Effect of Forming Process on Sintering Density and Microstructure Defects of WC-6Ni Fine Grained Cemented Carbides AITranslate
Abstract AITranslate
The forming processes of molding, cold isostatic pressing and molding + cold isostatic pressing were adopted for the preparation of WC-6Ni cemented carbides. The effects of different forming processes on the phase composition,physical properties and microstructure of WC-6Ni cemented carbides were main- ly discussed. The results show that the WC-6Ni fine grained cemented carbide with density of 98 % arid HV hardness of 1 457 can be obtained by sintering at 1 410 ℃ for 1 h of the WC-6Ni compact from molding + cold isostatic pressing. The above cemented carbide has uniformly distributed microstructure,and there are no voids and defects such as Ni pools on its surface.
KeyWords AITranslate
1温庆丰,刘莹,黄伟峰,索双富,刘向锋,王玉明.机械密封端面材料WC-Ni硬质合金的研究进展[J].粉末冶金材料科学与工程,2011,16(1):1-6. 被引量:28
2吴月天.机械密封用耐磨、耐蚀硬质材料-YCN3合金研制[J].硬质合金,1996,13(2):95-98. 被引量:10
3孙兰,李长案,贾成厂.放电等离子烧结压力对超细WC-Co硬质合金性能的影响[J].硬质合金,2012,29(1):19-23. 被引量:8
4林小为,肖志瑜,李小峰,朱权利,张文.放电等离子烧结制备超细晶WC-3Co硬质合金的组织和性能[J].粉末冶金材料科学与工程,2012,17(4):462-467. 被引量:14
5陈慧,彭玲玲,姜中涛,邓莹,涂铭旌.真空烧结温度对WC-TiC-TaC-Co硬质合金组织和性能的影响[J].粉末冶金工业,2015,25(3):33-36. 被引量:9
6罗电宏,马荣骏.对超细粉末团聚问题的探讨[J].湿法冶金,2002,21(2):57-61. 被引量:20
7孙五四,伏坤,李行,粟一峰,周建华.超粗晶WC粉的制备工艺研究[J].稀有金属与硬质合金,2016,44(2):13-17. 被引量:5
8羊建高,吕健,朱二涛,陈颢,郭圣达.连续还原碳化法制备纳米WC-Co复合粉研究[J].有色金属科学与工程,2013,4(5):23-27. 被引量:24
1刘强,陈吉,杨明川.真空烧结烧结温度和保温时间对WC-6%Ni细晶硬质合金组织及性能的影响[J].硬质合金,2017,34(6):393-397. 被引量:2
2何兵.不同水灰比对RPC基体性能的影响[J].科技创新导报,2018,15(10):92-94.
3马翔,黄德信,粘洪强,夏金峰.添加Y2O3对CaF2陶瓷烧结和抗水化性的影响[J].耐火材料,2018,52(1):40-43. 被引量:1
4王娴娴,马伯江,曹同坤.原位生成纳米晶对冷焊熔涂层组织与耐磨性能的影响[J].青岛科技大学学报:自然科学版,2018,39(5):53-57.
5袁亚,张娟荣,陈辉.Cu含量对Mo_5Si_3-Cu复合材料显微组织和力学性能的影响[J].有色金属工程,2018,8(5):7-10. 被引量:1
6张稳稳,罗兵辉,高阳,柏振海.Fe/Ni比对WC-Fe-Ni硬质合金微观组织及性能的影响[J].中国有色金属学报,2018,28(9):1798-1807. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TF125.3[冶金工程—粉末冶金]
Citation Information:
The forming processes of molding, cold isostatic pressing and molding + cold isostatic pressing were adopted for the preparation of WC-6Ni cemented carbides. The effects of different forming processes on the phase composition,physical properties and microstructure of WC-6Ni cemented carbides were main- ly discussed. The results show that the WC-6Ni fine grained cemented carbide with density of 98 % arid HV hardness of 1 457 can be obtained by sintering at 1 410 ℃ for 1 h of the WC-6Ni compact from molding + cold isostatic pressing. The above cemented carbide has uniformly distributed microstructure,and there are no voids and defects such as Ni pools on its surface.
quote
| GB/T 7714-2015 | [1] LIU Qiang, CHEN Ji, YANG Ming-chuan. Effect of Forming Process on Sintering Density and Microstructure Defects of WC-6Ni Fine Grained Cemented Carbides[J]. Rare Metals and Cemented Carbides, 2018(5): 79-82. |
| MLA | [1] LIU Qiang, et al., "Effect of Forming Process on Sintering Density and Microstructure Defects of WC-6Ni Fine Grained Cemented Carbides." Rare Metals and Cemented Carbides, no. 5, 2018, pp. 79-82. |
| APA | [1] LIU Qiang, CHEN Ji, & YANG Ming-chuan. (2018). Effect of Forming Process on Sintering Density and Microstructure Defects of WC-6Ni Fine Grained Cemented Carbides. Rare Metals and Cemented Carbides(5), 79-82. |
| IEEE | [1] LIU Qiang, CHEN Ji, and YANG Ming-chuan, "Effect of Forming Process on Sintering Density and Microstructure Defects of WC-6Ni Fine Grained Cemented Carbides," Rare Metals and Cemented Carbides, no. 5, pp. 79-82, 2018. keywords: {WC-6 Ni cemented carbide;forming process;molding;cold isostatic pressing;density;microstructure defect} |