Influence of Cu Doping on the Electro-chemical Property of MI(NiCoMnAlCu)5.0 Hydrogen Storage Alloy AITranslate

central south university;central south university;central south university;central south university
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A series of low-Co type hydrogen storage alloys are prepared by vacuum induction melting. Through X-ray diffraction (XRD) and electrochemistry, systematical study and analysis is made of the elec trochemical performances (maximum discharge capacity, high-rate capability and recycle stability), the mi crostructure and kinetic characteristics of hydrogen storage alloys.

KeyWords AITranslate

Ni/MH battery hydrogen storage alloy low-Co type x-ray diffraction (XRD) electroche.micalperformance

1Wada M, Yoshinaga H,Kajita O,et al. Production of copper-alloy complex granules for nickel/metal hydrides electrodes[J]. J Alloys Comp, 1993,192:167-169.

2潘洪革.Co对MlNi_(4.3-x)Co_xAl_(0.7)贮氢电极动力学性能的影响[J].中国有色金属学报,1999,9(3):453-457. 被引量:11

3陈立新,雷永泉,朱光明,王启东.掺杂Fe对贮氢合金Ml(Ni-Co-Mn-Ti)_5电化学性能的影响[J].稀有金属材料与工程,1998,27(3):135-138. 被引量:17

4陈兵,李宁,涂铭旌.低钴型稀土基贮氢合金的研究[J].机械,2001,28(4):65-67. 被引量:5

5周志刚,谭玲生,朴英子,刘雪省,冯颖,于英浩,汪继强.Co 含量对 LaNi_5 型贮氢合金电性能的影响[J].电源技术,1997,21(4):153-155. 被引量:9

6林玉芳,李蓉,张羊换,陈梅艳,王新林.Cu对MI(NiAlMnCoCu)_(5.1)贮氢合金电化学性能的影响[J].功能材料,2003,34(3):291-293. 被引量:13

1杨素霞,李媛,刘治平,杨淑琴,韩树民.Fe部分替代Cu对低钴AB_5型贮氢合金相结构和电化学性能的影响[J].物理化学学报,2010,26(8):2144-2150. 被引量:12

2张珑玲.低温烧结时间对AB_5型贮氢合金电极电化学动力学性能的影响[J].功能材料,2010,41(11):1978-1981.

1张艳红,王培培,王仲民,倪成员,颜瑞.快凝对MmNi_(5-x)(CoMn)_x合金电化学性能的影响[J].桂林电子科技大学学报,2011,31(2):168-172.

2刘宝忠,胡梦娟,李安铭,吉力强,张宝庆,朱惜林.Microstructure and electrochemical characteristics of La_(0.7)Ce_(0.3)Ni_(3.75)Mn_(0.35)Al_(0.15)Cu_(0.75-x)(V_(0.81)Fe_(0.19))_x hydrogen storage alloys[J].稀土学报:英文版,2012,30(8):769-774.

3Muhammad-Sadeeq,Adetunji Balogun,王仲民,黄贺伟,刘文平,倪成员,李高.LaNi_(4.1-x)Co_(0.6)Mn_(0.3)Al_x储氢合金结构及电化学储氢性能研究[J].桂林电子科技大学学报,2012,32(6):508-513.

4周顺,孙泰,唐仁衡,肖方明.无镨钕AB_5型Mm(Ni,Co,Mn,Al)_5合金储氢及电化学性能研究[J].中国稀土学报,2013,31(1):60-70. 被引量:8

5胡智,黄晓巍,陈杨辉.EDTA-甘氨酸法制备SmBaCo_2O_(5+δ)阴极材料及其性能[J].物理化学学报,2013,29(12):2585-2591. 被引量:4

6彭雯琦,戴豪,邓年进,卢照,蓝志强,郭进.Fe部分取代Co对La_(0.7)Zr_(0.1)Mg_(0.2)Ni_(2.75)Co_(0.75-x)Fe_x(x=0,0.05,0.1,0.15,0.2)合金储氢性能的影响[J].材料导报,2014,28(2):25-29. 被引量:3

7李忠岐,尹延西,胡志方,田丽森,王鑫,江洪林.Zr_(0.5)La_(0.5)Ni_(1.5)Fe_(0.5)储氢合金的制备及其显微组织[J].稀有金属材料与工程,2015,44(7):1796-1799.

