A Dual-Responsive, Freezing-Tolerant Hydrogel Sensor and Related Thermal- and Strain-Sensitive Mechanisms AITranslate
Abstract AITranslate
Freezing-tolerant and conductive hydrogels have attracted tremendous interest as promising materials for flexible sensors under the gelid condition. In this work, a freezing-tolerant, dual-responsive hydrogel sensor was developed by using an ionic–glycerol hybrid hydrogel. The fabricated hydrogel sensor was demonstrated to detect efficiently different temperatures ranging from −30 to 100 °C or to detect both small strains (e.g., 1%, 2%, 4%) and large strains (e.g., 10%, 20% and 30%) as a freezing-tolerant strain sensor. A systematic investigation was conducted to explore the thermal- and strain-sensitive mechanisms of the obtained hydrogel. It was found that the resistance of the hydrogel rapidly increased as the temperature (T) decreased. In addition, the strain sensitivity increased as T decreased from 0 °C to −30 °C. Surprisingly, an abrupt resistance increase was observed when the tensile strain of the gel reached a critical value (e.g., 2620% at 0 °C) or upon moving the hydrogel from 25 to −10 to −30 °C. Such a sharp increase in resistance was found to be mainly caused by the abrupt fracture of a vast amount of the inner hydrogel network at large strains or the appearance of microcrystals in the gel network at low temperatures. This work provides fundamental and practical insights into fabricating functional freezing-tolerant hydrogel sensors for engineering applications.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.0c01346
Chinese Library Classification Number:
Citation Information:
Freezing-tolerant and conductive hydrogels have attracted tremendous interest as promising materials for flexible sensors under the gelid condition. In this work, a freezing-tolerant, dual-responsive hydrogel sensor was developed by using an ionic–glycerol hybrid hydrogel. The fabricated hydrogel sensor was demonstrated to detect efficiently different temperatures ranging from −30 to 100 °C or to detect both small strains (e.g., 1%, 2%, 4%) and large strains (e.g., 10%, 20% and 30%) as a freezing-tolerant strain sensor. A systematic investigation was conducted to explore the thermal- and strain-sensitive mechanisms of the obtained hydrogel. It was found that the resistance of the hydrogel rapidly increased as the temperature (T) decreased. In addition, the strain sensitivity increased as T decreased from 0 °C to −30 °C. Surprisingly, an abrupt resistance increase was observed when the tensile strain of the gel reached a critical value (e.g., 2620% at 0 °C) or upon moving the hydrogel from 25 to −10 to −30 °C. Such a sharp increase in resistance was found to be mainly caused by the abrupt fracture of a vast amount of the inner hydrogel network at large strains or the appearance of microcrystals in the gel network at low temperatures. This work provides fundamental and practical insights into fabricating functional freezing-tolerant hydrogel sensors for engineering applications.
quote
| GB/T 7714-2015 | [1] Yonggan Yan, Luxing Wei, Xiaoyong Qiu, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.0c01346. |
| MLA | [1] Yonggan Yan, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.0c01346. |
| APA | [1] Yonggan Yan, Luxing Wei, Xiaoyong Qiu, Jinlong Shao, Hanlian Liu, Xin Cui, Jun Huang, Lei Xie, Zhenfeng Hu, & Chuanzhen Huang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.0c01346 |
| IEEE | [1] Yonggan Yan, Luxing Wei, Xiaoyong Qiu, Jinlong Shao, Hanlian Liu, Xin Cui, Jun Huang, Lei Xie, Zhenfeng Hu, and Chuanzhen Huang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.0c01346. keywords: {conductive hydrogel;freezing tolerance;selfhealing;strain sensor;temperature sensor;sensing mechanism} |