4D Printing of a Sodium Alginate Hydrogel with Step-Wise Shape Deformation Based on Variation of Crosslinking Density AITranslate
Abstract AITranslate
Stimuli-responsive hydrogels with tailored mechanical performances and tunable responsiveness are highly demanded in many fields, including actuators, sensors, drug delivery systems, etc. Herein, we prepared a 4D printing methacrylated alginate (SA-MA) hydrogel, and the effect of the degree of methacrylation on 3D printability, crosslinking density, and responsiveness to Ca2+/chitosan crosslinking were systematically studied. The 4D-printed SA-MA hydrogels perform a step-wise volume contraction and mechanical enhancement when sequentially immersed in Ca2+ and chitosan solutions due to the crosslinking increase. Based on this, a bilayer of SA-MA hydrogel with different chemical crosslinking densities performed an anisotropic shape change by Ca2+ soaking. Furthermore, the 4D-printed SA-MA hydrogel with gradient crosslinking density shows multiple deformations by two-step ionic immersion. This controllable shape change provides a strategy for well-defined structure manufacturing.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsapm.1c01034
Chinese Library Classification Number:
Citation Information:
Stimuli-responsive hydrogels with tailored mechanical performances and tunable responsiveness are highly demanded in many fields, including actuators, sensors, drug delivery systems, etc. Herein, we prepared a 4D printing methacrylated alginate (SA-MA) hydrogel, and the effect of the degree of methacrylation on 3D printability, crosslinking density, and responsiveness to Ca2+/chitosan crosslinking were systematically studied. The 4D-printed SA-MA hydrogels perform a step-wise volume contraction and mechanical enhancement when sequentially immersed in Ca2+ and chitosan solutions due to the crosslinking increase. Based on this, a bilayer of SA-MA hydrogel with different chemical crosslinking densities performed an anisotropic shape change by Ca2+ soaking. Furthermore, the 4D-printed SA-MA hydrogel with gradient crosslinking density shows multiple deformations by two-step ionic immersion. This controllable shape change provides a strategy for well-defined structure manufacturing.
quote
| GB/T 7714-2015 | [1] Pengrui Cao, Liming Tao, Junhui Gong, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01034. |
| MLA | [1] Pengrui Cao, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01034. |
| APA | [1] Pengrui Cao, Liming Tao, Junhui Gong, Tingmei Wang, Qihua Wang, Junping Ju, & Yaoming Zhang. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01034 |
| IEEE | [1] Pengrui Cao, Liming Tao, Junhui Gong, Tingmei Wang, Qihua Wang, Junping Ju, and Yaoming Zhang, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01034. keywords: {dual stimuliresponsive;4D printing;sodium alginate;hydrogels;crosslinking density} |