Effect of the Crystal Type of Violet Tungsten Oxides on Particle Size of Ultra-fine Tungsten Carbide Powder AITranslate
Abstract AITranslate
Using rod-shaped and needle-shaped violet tungsten oxides as raw materials, ultra-fine tungsten powders and ultra-fine tungsten carbide powders were prepared. The effects of rod-shaped and needle- shaped violet tungsten oxides on particle size of ultra-fine tungsten carbide powders were studied by using scanning electron microscope,specific surface meter,laser particle size distribution analyzer and X-ray dif- fractometer. The results show that high-quality ultra-fine tungsten carbide powder with finer particle size can be prepared by using needle-shaped violet tungsten oxide as the raw material.
KeyWords AITranslate
1姜文伟,陈响明.氧化钨微观结构的研究[J].稀有金属与硬质合金,2009,37(3):8-11. 被引量:1
2陈绍衣.超细钨粉、碳化钨粉研制方法的述评——推荐用传统流程生产超细碳化钨粉[J].中国钨业,1999,14(5):146-149. 被引量:16
3廖寄乔,黄志锋,吕海波,陈绍衣,邹志强.不同氧化钨氢还原制取超细钨粉[J].中南工业大学学报,2000,31(1):51-55. 被引量:27
4陈绍衣.紫色氧化钨制取钨粉[J].中南矿冶学院学报,1994,25(5):607-611. 被引量:19
5彭泽辉,李玲.紫色氧化钨制取工艺的研究及其应用[J].稀有金属与硬质合金,2003,31(2):8-11. 被引量:16
6张秋和,谢中华,陈树茂,王文华,钟映兰,赵会团.超细碳化钨粉工业生产实践[J].中国钨业,2009,24(6):32-34. 被引量:3
7宋志华,郭亨群,吴冲浒,吴其山.以紫钨为原料制备纳米钨粉体的研究[J].稀有金属材料与工程,2011,40(12):2216-2220. 被引量:9
1姜春辉.装舟量及还原时间对氧化钨物相形貌的影响[J].福建冶金,2019,48(2):35-37.
2张璐,陆必志,徐涛.超细碳化钨制备关键技术及评价方法研究的新进展[J].硬质合金,2019,36(6):460-471. 被引量:13
3喻相标,肖杰,郭少毓,肖义钰,廖春发,姜平国.蓝钨氢还原制备钨粉工艺研究[J].有色金属科学与工程,2021,12(3):35-41. 被引量:4
4谢凡,时凯华,顾金宝.传统方法制备超细WC粉末的质量控制研究进展[J].稀有金属与硬质合金,2021,49(3):31-36. 被引量:2
5潘锋,刘家义,杜占,朱庆山.超细碳化钨制备过程及机理研究进展[J].化工学报,2021,72(11):5455-5467. 被引量:4
6魏庭民,李志锋,林钊,张永会,陈伟豪.紫色氧化钨制备工艺研究[J].世界有色金属,2022(20):163-165.
1丁辉,李潇.碳化钨、碳化钼的制取及研究进展[J].产业科技创新,2020(15):37-38.
2刘志芳,梁瑜,钟腾飞,郭永忠,覃伟坚,汤昌仁.WC粉末碳化工艺与球磨时间对亚微晶硬质合金显微组织与性能的影响[J].中国钨业,2019,34(6):48-53. 被引量:5
3汪振华,刘奎,黄雷,袁军堂.放电等离子烧结WC-6wt.%Co-VC超细晶硬质合金力学性能和微观组织研究[J].南京理工大学学报,2020,44(5):524-530. 被引量:2
4谢凡,时凯华,顾金宝.优质WC用氧化钨的质量控制[J].硬质合金,2020,37(6):472-481. 被引量:2
5喻相标,肖杰,郭少毓,肖义钰,廖春发,姜平国.蓝钨氢还原制备钨粉工艺研究[J].有色金属科学与工程,2021,12(3):35-41. 被引量:4
6潘锋,刘家义,杜占,朱庆山.超细碳化钨制备过程及机理研究进展[J].化工学报,2021,72(11):5455-5467. 被引量:4
7张华民,陈贵华,蒋福海.粉体分散方法对细WC生产过程中粒度变化的影响[J].四川有色金属,2021(4):31-35. 被引量:1
8丁紫阳,白玲,晋玉霞,马宗彬.WC添加量对Ni基等离子熔覆层组织与性能的影响[J].稀有金属与硬质合金,2022,50(1):32-36. 被引量:1
9李梦超,王璐,杨帆,薛正良.CO-CO_(2)混合气体还原WO_(3)至WO_(2.72)的反应行为[J].中国有色金属学报,2022,32(3):866-882. 被引量:2
10全温灿,艾志龙,吴彤,史冠勇,豆志河.自蔓延高温合成制备碳化钨粉的热力学研究[J].江西冶金,2022,42(2):13-17.
