Abstract:Impacts of morphology and microstructure of yellow tungsten on properties of nanometer WC powders were studied. Two kinds of nanometer W powders were obtained respectively by hydrogen reduc-tion of pretreated fine-grained yellow tungsten and normal yellow tungsten in a tube furnace at 560-760 ℃. After mixed with carbon black powders,both the two kinds of W powders were carbonized at 1 180 ℃ to prepare nanometer WC powders. Ultrafine-grained WC-Co sintered bodies were obtained by mixing, pressing and sintering of WC powders. And then the properties of nanometer WC powders and WC-Co sin- tered bodies were characterized. The results show that nanometer W powders of loose microstructure and good dispersion can be obtained more easily with fine-grained yellow tungsten of loose porous microstruc-ture. The obtained nanometer WC powders are more uniform,and the corresponding ultrafine-grained WC -Co sintered body has uniform microstructure and excellent performance.
KeyWords AITranslate
1Akhtar F, Humail I S, Askari S J, et al. Effect of WC particle size on the microstructure,mechanical properties and fracture behavior of WC-(W,Ti,Ta)C-6wt% Co ce mented carbides[J]. International Journal of Refractory Metals Hard Materials,2007,25(5-6) :405-410.
2Zhang Li, Wang Yuanjie, Yu Xianwang, et al. Crack propagation characteristic and toughness of functional- lygraded WC- Co cemented carbide [J]. International Journal of Refractory Metals g Hard Materials, 2008, 26(4) :295-300.
3Fang Z Z,Wang Xu,Ryu Taegong,et al. Sintering and mechanical properties of nanocrystalline cemented tung- sten carbide A review[J]. Int Journal of Refractory Metals Hard Materials, 2009,27 (2) : 288-299.
4Michalski A, Siemiaszko D. Nanocrystalline cemented carbides sintered by the pulse plasma method[J]. Inter- national Journal of Refractory Metals Hard Materi- als,2007,25(2) :153-158.
5Mallika K, Komanduri R. Diamond coatings on cemented tungsten carbide tools by low-pressure microwave CVD [J]. Wear,1999,224(2) :245-266.
6张凤林,朱敏,王成勇.纳米硬质合金进展[J].稀有金属,2002,26(1):54-58. 被引量:30
7佘建芳.德国维迪阿公司超细硬质合金的发展[J].稀有金属与硬质合金,2002,30(2):55-58. 被引量:6
8张立,陈述,刘刚,杨贵彬,黄泽兰,黄伯云,张传福.高性能超细、纳米硬质合金及其制备过程中的关键技术问题[J].材料导报,2005,19(11):4-7. 被引量:21
9Bonache V,Salvador M D,Rocha V G,et al. Microstruc rural control of ultrafine and nanocrystalline WC-12Co VC/Cr3C2 mixture by spark plasma sintering[J]. Ce ramics International,2011,37(3) :1 139-1 142.
10Saito Hiroyuki, Iwabuchi Akira, Shimizu Tomoharu. Effects of Co content and WC grain size on wear of WC cemented carbide[J]. Wear, 2006, 261 (2): 126- 132.
1雷纯鹏,赵勇军,刘刚,唐建成.3种特殊微结构WC-Co硬质合金的研究进展[J].粉末冶金工业,2014,24(5):48-53. 被引量:6
1钟毓斌,肖晗,孙娟,朱坤.碳化工艺对中细WC粉性能的影响[J].中国钨业,2016,31(4):58-60. 被引量:5
2钟毓斌,孙娟,涂洁,郝立伟.超细、纳米晶硬质合金的原料制备研究[J].中国钨业,2016,31(6):35-40. 被引量:6
3王蕾,刘辛,谢焕文,邹黎明,蔡一湘.不同方法制备的球形铸造碳化钨粉末的性能研究[J].粉末冶金工业,2017,27(4):7-11. 被引量:2
4石建萍,丁海萍,周筱.热分解法制备喷涂用Co-Cr-V复合粉末[J].粉末冶金工业,2018,28(1):11-14.