8秦海青,刘文平,林峰,张振军,张建伟,雷晓旭.纳米铜粉对储氢合金电极电化学性能的影响[J].有色金属工程,2016,6(1):18-21. 被引量:3

9徐申东,方亮,丁晓丽.影响TiMn_x非计量比合金储氢容量的结构因素[J].物理化学学报,2016,32(3):780-786. 被引量:1

10赵军军,冯佃臣,胡峰,蔡颖,王西涛.Fe部分替代Mn对AB_5型储氢合金结构与电化学性能的影响[J].内蒙古科技大学学报,2016,35(2):157-160. 被引量:1

1尹树峰,李全安,文九巴,张荥渊,张清.低Co贮氢合金的研究进展[J].稀有金属材料与工程,2004,33(9):913-917. 被引量:8

2唐与谌.高容量镍—金属氢化物电池用贮氢合金[J].国外金属材料,1990(3):21-26. 被引量:1

3刘红,韩莹,程云阶,丛伟.储氢合金的性质及发展趋势[J].沈阳航空工业学院学报,2000,17(1):38-41. 被引量:1

4苗鹤,林燕,李锐,高明霞,雷永泉,潘洪革.热处理对贮氢电极合金La_(0.7)Mg_(0.3)Ni_(2.45)Co_(0.75)Mn_(0.1)Al_(0.2)的微结构与电化学性能的影响(英文)[J].中山大学学报:自然科学版,2007,46(B06):310-311. 被引量:1

5同艳维,高家诚,邓刚,张雪峰,王能为.氧含量对V_(2-x)Ti_(0.5)Cr_(0.5)NiO_x(x=0~0.35)贮氢合金组织结构和电化学性能的影响(英文)[J].稀有金属材料与工程,2015,44(5):1052-1056. 被引量:1

6李全安,陈云贵,涂铭旌.热处理对快淬贮氢合金组织和电化学性能的影响[J].稀土,2004,25(1):5-8. 被引量:7

7唐与谌.Ni—MH电池及贮氢合金的生产[J].国外金属材料,1991(5):31-32.

8张清,李全安,文九巴,张兴渊.镀镍对AB_5型贮氢合金电化学性能的影响[J].表面技术,2006,35(3):23-24. 被引量:3

9徐艳辉,陈长聘,王启东.新型储氢合金电极Ti_3Ni_2的电化学性能[J].稀有金属材料与工程,2001,30(1):23-26. 被引量:8

10王利伟,金自力,张羊换,曾敏,林郁芳,王新林.La-Mg-Ni系贮氢合金的研究进展[J].金属功能材料,2009,16(2):46-50. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TG139.7[一般工业技术—材料科学与工程]

Citation Information:

A series of low-Co type hydrogen storage alloys are prepared by vacuum induction melting. Through X-ray diffraction (XRD) and electrochemistry, systematical study and analysis is made of the elec trochemical performances (maximum discharge capacity, high-rate capability and recycle stability), the mi crostructure and kinetic characteristics of hydrogen storage alloys.

quote

GB/T 7714-2015 [1] HUANG Ke-long, YANG Guo-li, TAN Fei-peng, et al. Influence of Cu Doping on the Electro-chemical Property of MI(NiCoMnAlCu)5.0 Hydrogen Storage Alloy[J]. Rare Metals and Cemented Carbides, 2007(4): 6-8.
MLA [1] HUANG Ke-long, et al., "Influence of Cu Doping on the Electro-chemical Property of MI(NiCoMnAlCu)5.0 Hydrogen Storage Alloy." Rare Metals and Cemented Carbides, no. 4, 2007, pp. 6-8.
APA [1] HUANG Ke-long, YANG Guo-li, TAN Fei-peng, & XU Gu-ya. (2007). Influence of Cu Doping on the Electro-chemical Property of MI(NiCoMnAlCu)5.0 Hydrogen Storage Alloy. Rare Metals and Cemented Carbides(4), 6-8.
IEEE [1] HUANG Ke-long, YANG Guo-li, TAN Fei-peng, and XU Gu-ya, "Influence of Cu Doping on the Electro-chemical Property of MI(NiCoMnAlCu)5.0 Hydrogen Storage Alloy," Rare Metals and Cemented Carbides, no. 4, pp. 6-8, 2007. keywords: {Ni/MH battery;hydrogen storage alloy;low-Co type;x-ray diffraction (XRD);electroche.micalperformance}