现代制造工程,2006(1):136-138. 被引量:2

8程涛,汪重露.纳米硬质合金的研究进展[J].稀有金属与硬质合金,2006,34(3):46-50. 被引量:13

9齐志宇,李静,李成威,杨大正.高压热等静压工艺烧结超细WC-10Co复合粉烧结体[J].鞍山科技大学学报,2007,30(2):124-127. 被引量:1

10史晓亮,杨华,邵刚勤,段兴龙,周芙蓉,孙鹏.立方氮化硼-碳化钨-钴复合材料制备工艺的改进[J].机械工程材料,2007,31(4):71-73. 被引量:1

1张建兵,李小强,龙雁,陈维平,李元元.WC-6Co-1.5Al合金高能球磨-电场活化烧结工艺的研究[J].粉末冶金工业,2005,15(6):13-17.

2李长案,孙兰,熊计,贾成厂.球磨WC-8Co粉末的放电等离子烧结[J].四川大学学报:工程科学版,2012,44(S1):285-290. 被引量:4

3陈玮.纳米WC-Co硬质合金研究现状[J].现代制造工程,2006(1):136-138. 被引量:2

4孙兰,贾成厂,曹瑞军.纳米粉末烧结的研究现状与前景[J].粉末冶金技术,2006,24(2):146-150. 被引量:12

5颜杰,唐楷.硬质合金的脏化原因和解决方法[J].粉末冶金工业,2006,16(5):29-33. 被引量:16

6颜杰,唐楷,黄新,汪建昌,姜宁.硬质合金生产中的增氧反应及其影响[J].硬质合金,2006,23(4):218-221. 被引量:6

7邱友绪,李宁,张伟,文玉华,张勇,周永贵.WC-Co超细晶硬质合金晶粒长大抑制剂及其机理的研究[J].硬质合金,2006,23(4):254-257. 被引量:21

8张武装,刘咏,黄伯云.纳米晶WC-Co硬质合金的研究现状[J].材料导报,2007,21(2):79-82. 被引量:22

9高玉喜,郭志猛.钒元素对纳米钨粉在高温加热过程中颗粒长大的抑制作用[J].稀有金属快报,2007,26(4):18-21.

10张凤林,崔晓龙,朱敏,王成勇.高能球磨制备纳米WC-Co复合粉末及其SPS烧结[J].硬质合金,2007,24(2):80-83. 被引量:12

1亓家钟.粉末冶金的研究趋势[J].粉末冶金工业,1992(1):23-24.

2史晓亮,王学广,邵刚勤,段兴龙,袁润章.纳米晶WC-Co硬质合金的烧结[J].材料导报,2004,18(F04):29-32. 被引量:1

3殷志勇,成海芳,张文彬.生物技术在湿法冶金领域的应用现状及研究趋势[J].湿法冶金,2006,25(3):113-116. 被引量:13

4闫建新,李在元.粉末高速钢的研究进展[J].硬质合金,2010,27(5):316-320. 被引量:10

5唐海燕,李京社,吉传波,梁永昌,吴拓,王建磊.连铸结晶器内钢液流动的研究进展[J].河南冶金,2014,22(2):1-7. 被引量:2

6向波,刘秀庆,金大庆,贺跃辉.超细钴粉的制备及国内外的研究现状[J].材料导报:纳米与新材料专辑,2009,23(1):461-464. 被引量:5

7魏莉,姚广春,张晓明,罗洪杰.粉末冶金法制备多孔金属材料技术[J].材料导报,2004,18(7):15-18. 被引量:6

8周静,李运刚,牛江峰.金属硅粉的研究现状及发展概况[J].河北理工学院学报,2007,29(2):39-43. 被引量:1

9张春友,陈成,陈硕.节钴型梯度硬质合金的研究[J].湖南冶金,2005,33(2):3-6.

10I.肖,张兴仁,肖力子.铂族矿物性质研究和回收方法综述(Ⅰ)[J].国外金属矿选矿,2004,41(12):4-12. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]

Citation Information:

This paper reviewed the development of the synthesis techniques of nanocrystalline WC-Co composite powders,summarized the sintering characteristics of nanocrystalline WC-Co cemented carbide.The present reaesach status is analyzed,the problems and research tendency are also discussed in the paper.

quote

GB/T 7714-2015 [1] SUN Jian-fei, ZHANG Fa-ming, SHEN Jun. The Prepration and Sintering Characteristics of Nanocrystalline WC-Co Composites[J]. Rare Metals and Cemented Carbides, 2002(1): 33-37.
MLA [1] SUN Jian-fei, et al., "The Prepration and Sintering Characteristics of Nanocrystalline WC-Co Composites." Rare Metals and Cemented Carbides, no. 1, 2002, pp. 33-37.
APA [1] SUN Jian-fei, ZHANG Fa-ming, & SHEN Jun. (2002). The Prepration and Sintering Characteristics of Nanocrystalline WC-Co Composites. Rare Metals and Cemented Carbides(1), 33-37.
IEEE [1] SUN Jian-fei, ZHANG Fa-ming, and SHEN Jun, "The Prepration and Sintering Characteristics of Nanocrystalline WC-Co Composites," Rare Metals and Cemented Carbides, no. 1, pp. 33-37, 2002. keywords: {nanocrystalline;WC-Co;composite powders;sintering}