1陈丽杰,田磊,徐志峰,谢中华,聂华平.不同氧含量的氧化钨粉对超细钨粉制备的影响[J].有色金属:冶炼部分,2018(6):61-66. 被引量:10
2瑞稻.东芝研发出负极材料采用紫钨的超高速充放电锂电池[J].电力设备管理,2018,0(6):91-91.
3宋翰林,姜平国,刘文杰,汪正兵.氧化钨氢还原动力学的研究进展[J].有色金属科学与工程,2017,8(5):64-69. 被引量:6
4周成,王海滨,王西龙,马捷,宋晓艳.纯相低氧纳米WC-Co复合粉的制备[J].稀有金属材料与工程,2017,46(12):3887-3892.
5黄伟国,刘孝伟,陈理,徐志彬,沈浩宇,吴永新.活性炭结构特性对铅炭电池性能的影响[J].蓄电池,2018,55(5):220-224. 被引量:4
6陈丽杰,谢中华,王瑞祥,田磊,聂华平.氧化钨粉还原碳化机理分析及超细碳化钨粉的制备[J].稀有金属与硬质合金,2018,46(2):11-15. 被引量:7
7陆必志.超细碳化钨粉末团粒特性及其对硬质合金晶粒异常长大的影响[J].硬质合金,2017,34(4):233-242. 被引量:5
8王东升,张素玲,魏磊,卢艳红,景学敏.用于低温浆态床二甲醚水蒸气重整制氢的水解组分γ-Ga_2O_3的制备与表征[J].燃料化学学报,2018,46(6):666-672. 被引量:2
9杜磊,曹晓晖,杨少华,赵彦龙,占先知.热电池Cu_3V_2O_8正极材料的水热制备及放电性能研究[J].电源技术,2018,42(9):1347-1348. 被引量:1
10张烁,宋江凤,潘复生,刘强,杨丽.微量硼添加对镁合金组织和性能影响的研究进展[J].材料导报,2018,32(19):3405-3413. 被引量:4
Basic Information:
DOI:
Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]
Citation Information:
Using rod-shaped and needle-shaped violet tungsten oxides as raw materials, ultra-fine tungsten powders and ultra-fine tungsten carbide powders were prepared. The effects of rod-shaped and needle- shaped violet tungsten oxides on particle size of ultra-fine tungsten carbide powders were studied by using scanning electron microscope,specific surface meter,laser particle size distribution analyzer and X-ray dif- fractometer. The results show that high-quality ultra-fine tungsten carbide powder with finer particle size can be prepared by using needle-shaped violet tungsten oxide as the raw material.
quote
| GB/T 7714-2015 | [1] XIANG Pei-yun, ZHANG Hua-min. Effect of the Crystal Type of Violet Tungsten Oxides on Particle Size of Ultra-fine Tungsten Carbide Powder[J]. Rare Metals and Cemented Carbides, 2018(5): 75-78. |
| MLA | [1] XIANG Pei-yun, and ZHANG Hua-min. "Effect of the Crystal Type of Violet Tungsten Oxides on Particle Size of Ultra-fine Tungsten Carbide Powder." Rare Metals and Cemented Carbides, no. 5, 2018, pp. 75-78. |
| APA | [1] XIANG Pei-yun, & ZHANG Hua-min. (2018). Effect of the Crystal Type of Violet Tungsten Oxides on Particle Size of Ultra-fine Tungsten Carbide Powder. Rare Metals and Cemented Carbides(5), 75-78. |
| IEEE | [1] XIANG Pei-yun and ZHANG Hua-min, "Effect of the Crystal Type of Violet Tungsten Oxides on Particle Size of Ultra-fine Tungsten Carbide Powder," Rare Metals and Cemented Carbides, no. 5, pp. 75-78, 2018. keywords: {violet tungsten oxide;crystal type;ultra-fine tungsten powder;ultra-fine tungsten carbide powder;particle size} |