Abstract AITranslate

Increasing water pollution and the lack of large-scale purification processes pose a great environmental burden. In the present work, water-borne polyurethane composite membranes containing TiO2 active particles are prepared via a single-step electrospinning procedure by using water as the unique solvent. The mats are then explored as photocatalytic platforms for wastewater treatment. Despite the fact that the amount of embedded TiO2 is found to influence the nanofiber dimension (i.e., 540–840 nm), the fabricated mats are generally characterized by self-standing nature, high porosity, marked thermal stability, and excellent mechanical resistance. TiO2 particles are proved to endow the composite membranes with photocatalytic features when irradiated with solar light, giving marked adsorption ability and abatement capacity. In addition, mat reusability is demonstrated over five cycles showing no activity loss. Due to their low cost, great efficiency, and high fabrication rate, the proposed composite mats represent a promising class of recyclable filtering materials.

KeyWords AITranslate

electrospun nanofibers waterborne polyurethanes titanium dioxidebased composites photocatalytic properties Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01029

Chinese Library Classification Number:

Citation Information:

Increasing water pollution and the lack of large-scale purification processes pose a great environmental burden. In the present work, water-borne polyurethane composite membranes containing TiO2 active particles are prepared via a single-step electrospinning procedure by using water as the unique solvent. The mats are then explored as photocatalytic platforms for wastewater treatment. Despite the fact that the amount of embedded TiO2 is found to influence the nanofiber dimension (i.e., 540–840 nm), the fabricated mats are generally characterized by self-standing nature, high porosity, marked thermal stability, and excellent mechanical resistance. TiO2 particles are proved to endow the composite membranes with photocatalytic features when irradiated with solar light, giving marked adsorption ability and abatement capacity. In addition, mat reusability is demonstrated over five cycles showing no activity loss. Due to their low cost, great efficiency, and high fabrication rate, the proposed composite mats represent a promising class of recyclable filtering materials.

quote

GB/T 7714-2015 [1] Stefano Alberti, Andrea Dodero, Emanuela Sartori, et al. ACS Applied Polymer Materials, 2021(3). DOI:10.1021/acsapm.1c01029.
MLA [1] Stefano Alberti, et al., ACS Applied Polymer Materials, no. 3, 2021, https://doi.org/10.1021/acsapm.1c01029.
APA [1] Stefano Alberti, Andrea Dodero, Emanuela Sartori, Silvia Vicini, Maurizio Ferretti, & Maila Castellano. (2021). ACS Applied Polymer Materials(3). https://doi.org/10.1021/acsapm.1c01029
IEEE [1] Stefano Alberti, Andrea Dodero, Emanuela Sartori, Silvia Vicini, Maurizio Ferretti, and Maila Castellano, ACS Applied Polymer Materials, no. 3, 2021, doi: 10.1021/acsapm.1c01029. keywords: {electrospun nanofibers;waterborne polyurethanes;titanium dioxidebased composites;photocatalytic properties;Show More}