Study of Zirconium Sulfate Production Process AITranslate
Abstract AITranslate
Study is made of the process for the production of zirconium sulfate from zircon.The main Steps are as follows:alkali fusion,water washing and conversion,primary and secondary crystallization;centrifugal packing.This unique process has solved the problems in Zr and Na separation,Zr and Fe separation and crystal morphology etc.The product quality can meet the requirements of the customers both at home and abroad.
KeyWords AITranslate
1傅鹰.大学普通化学[M].北京:人民教育出版社,1981.7.
2麦耶尔松.稀有金属冶金学教程[M].北京:冶金工业出版社,1960..
1李中军,黄银霞,要红昌,杨民乐,陈建立.碳化锆碱熔制备氧氯化锆的研究[J].稀有金属,2006,30(3):415-418. 被引量:7
2陈静,张弟妹,陈周玲,潘荣楷.由锆英石制备硫酸锆的工艺研究[J].广东化工,2010,37(6):10-11. 被引量:1
3黎志万,刘小龙,任萌,张嘉,刘锦洪.用工业级氯氧化锆制备硫酸锆[J].湿法冶金,2016,35(4):339-341.
4刘柳辉,吴海国.硫酸锆生产工艺的改进[J].湖南有色金属,2002,18(5):16-17. 被引量:1
5唐晓星,马继飞,刘忠英,李玉兰,钱渊.电感耦合等离子体发射光谱法测定铍盐中痕量硼[J].分析试验室,2020,39(8):910-913. 被引量:3
1倪亮,姚毅,王文渊,刘继平,张建军,旷翔,张先林.僵蚕新型伪品中标志物硼砂的定性定量检测方法研究[J].中药材,2021,44(8):1848-1850. 被引量:4
2张建东,陈伟东,吴延科,徐志高,王力军.氯氧化锆生产中废碱水和锆硅渣回收利用研究进展[J].稀有金属,2010,34(6):936-944. 被引量:9
3Zhang, Jiandong, Wang, Lijun, Jiang, Dongmin.Decomposition process of zircon sand concentrate with CaO-NaOH[J].稀有金属:英文版,2012(4):410-414. 被引量:3
4陈静,张弟妹,陈周玲,潘荣楷.由锆英石制备硫酸锆的工艺研究[J].广东化工,2010,37(6):10-11. 被引量:1
5朱露,罗远辉,张建东,张力,王力军.NaOH-KOH混合碱分解锆英砂的工艺研究[J].稀有金属,2012,36(5):799-803. 被引量:3
6陈伟东,闫国庆,赵健翔,张亚增,闫淑芳.CaCl_2和NaOH复合分解锆英砂工艺研究[J].钛工业进展,2013,30(1):38-40. 被引量:7
7张建东,陈洋,张顺利,王力军.氧化钙和氢氧化钠混合分解锆英砂的工艺及机理[J].钛工业进展,2013,30(2):38-42. 被引量:5
8黄淑梅,陈伟东,王运锋,何蕾,郭薇.中国氧氯化锆产业现状及发展对策[J].钛工业进展,2014,31(2):1-7. 被引量:13
9罗六保,温盛红,谢志鹏.氧氯化锆湿法生产工艺及其废渣处理研究进展[J].化学研究,2016,27(6):791-796. 被引量:2
10孙宏骞,宋静,孙帅,曲景奎,吕伟,齐涛.锆英砂在氢氧化钠亚熔盐中的分解动力学(英文)[J].中国有色金属学报:英文版,2019,29(9):1948-1955. 被引量:1
1刘柳辉,吴海国.硫酸锆生产工艺的改进[J].湖南有色金属,2002,18(5):16-17. 被引量:1
2陈景友.碳热法冶炼硅锆合金的实践[J].铁合金,2008,39(5):24-25. 被引量:1
3宋兴诚,沐彩兰,皇甫智伟.低锡高铅粗合金电解试验研究[J].中国有色冶金,1998,31(9):23-29.
4黎志万,刘小龙,任萌,张嘉,刘锦洪.用工业级氯氧化锆制备硫酸锆[J].湿法冶金,2016,35(4):339-341.
5于学成,王泽彬,王岷,孙越.碱式硫酸锆的制备条件研究[J].稀有金属快报,2005,24(2):33-34.
6雷湘,陈金魁,吴海国,周美红.工业氧化铍生产过程中用硫酸铅取代锆盐除磷的研究[J].湖南有色金属,2011,27(6):17-19.
7纪东海.硫化铜精矿综合利用的研究[J].山东冶金,2001,23(2):42-44. 被引量:5
8宋兴诚,沐彩兰.低锡高铅粗合金电解试验研究[J].云锡科技,1997,24(3):18-31.
9孙志宏,任万益,姚高波.工业铝电解槽炉膛再造技术探讨[J].轻金属,2007(6):33-36. 被引量:2
10张建新.电炉生产60Si2Mn钢过程吸氮分析及控制[J].新疆钢铁,2009(1):29-31.
Basic Information:
DOI:
Chinese Library Classification Number:TF841.4[冶金工程—有色金属冶金]
Citation Information:
Study is made of the process for the production of zirconium sulfate from zircon.The main Steps are as follows:alkali fusion,water washing and conversion,primary and secondary crystallization;centrifugal packing.This unique process has solved the problems in Zr and Na separation,Zr and Fe separation and crystal morphology etc.The product quality can meet the requirements of the customers both at home and abroad.
quote
| GB/T 7714-2015 | [1] CHENG Quan-hui. Study of Zirconium Sulfate Production Process[J]. Rare Metals and Cemented Carbides, 2002(1): 28-32. |
| MLA | [1] CHENG Quan-hui. "Study of Zirconium Sulfate Production Process." Rare Metals and Cemented Carbides, no. 1, 2002, pp. 28-32. |
| APA | [1] CHENG Quan-hui. (2002). Study of Zirconium Sulfate Production Process. Rare Metals and Cemented Carbides(1), 28-32. |
| IEEE | [1] CHENG Quan-hui, "Study of Zirconium Sulfate Production Process," Rare Metals and Cemented Carbides, no. 1, pp. 28-32, 2002. keywords: {zirconium sulfate;alkalifusion;conversion;iron removal crystallization;process} |