Effect of Particle Morphology of Tungsten Powders on Mixing Uniformity of Carbon Black Blending and Quality of Tungsten Carbide Powders AITranslate
Abstract AITranslate
Mixing Uniformity of tungsten powders and carbon black after carbon blending for tungsten pow- ders with different particle morphology in the same equipment was studied as well as the quality of subse- quent tungsten carbide powders. The results show that the particle morphology of tungsten powders has a great effect on the uniformity of the W+C mixture after carbon blending. The tungsten powder with dis- perse particles is more uniformly mixed with carbon black,and the produced tungsten carbide powder has a lower content of free carbon and W2C.
KeyWords AITranslate
1吴悦梅,熊计,赖人铭.碳含量对WC-Co硬质合金显微组织的影响及其控制[J].硬质合金,2008,25(3):179-185. 被引量:25
2田建华.粗颗粒钨粉配碳新工艺的研究[J].硬质合金,2006,23(2):79-83. 被引量:4
1张华民,蒋福海.添加微量液体石蜡对超粗钨粉配炭及碳化效果的影响[J].稀有金属与硬质合金,2021,49(4):76-80.
1刘宝刚,马启林,刘超,彭馨可,朱肖运,季晴.超音速火焰喷涂88WC-12Co涂层的抗氧化性能[J].粉末冶金材料科学与工程,2018,23(4):422-426.
2司景航,周雪松.两性聚丙烯酰胺的水分散聚合及其在纸张增强中的应用[J].造纸科学与技术,2017,36(5):51-57. 被引量:2
3罗虞霞,高峰,王大锋.双尺度WC-CoCr涂层的组织结构分析[J].热喷涂技术,2018,10(3):33-37. 被引量:1
4王涛,徐冲,路媛媛,郭溪溪,杜锦铮,肖鱼,刘德健.WC体积分数对激光熔注WC/NiBSi复合材料层组织和性能的影响[J].应用激光,2018,38(4):517-521. 被引量:2
5郭圣达,鲍瑞,刘亮,杨平,易健宏,羊建高,陈颢.原位合成复合粉制备超细WC-Co硬质合金[J].稀有金属材料与工程,2017,46(12):3977-3982. 被引量:7
6冀国娟,高峰,王大锋.碳化钨喷涂粉末在超音速火焰喷涂过程中的失碳研究[J].热喷涂技术,2018,10(3):38-42. 被引量:3
7马国政,雍青松,王海斗,何鹏飞,徐滨士.调制周期对纳米多层类石墨薄膜力学性能及摩擦学性能的影响[J].机械工程学报,2018,0(15):92-99. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:TG135.5[一般工业技术—材料科学与工程]
Citation Information:
Mixing Uniformity of tungsten powders and carbon black after carbon blending for tungsten pow- ders with different particle morphology in the same equipment was studied as well as the quality of subse- quent tungsten carbide powders. The results show that the particle morphology of tungsten powders has a great effect on the uniformity of the W+C mixture after carbon blending. The tungsten powder with dis- perse particles is more uniformly mixed with carbon black,and the produced tungsten carbide powder has a lower content of free carbon and W2C.
quote
| GB/T 7714-2015 | [1] LONG Ai-wu, XIE Yong-cai. Effect of Particle Morphology of Tungsten Powders on Mixing Uniformity of Carbon Black Blending and Quality of Tungsten Carbide Powders[J]. Rare Metals and Cemented Carbides, 2018(5): 72-74. |
| MLA | [1] LONG Ai-wu, and XIE Yong-cai. "Effect of Particle Morphology of Tungsten Powders on Mixing Uniformity of Carbon Black Blending and Quality of Tungsten Carbide Powders." Rare Metals and Cemented Carbides, no. 5, 2018, pp. 72-74. |
| APA | [1] LONG Ai-wu, & XIE Yong-cai. (2018). Effect of Particle Morphology of Tungsten Powders on Mixing Uniformity of Carbon Black Blending and Quality of Tungsten Carbide Powders. Rare Metals and Cemented Carbides(5), 72-74. |
| IEEE | [1] LONG Ai-wu and XIE Yong-cai, "Effect of Particle Morphology of Tungsten Powders on Mixing Uniformity of Carbon Black Blending and Quality of Tungsten Carbide Powders," Rare Metals and Cemented Carbides, no. 5, pp. 72-74, 2018. keywords: {tungsten powder particle morphology;carbon blending;mixing uniformity;tungsten carbidepowder;disperse particle;free carbon;W2C} |