Extraction and Recovery of Cobalt from the Heap Leaching Solution of Copper-Cobalt Ore with HBL110 AITranslate
Abstract AITranslate
A new process was applied of copper extraction with Mextral 984 Hat first and then cobalt extraction with a new extractant of HBL110,to recover cobalt from the heap leaching solution of copper-cobalt ore containing such impurities as iron.The effects were investigated of extractant concentration and saponification rate,equilibrium pH value,temperature and phase ratio on cobalt extraction.The experimental results show that cobalt extraction rate is over 95% after four-stage countercurrent extraction under the conditions as follows:extractant concentration of 50.5%,saponification rate of 50%,equilibrium pH value of 2.4~2.6,phase ratio of 1∶1,temperature of 30 ℃ and time of 5 min.The loaded organic phase was washed by pure water and then cobalt was stripped.The stripping rate of cobalt is more than 94% after four-stage countercurrent stripping with 0.7mol/L H2SO4 solution under the conditions as follows:phase ratio of 8∶1,temperature of 40℃and time of 5min.Cobalt is enriched and separated from such impurities as iron,manganese and magnesium,and its concentration is 20g/L in the stripped solution.
KeyWords AITranslate
1胡宇杰.采用非洲某铜钴矿生产铜钴合金的工艺研究[J].湖南工业大学学报,2012,26(3):20-24. 被引量:4
2曹异生.世界钴工业现状及前景展望[J].中国金属通报,2007(42):30-34. 被引量:32
3张超,钟宏,王帅.镍、钴分离与回收技术研究进展[J].铜业工程,2011(5):29-32. 被引量:10
4徐彦宾,谢燕婷,闫兰,杨汝栋.硫化物沉淀法从氧化镍矿酸浸液中富集有价金属[J].有色金属:冶炼部分,2006(3):8-10. 被引量:25
5常耀超,王云,余群波.制酸烧渣综合回收铜钴实验[J].有色金属:冶炼部分,2010(5):12-14. 被引量:6
6张阳,满瑞林,王辉,梁永煌.用P507萃取分离钴及草酸反萃制备草酸钴[J].中南大学学报:自然科学版,2011,42(2):317-322. 被引量:16
7曹康学,李少龙.Cyanex272镍钴分离萃取连续扩大试验总结[J].中国有色冶金,2011,40(1):30-33. 被引量:8
8陈奇志,高锋,史磊.全湿法从锰钴镍渣中回收钴、镍的试验研究[J].企业技术开发,2014,33(2):20-22. 被引量:6
9龙志军,旷永宁.攀西地区低品位钴资源综合回收利用的工业实践[C]//第五届矿山技术论文发布会.昆明:云南省有色金属学会,2009:281-295.
10莫兴德,肖连生,张贵清,蔡旭东.HBL110从红土镍矿加压浸出液中萃取镍的研究[J].有色金属:冶炼部分,2014(6):30-33. 被引量:16
1房孟钊,余珊,李伟,彭明,宁瑞.赞比亚某铜钴矿金属回收试验研究[J].中国有色冶金,2021,50(1):86-89. 被引量:4
1宁瑞,房孟钊,李伟.两种白合金的浸出性能对比[J].有色矿冶,2022,38(1):30-35. 被引量:1
2任婷,牟兴兵,施辉献,庄晓东,袁野,徐庆鑫.从净化钴渣中富集Co的工艺研究[J].云南冶金,2022,51(4):77-79.
3房孟钊.非洲铜钴矿中钴资源回收利用的发展现状[J].硫磷设计与粉体工程,2023(2):14-17.
4房孟钊.铜钴矿脱砷处理工艺的可行性分析[J].硫磷设计与粉体工程,2023(3):5-9.
1Steve N.Dixon,范正.滴淋优于喷淋[J].黄金科技动态,1990(10):23-25.
