daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Efficient NiO Impregnated Walnut Shell-Derived Carbon for Dye-Sensitized Solar Cells AITranslate

Al-Azhar University; Wuhan University of Technology; Al-Azhar University; Wuhan University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The conversion of biowaste into useful materials for technological uses has received a lot of interest in recent years. Here, a NiO@walnut shell (WS)-derived carbon composite (NiO@WS-derived carbon) was synthesized to be employed as an alternate counter electrode (CE) in dye-sensitized solar cells (DSSCs). The morphological studies demonstrated that NiO nanoparticles were uniformly impregnated into the WS-derived carbon frameworks. The electrochemical investigations showed that the NiO@WS-derived carbon composite CE displayed high catalytic activity and significant stability toward the I3–/I– redox couple after 100 CV cycles. The charge-transfer resistance of the NiO@WS-derived carbon composite CE (2.21 Ω) was also lower than that of the Pt-CE (3.04 Ω). The power conversion efficiency of the assembled DSSC with NiO@WS-derived carbon composite CE is 8.30%, which is comparable to Pt-CE (8.18%). NiO@WS-derived carbon composite CE is a possible alternative to the pricey Pt-CE in DSSC due to its low cost and excellent catalytic activity with acceptable stability.

KeyWords AITranslate

sustainable energy biomassderived carbon metal oxides porous carbon redox couples
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01216

Chinese Library Classification Number:

Citation Information:

The conversion of biowaste into useful materials for technological uses has received a lot of interest in recent years. Here, a NiO@walnut shell (WS)-derived carbon composite (NiO@WS-derived carbon) was synthesized to be employed as an alternate counter electrode (CE) in dye-sensitized solar cells (DSSCs). The morphological studies demonstrated that NiO nanoparticles were uniformly impregnated into the WS-derived carbon frameworks. The electrochemical investigations showed that the NiO@WS-derived carbon composite CE displayed high catalytic activity and significant stability toward the I3–/I– redox couple after 100 CV cycles. The charge-transfer resistance of the NiO@WS-derived carbon composite CE (2.21 Ω) was also lower than that of the Pt-CE (3.04 Ω). The power conversion efficiency of the assembled DSSC with NiO@WS-derived carbon composite CE is 8.30%, which is comparable to Pt-CE (8.18%). NiO@WS-derived carbon composite CE is a possible alternative to the pricey Pt-CE in DSSC due to its low cost and excellent catalytic activity with acceptable stability.

quote

GB/T 7714-2015 [1] Abdelaal S. A. Ahmed, Wanchun Xiang, Mohamed Abdelmotalleib, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01216.
MLA [1] Abdelaal S. A. Ahmed, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01216.
APA [1] Abdelaal S. A. Ahmed, Wanchun Xiang, Mohamed Abdelmotalleib, & Xiujian Zhao. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01216
IEEE [1] Abdelaal S. A. Ahmed, Wanchun Xiang, Mohamed Abdelmotalleib, and Xiujian Zhao, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01216. keywords: {sustainable energy biomassderived carbon metal oxides porous carbon redox couples}