daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Nd_2O_3 Recovery from Sintered NdFeB Scrap AITranslate

Department of Chemistry, Mianyang Teachers College;Department of Chemistry, Mianyang Teachers College;Department of Chemistry, Mianyang Teachers College;Department of Chemistry, Mianyang Teachers College;Department of Chemistry, Mianyang Teachers College
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The process flowsheet of Nd2O3 recovery from the scrap of sintered NdFeB magnet is studied. Based on the chemical properties of the elements in the scrap, Na2SO4 double-salt precipitation and oxalate secondary precipitation were employed in Nd2O3 recovery respectively. Both the impurity content and recovery rate are compared between the different recovery methods to obtain simple and feasible process conditions of high benefit. The test results show that rare earth elements are precipitated more completely by Na2SO4 double-salt precipitation, the product also has a higher purity and the Nd2O3 recovery is more than 82%.

KeyWords AITranslate

sintered NdFeB magnet scrap Nd2O3 recovery Na2SO4 double-salt precipitation

1杨沂凤,李锡英,黄贞岚,吴晓.从钕铁硼磁体的废料中提取氧化钕的工艺方法[J].江西化工,1999(2):33-35. 被引量:5

2张万琰,吴光源.从钕铁硼废料中回收稀土及氧化钴的条件试验[J].江西有色金属,2001,15(4):23-26. 被引量:12

3肖荣晖.钕铁硼生产中废料的回收及利用[J].有色冶炼,2001,30(1):23-25. 被引量:26

4苏华.NdFeB废料回收Nd_2O_3工艺试验及实践[J].稀有金属与硬质合金,1999(2):40-42. 被引量:7

5王毅军,刘宇辉,翁国庆,李四勇,刘荣丽,王素玲.盐酸优溶法回收NdFeB废料中稀土元素的研究与生产[J].稀有金属与硬质合金,2007,35(2):25-27. 被引量:13

6王毅军,刘宇辉,郭军勋,王素玲,翁国庆.用盐酸优溶法从NdFeB废料中回收稀土[J].湿法冶金,2006,25(4):195-197. 被引量:30

1唐杰,杨梨容,赵导文,张林,刘畅.烧结Nd-Fe-B磁体废料回收Nd2O3的方法研究[J].稀有金属与硬质合金,2020(1):5-8.

2孟凡伟,何桂荣.烧结钕铁硼二次资源的回收利用[J].四川稀土,2009(3):18-20. 被引量:1

3魏成富,代强,唐杰,杨梨容,李想,张林.硫酸复盐法回收NdFeB废料中含铁水的处理[J].绵阳师范学院学报,2010,29(5):38-40. 被引量:8

4董传博,刘敏,赖伟鸿,尹小文,王雁,岳明,索红莉.硫化物除杂法回收钕铁硼废料中稀土元素的研究[J].硅酸盐通报,2013,32(10):2127-2132. 被引量:4

5刘晓杰,许涛,于亚辉,肖春,包一凡.ICP-AES法测定钕铁硼废料中非稀土杂质[J].稀土,2013,34(6):51-55. 被引量:3

6刘晓杰,许涛,郝茜,崔建国.钕铁硼磁性材料生产工艺及其废料综合利用的研究进展[J].稀有金属与硬质合金,2014,42(3):48-53. 被引量:8

7张晓伟,李梅,阳建平,柳召刚,胡艳宏,王觅堂,刘佳.复盐沉淀法分离络合浸出液中稀土研究[J].中南大学学报:自然科学版,2014,45(9):2952-2958. 被引量:6

8尹小文,刘敏,赖伟鸿,董传博,岳明,索红莉.草酸盐沉淀法回收钕铁硼废料中稀土元素的研究[J].稀有金属,2014,38(6):1093-1098. 被引量:17

9赖伟鸿,刘敏,尹小文,索红莉,岳明.NH_3-OH体系中共沉淀法同时回收钕铁硼废料中Nd-Pr-Co-Fe[J].稀有金属,2015,39(1):68-74. 被引量:7

10邓永春,吴胜利,姜银举,李海啸.直接还原-渣金熔分法回收钕铁硼废料[J].稀土,2015,36(5):8-13. 被引量:11

1唐杰,杨梨容,赵导文,张林,刘畅.烧结Nd-Fe-B磁体废料回收Nd2O3的方法研究[J].稀有金属与硬质合金,2020(1):5-8.

