Study of Electrochemical Property of LiFePO_4 Anode Material of Ti4+ doped Modified Lithium-ion Battery AITranslate

School of Physics and Engineering, Sun Yat -sen University;School of Physics and Engineering, Sun Yat -sen University;School of Physics and Engineering, Sun Yat -sen University;School of Physics and Engineering, Sun Yat -sen University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Lil-yTiy FePO4 is synthesized by Ti doping with solid-phase processs, tudy is made of the effect of doped Ti content, roasting temperature and duration, as well as the electrochemical properties of lithium ion battery. The following optimum technological parameters were confirmed through Latin orthogonal experi- ment [L9 (3^3)] : doped Ti^4+ content 1% (x), the roasting temperature 700 ℃, roasting duration 16 h. The test results proves that the optimized synthesis technology is good for improvement of electrochemical property of lithium ion battery anode material.

KeyWords AITranslate

lithium ion battery anode material LiFePO4 orthogonal test Ti^4+ doping

1Duong T Q. USABC and PNGV test procedures[J].J Power Sources, 2000,89 (2) : 244-248.

2Zhang X, Ross P N, Kostecki R,et al. Diagnostic characterization of high power lithium-ion batteries for use in hybrid electric vehicles[J].J Electrochem Soc, 2001,148 (5):A463-A470.

3Padhi A K,Nanjundawamy K S,Goodenough J B. Phospho-olivines as positive-electrode materials for rechargeable lithium batteries[J]. J Electrchem Soc, 1997, 144 (4):1 188-1 194.

4Padhi A K,Nanjundawamy K S,Goodenough J B,et al. Effect of structure on the Fe^3+/Fe^2+ redox couple in iron phosphates[J].J Electrchem Soc, 1997,144 (5):1 609- 1 613.

5Andersson A S, Thomas J O. The source of first-cycle capacity loss in LiFePO4 [J].J Power Sources, 2001,97- 98: 498-502.

6Yamada A, Chung S C, Hinokuma k. Optimized LiFePO4 for lithium battery cathodes[J].J Electrchem Soc, 2001,148(3) :A224-A229.

7Croce F, Epifanio A D, Hassoun J, et al. A novel concept for the synthesis of an improved LiFePO4 lithium battery cathode[J].Electrochem and Solid State Lett, 2002,5 (3) :A47-AS0.

8Park K S,Son J T,Chung H T,et al. Surface modification by silver coating for improving electrochemical properties of LiFePO4[J]. Solid State Communications, 2004,129 (5) :311-314.

9Qu T, Tian Y W, Ding Y, et al. Optimized synthesis technology of LiFePO4 for Li-ion battery[J].Trans Nonferrous Met Soc China, 2005,15 ( 3 ) : 583-588.

10Huang H,Yin S C, Nazar L F. Approaching theoretical capacity of LiFePO4 at room temperature at high rates[J]. Electrochem and Solid State Lett, 2001,4(10): A170-A172.

1张胜利,杨胜杰,宋延华,李维.锂离子电池正极材料LiFePO_4掺杂改性研究进展[J].电源技术,2010,34(3):299-302. 被引量:3

2胡伟,钟盛文,黄冰.富锂锰基正极材料的改性及电化学性能研究[J].有色金属科学与工程,2014,5(4):32-36. 被引量:7

3李立平.铝、钛、铜元素掺杂对磷酸铁锂正极材料性能影响的研究进展[J].广州化学,2022,47(5):1-8.

1刘旭恒,黄少波,赵中伟,王德志.Nb^(5+)掺杂LiFePO_4/C的反应挤出合成[J].中国有色金属学报,2012,22(11):3236-3240. 被引量:1

2黄霞.富锂锰基层状正极材料的发展现状[J].中国锰业,2015,33(2):9-13. 被引量:3

3吴汉杰,梁兴华,毛杰.锰基锂正极材料Li_(1.2)Ni_(0.13)Co_(0.13)Mn_(0.54)O_2的制备与电化学特性研究[J].化工新型材料,2016,44(9):139-141. 被引量:5

4黄小丽,岳波,王俊安,李延俊.高性能锂离子电池正极材料LiFePO_4/C的制备及表征[J].四川有色金属,2016(4):54-57.

5于天恒,徐国锋,李建玲.富锂材料Li[Li_(0.2)Mn_(0.54)Co_(0.13)Ni_(0.13)]O_2的ZrO_2包覆及电化学性能[J].有色金属科学与工程,2017,8(1):51-55. 被引量:1

6吴汉杰,梁兴华.富锂锰基正极材料Li_(1.2)Ni_(0.13)Co_(0.13)Mn_(0.54)O_2的Zn^(2+)掺杂改性[J].材料导报,2017,31(6):25-28. 被引量:4

7高玉梅,杨文鑫,刘萍,陈卉.层状富锂锰基NCM正极材料包覆与掺杂改性[J].电源技术,2017,41(8):1198-1201. 被引量:2

8杨陈,向延鸿,章顺坤,龙博,陈经玲,唐淑敏,唐欢,廖启军,田林.Co掺杂对富锂锰基正极材料Li1.2Ni0.2Mn0.6O2电化学性能的影响[J].人工晶体学报,2018,47(3):629-634. 被引量:6

9王雷,向延鸿,廖启军,田林,吴贤文,吴显明,熊利芝,何则强.葡萄糖的添加对富锂锰基正极材料Li1.2Ni0.2Mn0.6O2的影响[J].吉首大学学报:自然科学版,2019,40(3):47-52.

