Thermodynamic Analysis and Research on the Production of Lithium Metal by Vacuum Thermal Reduction AITranslate
Abstract AITranslate
The silicothermic reaction of lithia in vacuum is analyzed from thermodynamics,and its minimum temperature and the corresponding dew point temperature under different conditions are calculated. The results show that the reaction temperature and the corresponding clew-point temperature should be over 900 ℃ and 606 ℃ respectively to obtain the liquid-condensed lithium by silicothermic reduction of lithia. The verification test was carried out in a vacuum silicothermic reducing furnace to obtain the condensed lithium metal.
KeyWords AITranslate
1狄晓亮,庞全世,李权.金属锂提取工艺比较分析[J].盐湖研究,2005,13(2):45-52. 被引量:24
2游清治.锂在高新技术领域中的应用及进展[J].新疆有色金属,2003,26(S2):70-72. 被引量:14
3游清治.锂在玻璃陶瓷工业中的应用[J].世界有色金属,2000,25(2):26-31. 被引量:26
4张明杰,郭清富.21世纪的能源金属——锂的冶金现状及发展[J].盐湖研究,2001,9(3):52-60. 被引量:47
5曹大义.真空热还原制锂工艺的技术经济分析[J].有色金属:冶炼部分,2003(2):33-33. 被引量:5
1谢苏云,彭晓东,郑笑芳,魏群义.真空硅热还原制备金属锂研究[J].轻金属,2012(6):21-24. 被引量:4
2郑笑芳,彭晓东,苏中华,魏群义.真空硅热直接还原制备镁锂合金研究[J].真空科学与技术学报,2012,32(11):1021-1025. 被引量:1
3冯俊小,林佳,周敬之.金属锂还原罐内化学反应与传热耦合特性[J].北京科技大学学报,2014,36(10):1287-1291.
4刘畅,黄润,袁溢,袁鹏,张恒.攀枝花钛精矿真空碳热还原热力学模拟研究[J].钢铁钒钛,2015,36(4):13-18. 被引量:3
5王潇.高纯金属锂精炼工艺的改进方法分析[J].冶金丛刊,2017(5):232-233. 被引量:1
1刘帅,张宗旺,张建良,王振阳.高钛型高炉渣钛提取工艺研究现状及发展展望[J].中国冶金,2020,0(3):1-7. 被引量:14
2牛立斌,许臻,彭建洪,王晓刚,樊子民.气相合金化制备镁锌二元合金的研究[J].真空科学与技术学报,2015,35(6):685-688. 被引量:1
3岳跃辉,黄润,刘鹏胜,陈朝轶,张金柱.攀枝花钛精矿的真空碳热还原试验[J].中国冶金,2016,26(7):21-25. 被引量:1
4张士举,刘松利,谢金洋.钛精矿配碳还原的过程优化[J].矿产保护与利用,2017,37(4):73-80.
5李忠岐,洪侃,陈冬英,徐建兵,赖耀斌,梁鑫.金属锂制备工艺研究进展[J].新疆有色金属,2019,42(5):82-84. 被引量:4
6王冬斌,梁精龙,邓孝纯,王晶.锂资源提取与回收及锂制备工艺研究现状[J].无机盐工业,2020,52(6):8-12. 被引量:10
7尤晶,王耀武,贺晓军.碳酸锂煅烧制备氧化锂的工艺研究[J].轻金属,2020(11):4-6. 被引量:1
8逄启寿,李彬,张雨开.锂电解槽的热场分析[J].有色金属工程,2021,11(1):62-67.
1段春才,钟吕炎.降低碱渣中氧化锂含量的途径探讨——Li_2CO_3—Na_2CO_3—H_2O 系相图的应用[J].新疆有色金属,1991,0(4):24-28.
2李志华,戴永年,薛怀生.真空碳热还原氧化镁的热力学分析及实验验证[J].有色金属,2005,57(1):56-59. 被引量:28
3冷文波,罗大为,沈卓身.可伐合金在模拟现场N_2/H_2O二元气氛下的氧化行为[J].北京科技大学学报,2006,28(12):1126-1130.
4Minfang Han Ze Liu Su Zhou Lian Yu.Influence of Lithium Oxide Addition on the Sintering Behavior and Electrical Conductivity of Gadolinia Doped Ceria[J].材料科学技术:英文版,2011,27(5):460-464. 被引量:3
5新技术与成果[J].中国金属通报,1996,0(44):18-18.
6ParezanovicMSpiegel,朱文英,王波.露点温度对冷轧DP和Ti-IF钢选择氧化的影响[J].世界钢铁,2004,4(6):26-32. 被引量:4
7陈殿斐.处理黄金属尾矿砂制做玻璃品的方法[J].黄金科学技术,2005,13(3):6-6.
8周士凯,王蓉,王文学.结晶器冷却水系统压强损失计算[J].重型机械,2010(S1):228-231.
9张长桥,主沉浮,于萍,魏云鹤,张晓茹,高峰,牟善良.热镀Ni_3Al耐蚀合金镀层液态冷凝过程的分子动力学模拟研究[J].材料工程,2003,31(3):7-10.
10周恒龙,王智增,徐杨.连续退火炉炉内露点温度高故障分析与控制[J].金属世界,2017(2):46-49.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.263[金属学及工艺—金属材料]
Citation Information:
The silicothermic reaction of lithia in vacuum is analyzed from thermodynamics,and its minimum temperature and the corresponding dew point temperature under different conditions are calculated. The results show that the reaction temperature and the corresponding clew-point temperature should be over 900 ℃ and 606 ℃ respectively to obtain the liquid-condensed lithium by silicothermic reduction of lithia. The verification test was carried out in a vacuum silicothermic reducing furnace to obtain the condensed lithium metal.
quote
| GB/T 7714-2015 | [1] DI Yue-zhong, DONG Wei-wei, FENG Nai-xiang, et al. Thermodynamic Analysis and Research on the Production of Lithium Metal by Vacuum Thermal Reduction[J]. Rare Metals and Cemented Carbides, 2009(1): 5-8. |
| MLA | [1] DI Yue-zhong, et al., "Thermodynamic Analysis and Research on the Production of Lithium Metal by Vacuum Thermal Reduction." Rare Metals and Cemented Carbides, no. 1, 2009, pp. 5-8. |
| APA | [1] DI Yue-zhong, DONG Wei-wei, FENG Nai-xiang, WANG Yao-wu, WU Xiao-lei, & HU Wen-xin. (2009). Thermodynamic Analysis and Research on the Production of Lithium Metal by Vacuum Thermal Reduction. Rare Metals and Cemented Carbides(1), 5-8. |
| IEEE | [1] DI Yue-zhong, DONG Wei-wei, FENG Nai-xiang, WANG Yao-wu, WU Xiao-lei, and HU Wen-xin, "Thermodynamic Analysis and Research on the Production of Lithium Metal by Vacuum Thermal Reduction," Rare Metals and Cemented Carbides, no. 1, pp. 5-8, 2009. keywords: {vacuum thermal reduction;lithia;lithium metal;thermodynamic analysis} |