Phosphate-based Ce(IV) Ion-Imprinted Polymers for Separation of Berkelium: Testing the Homologue Imprinting Approach for Heavy Actinides AITranslate
Abstract AITranslate
The present study focuses on the synthesis of phosphate-based ion imprinted polymers (IIPs) using a chemical homologue (cerium(IV)) for the fast and selective separation of Bk(IV) from a large number of fission products. Two imprinted phosphate-based gels, poly(bis[2-(methacryloyloxy)ethyl] phosphate) (poly-BMEP) and poly(bis[2-(methacryloyloxy)ethyl] phosphate-co-acrylic acid) (poly-(BMEP-AA)) have been prepared by in situ UV polymerization. The imprinting has been achieved by complexation of the phosphate-based monomers with the Ce(IV) ion. The desorption of Ce(IV) ions from the imprinted gels has been studied with H2O2. The prepared gels have been characterized by FE-SEM, FT-IR, XRD, and XPS. The imprinted gels have been shown to extract Ce(IV) ions selectively from an 8 mol L–1 HNO3 medium in the presence of fission products (Ba, Ru, Tb). DFT calculations show formation of a 1:4 Ce(IV):BMEP complex. The presence of acrylic acid (AA) has been shown to improve the kinetics of Ce(IV) uptake owing to the decrease in the tortuosity of the polymeric structure due to the AA presence. The imprinted gels though do not show kinetic selectivity toward Ce(IV) compared to non-imprinted gels; they show thermodynamic selectivity toward Ce(IV), indicating the inability of the non-imprinted gels to retain Ce(IV) for longer periods. Also, the imprinted gels have been found to be more selective compared to solvent extraction with BMEP as the complexing agent. These two imprinted gels were used to extract Bk, which was produced in 11B + 238U at a 66 MeV beam energy. The extraction by IIPs have been found to be much faster with the reduction in overall extraction time by ∼80% relative to the earlier reported method though with a lesser selectivity for some elements. The present approach, as guided by DFT calculations, offers a possibility of preparing IIPs for the selective extraction of heavy actinides and trans-actinides using their chemical homologues as the imprinting ion.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01342
Chinese Library Classification Number:
Citation Information:
The present study focuses on the synthesis of phosphate-based ion imprinted polymers (IIPs) using a chemical homologue (cerium(IV)) for the fast and selective separation of Bk(IV) from a large number of fission products. Two imprinted phosphate-based gels, poly(bis[2-(methacryloyloxy)ethyl] phosphate) (poly-BMEP) and poly(bis[2-(methacryloyloxy)ethyl] phosphate-co-acrylic acid) (poly-(BMEP-AA)) have been prepared by in situ UV polymerization. The imprinting has been achieved by complexation of the phosphate-based monomers with the Ce(IV) ion. The desorption of Ce(IV) ions from the imprinted gels has been studied with H2O2. The prepared gels have been characterized by FE-SEM, FT-IR, XRD, and XPS. The imprinted gels have been shown to extract Ce(IV) ions selectively from an 8 mol L–1 HNO3 medium in the presence of fission products (Ba, Ru, Tb). DFT calculations show formation of a 1:4 Ce(IV):BMEP complex. The presence of acrylic acid (AA) has been shown to improve the kinetics of Ce(IV) uptake owing to the decrease in the tortuosity of the polymeric structure due to the AA presence. The imprinted gels though do not show kinetic selectivity toward Ce(IV) compared to non-imprinted gels; they show thermodynamic selectivity toward Ce(IV), indicating the inability of the non-imprinted gels to retain Ce(IV) for longer periods. Also, the imprinted gels have been found to be more selective compared to solvent extraction with BMEP as the complexing agent. These two imprinted gels were used to extract Bk, which was produced in 11B + 238U at a 66 MeV beam energy. The extraction by IIPs have been found to be much faster with the reduction in overall extraction time by ∼80% relative to the earlier reported method though with a lesser selectivity for some elements. The present approach, as guided by DFT calculations, offers a possibility of preparing IIPs for the selective extraction of heavy actinides and trans-actinides using their chemical homologues as the imprinting ion.
quote
| GB/T 7714-2015 | [1] Amol Mhatre, Chhavi Agarwal, Tarak Nath Nag, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01342. |
| MLA | [1] Amol Mhatre, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01342. |
| APA | [1] Amol Mhatre, Chhavi Agarwal, Tarak Nath Nag, Arunasis Bhattacharyya, & Rahul Tripathi. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01342 |