2田庆华,程利振,袁廷刚,辛云涛,郭学益.NaOH-Na_2S熔盐法处理分银渣[J].中南大学学报:自然科学版,2014,45(8):2553-2558. 被引量:9
3孙召明,孙培梅.选择性沉淀法从堆浸液中分离回收铜镍[J].湖南有色金属,2004,20(2):12-14. 被引量:3
4吴洁.克尔罗奇斯特公司堆浸液的管理技术[J].黄金科技动态,1992(3):21-23. 被引量:1
5胡锦珂,谢继武,庞桐柏,芦胜利.从多杂质高浓度堆浸液中提取高纯五氧化二钒[J].河南化工,1992(12):7-10.
6黄万抚,王淀佐,胡永平.乳状液膜技术自铜矿堆浸液回收Cu^(2+)的研究[J].金属矿山,2002(6):17-19. 被引量:11
7杨项军,陈景,韦群燕,赵家春,李奇伟.从碱性氰化液中萃取低浓度Au(Ⅰ)的放大实验[J].化学研究与应用,2004,16(5):693-694. 被引量:1
8张健,肖连生,孙振,曾理.用HBL110从高浓度硫酸钴溶液中萃取分离镍[J].湿法冶金,2016,35(5):399-402. 被引量:3
9郑雅杰,陈学文,乐红春,彭丽婧.高铁生物堆浸液Na_2S_2O_3回收铜新工艺[J].湖南有色金属,2011,27(1):13-16. 被引量:2
10李桂英,戴子林,唐谦.水相pH值和有机相配比对从石煤酸浸液中萃取钒影响的研究[J].材料研究与应用,2010,4(2):142-144. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TF816[冶金工程—有色金属冶金]
Citation Information:
A new process was applied of copper extraction with Mextral 984 Hat first and then cobalt extraction with a new extractant of HBL110,to recover cobalt from the heap leaching solution of copper-cobalt ore containing such impurities as iron.The effects were investigated of extractant concentration and saponification rate,equilibrium pH value,temperature and phase ratio on cobalt extraction.The experimental results show that cobalt extraction rate is over 95% after four-stage countercurrent extraction under the conditions as follows:extractant concentration of 50.5%,saponification rate of 50%,equilibrium pH value of 2.4~2.6,phase ratio of 1∶1,temperature of 30 ℃ and time of 5 min.The loaded organic phase was washed by pure water and then cobalt was stripped.The stripping rate of cobalt is more than 94% after four-stage countercurrent stripping with 0.7mol/L H2SO4 solution under the conditions as follows:phase ratio of 8∶1,temperature of 40℃and time of 5min.Cobalt is enriched and separated from such impurities as iron,manganese and magnesium,and its concentration is 20g/L in the stripped solution.
quote
| GB/T 7714-2015 | [1] MOU Hong-ying, XIAO Lian-sheng, YAO Kun. Extraction and Recovery of Cobalt from the Heap Leaching Solution of Copper-Cobalt Ore with HBL110[J]. Rare Metals and Cemented Carbides, 2016(3): 21-24. |
| MLA | [1] MOU Hong-ying, et al., "Extraction and Recovery of Cobalt from the Heap Leaching Solution of Copper-Cobalt Ore with HBL110." Rare Metals and Cemented Carbides, no. 3, 2016, pp. 21-24. |
| APA | [1] MOU Hong-ying, XIAO Lian-sheng, & YAO Kun. (2016). Extraction and Recovery of Cobalt from the Heap Leaching Solution of Copper-Cobalt Ore with HBL110. Rare Metals and Cemented Carbides(3), 21-24. |
| IEEE | [1] MOU Hong-ying, XIAO Lian-sheng, and YAO Kun, "Extraction and Recovery of Cobalt from the Heap Leaching Solution of Copper-Cobalt Ore with HBL110," Rare Metals and Cemented Carbides, no. 3, pp. 21-24, 2016. keywords: {cobalt recovery;copper-cobalt ore;heap leaching solution;HBL110;extraction;stripping} |