10何晶晶,段建国,曹雁冰,王贤树,王丁,张英杰.LiMnPO_(4)/C复合锂离子电池正极材料超价离子掺杂改性研究[J].有色设备,2023,37(1):72-77.

1唐致远,高飞,薛建军,余明远,郭稳尚.锂离子电池正极材料LiFePO_4的制备及电化学性能研究[J].天津大学学报,2007,40(4):468-472. 被引量:5

2伍凌,王志兴,李新海,李灵均,郑俊超,郭华军,刘久清.前驱体掺杂-常温球磨还原制备Ti^(4+)掺杂LiFePO_4[J].中南大学学报:自然科学版,2009,40(2):288-293. 被引量:9

3丁士华,徐琴,张倩,曾卓玮,邓涛.Ti^(4+)掺杂对α-BZN结构与介电性能的影响[J].西华大学学报:自然科学版,2013,32(4):14-17.

4汪敏,杨猛,马立群,王禹,张栩,李悦,沈晓冬.Ti掺杂对锂离子电池正极材料Li_2FeSiO_4结构及电化学性能影响[J].南京工业大学学报:自然科学版,2016,38(2):64-69. 被引量:1

5王先友,白艳松,杨秀康,舒洪波,吴强.锂含量对富锂正极材料Li_(1+x)[Ni_(0.5)Co_(0.2)Mn_(0.3)]_(1-x)O_2(x=0.091,0.115,0.138)结构、形貌及电化学性能的影响[J].湘潭大学自然科学学报,2012,34(3):48-54. 被引量:2

6王秋艳,徐连义,张艳丽,王晓明,谢嫚.V_2O_5包覆对Li_(1.6)(Fe_(0.2)Ni_(0.2)Mn_(0.6))O_(2.6)材料的表面改性(英文)[J].稀有金属材料与工程,2014,43(3):530-534.

7杨平,张传福,戴曦,樊友奇,湛菁,蒋伟燕.正极材料Li(Ni_(l/3)Co_(l/3-x)Mn_(l/3))M_xO_2(M=Ti,Mg)的合成及性能[J].中国有色金属学报,2009,19(1):101-107. 被引量:7

8曹阳,陈孝康,祝志东.聚乙炔的固体电解质Lil电池及其性能[J].苏州大学学报:自然科学版,1991,7(4):431-434.

9刘柱揆,许守东,周鑫,刘振松,陈勇,覃日升.基于模拟变电站运行状态的全站交流二次回路检验方法[J].南方电网技术,2013,7(3):99-103. 被引量:4

10余仲宝,王静,万新华,刘庆国.共混材料Li_(1.04)Mn_2O_4/LiNi_(0.94)Co_(0.06)O_2为正极的锂离子蓄电池性能[J].电源技术,2003,27(5):419-421.

Basic Information:

DOI:

Chinese Library Classification Number:TM912.9[电气工程—电力电子与电力传动]

Citation Information:

Lil-yTiy FePO4 is synthesized by Ti doping with solid-phase processs, tudy is made of the effect of doped Ti content, roasting temperature and duration, as well as the electrochemical properties of lithium ion battery. The following optimum technological parameters were confirmed through Latin orthogonal experi- ment [L9 (3^3)] : doped Ti^4+ content 1% (x), the roasting temperature 700 ℃, roasting duration 16 h. The test results proves that the optimized synthesis technology is good for improvement of electrochemical property of lithium ion battery anode material.

quote

GB/T 7714-2015 [1] QU Tao, SHEN Pei-kang, YAO Guo-liang, et al. Study of Electrochemical Property of LiFePO_4 Anode Material of Ti4+ doped Modified Lithium-ion Battery[J]. Rare Metals and Cemented Carbides, 2007(4): 1-5.
MLA [1] QU Tao, et al., "Study of Electrochemical Property of LiFePO_4 Anode Material of Ti4+ doped Modified Lithium-ion Battery." Rare Metals and Cemented Carbides, no. 4, 2007, pp. 1-5.
APA [1] QU Tao, SHEN Pei-kang, YAO Guo-liang, & XU Jia-hong. (2007). Study of Electrochemical Property of LiFePO_4 Anode Material of Ti4+ doped Modified Lithium-ion Battery. Rare Metals and Cemented Carbides(4), 1-5.
IEEE [1] QU Tao, SHEN Pei-kang, YAO Guo-liang, and XU Jia-hong, "Study of Electrochemical Property of LiFePO_4 Anode Material of Ti4+ doped Modified Lithium-ion Battery," Rare Metals and Cemented Carbides, no. 4, pp. 1-5, 2007. keywords: {lithium ion battery;anode material;LiFePO4;orthogonal test;Ti^4+ doping}