5郑娟,赵志伟,刘晓芳,陈飞晓,杨宝震.纳米复合抑制剂对微波法制备WC-TiC-Co硬质合金组成和微观结构的影响[J].粉末冶金工业,2018,28(4):21-25. 被引量:2
6朱二涛,张久兴,杨新宇,潘亚飞,羊建高.超细硬质合金原材料性能对比研究[J].粉末冶金工业,2020,30(6):74-79. 被引量:2
1罗骥,方哲成,郭志猛,邵慧萍.含V和Cr纳米W粉碳化热力学分析及实验[J].材料热处理学报,2011,32(2):26-29.
2雷纯鹏,唐建成,刘刚,刘原.氧化钨还原过程中的形貌结构遗传特性研究[J].稀有金属与硬质合金,2012,40(5):1-6. 被引量:7
3高海燕,曹顺华.机械合金化制备纳米晶硬质合金粉的进展[J].粉末冶金技术,2003,21(6):355-358. 被引量:6
4黄柱成,傅伯诒,李树根,刘沂渊,冯国良.冷固结球团直接还原采用强力混合机的研究[J].烧结球团,1995,20(2):19-22.
5张永平,包崇军,崔丁方,雷志华,张薇.顶吹炉处理铅阳极泥的工业试验[J].有色金属:冶炼部分,2016(11):5-7. 被引量:4
6王春星.硬质合金厂混合料制备工艺设备的合理选择[J].工程设计与研究(长沙),1994(1):17-22. 被引量:1
7傅小明.纳米碳化钨的制备技术及研究现状[J].稀有金属与硬质合金,2011,39(1):57-60. 被引量:4
8罗骥,郭志猛,林涛,胡学晟.纳米WC粉氢处理脱除游离碳的研究[J].材料热处理学报,2007,28(1):38-41. 被引量:2
9吴桐,唐建成,叶楠,卓海鸥,薛滢妤,周旭升.碳辅助氢还原制备纳米钨粉的工艺及机理[J].中国有色金属学报,2016,26(5):1027-1033. 被引量:8
10潘小伟.冶金过程的搅拌混合和精炼[J].大型铸锻件,1990(1):30-33.
Basic Information:
DOI:
Chinese Library Classification Number:TF122[冶金工程—粉末冶金]
Citation Information:
Abstract:Impacts of morphology and microstructure of yellow tungsten on properties of nanometer WC powders were studied. Two kinds of nanometer W powders were obtained respectively by hydrogen reduc-tion of pretreated fine-grained yellow tungsten and normal yellow tungsten in a tube furnace at 560-760 ℃. After mixed with carbon black powders,both the two kinds of W powders were carbonized at 1 180 ℃ to prepare nanometer WC powders. Ultrafine-grained WC-Co sintered bodies were obtained by mixing, pressing and sintering of WC powders. And then the properties of nanometer WC powders and WC-Co sin- tered bodies were characterized. The results show that nanometer W powders of loose microstructure and good dispersion can be obtained more easily with fine-grained yellow tungsten of loose porous microstruc-ture. The obtained nanometer WC powders are more uniform,and the corresponding ultrafine-grained WC -Co sintered body has uniform microstructure and excellent performance.
quote
| GB/T 7714-2015 | [1] LEI Chun-peng, LIU Gang, TANG Jian-cheng, et al. Impacts of Morphology and Microstructure of Tungsten Oxide on Properties and Sintering Performance of Nanometer WC Powders[J]. Rare Metals and Cemented Carbides, 2013(2): 53-57. |
| MLA | [1] LEI Chun-peng, et al., "Impacts of Morphology and Microstructure of Tungsten Oxide on Properties and Sintering Performance of Nanometer WC Powders." Rare Metals and Cemented Carbides, no. 2, 2013, pp. 53-57. |
| APA | [1] LEI Chun-peng, LIU Gang, TANG Jian-cheng, & ZHANG Fang. (2013). Impacts of Morphology and Microstructure of Tungsten Oxide on Properties and Sintering Performance of Nanometer WC Powders. Rare Metals and Cemented Carbides(2), 53-57. |
| IEEE | [1] LEI Chun-peng, LIU Gang, TANG Jian-cheng, and ZHANG Fang, "Impacts of Morphology and Microstructure of Tungsten Oxide on Properties and Sintering Performance of Nanometer WC Powders," Rare Metals and Cemented Carbides, no. 2, pp. 53-57, 2013. keywords: {tungsten oxide;nanometer W powder;nanometer WC powder;morphology and microstructure;sintering performance} |