2许轩,贾晓峥,荆鹏,刘宝仓,张军.钕铁硼废料综合回收技术的研究进展[J].稀土,2023,44(1):32-53. 被引量:1

3刘晓杰,许涛,郝茜,崔建国.钕铁硼磁性材料生产工艺及其废料综合利用的研究进展[J].稀有金属与硬质合金,2014,42(3):48-53. 被引量:8

4赖伟鸿,刘敏,尹小文,索红莉,岳明.NH_3-OH体系中共沉淀法同时回收钕铁硼废料中Nd-Pr-Co-Fe[J].稀有金属,2015,39(1):68-74. 被引量:7

5王东杰,许涛,王素梅,于小征,郝茜,张翼明.钐钴合金中钴的测定方法研究[J].稀土,2015,36(1):89-92. 被引量:3

6唐杰,张铭杰,王晓军,赵导文,张林,魏成富.物理法整体再利用废弃Nd-Fe-B合金研究[J].稀有金属,2015,39(9):782-786. 被引量:2

7唐杰,魏成富,王晓军,赵导文,陈亚君.废弃Nd-Fe-B磁体的回收技术研究[J].稀有金属与硬质合金,2016,44(2):54-57. 被引量:1

8聂帅,刘鹏宇,李宝城,田佳,鲍叶琳,刘兵.钕铁硼合金中13种元素辉光放电质谱法定量分析研究[J].稀有金属,2016,40(8):756-762. 被引量:7

9李宏煦,王帅,李超.稀土元素回收技术及其生命周期循环分析[J].稀有金属,2016,40(9):945-954. 被引量:13

10左泽军,李正,吕灵灵,高明军,刘晨光.从FCC烟气脱硫污泥中提取稀土试验研究[J].湿法冶金,2016,35(5):436-439. 被引量:2

1党光耀,房建国,韩作振,刘志钧.矸石电厂粉煤灰制备微晶玻璃预提取铁、铝的研究[J].能源环境保护,2005,19(5):24-26.

2曾佑群.亚铁盐处理铁氰化钾废水[J].广东化工,2015,42(11):186-187.

3李现涛,岳明,ZAKOTNIK Miha,刘卫强,张东涛,左铁镛.Regeneration of waste sintered Nd-Fe-B magnets to fabricate anisotropic bonded magnets[J].稀土学报:英文版,2015,33(7):736-739. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:X758[环境科学与工程—环境工程]

Citation Information:

The process flowsheet of Nd2O3 recovery from the scrap of sintered NdFeB magnet is studied. Based on the chemical properties of the elements in the scrap, Na2SO4 double-salt precipitation and oxalate secondary precipitation were employed in Nd2O3 recovery respectively. Both the impurity content and recovery rate are compared between the different recovery methods to obtain simple and feasible process conditions of high benefit. The test results show that rare earth elements are precipitated more completely by Na2SO4 double-salt precipitation, the product also has a higher purity and the Nd2O3 recovery is more than 82%.

quote

GB/T 7714-2015 [1] TANG Jie, WEI Cheng-fu, ZHAO Dao-wen, et al. Nd_2O_3 Recovery from Sintered NdFeB Scrap[J]. Rare Metals and Cemented Carbides, 2009(1): 9-11.
MLA [1] TANG Jie, et al., "Nd_2O_3 Recovery from Sintered NdFeB Scrap." Rare Metals and Cemented Carbides, no. 1, 2009, pp. 9-11.
APA [1] TANG Jie, WEI Cheng-fu, ZHAO Dao-wen, LIN Hong, & TIAN Gui-hua. (2009). Nd_2O_3 Recovery from Sintered NdFeB Scrap. Rare Metals and Cemented Carbides(1), 9-11.
IEEE [1] TANG Jie, WEI Cheng-fu, ZHAO Dao-wen, LIN Hong, and TIAN Gui-hua, "Nd_2O_3 Recovery from Sintered NdFeB Scrap," Rare Metals and Cemented Carbides, no. 1, pp. 9-11, 2009. keywords: {sintered NdFeB magnet;scrap;Nd2O3;recovery;Na2SO4 double-salt precipitation}